Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.710 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
11.27 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P63/mmc [194]
Hall
-P 6c 2c
Point Group
6/mmm
Crystal System
hexagonal

Electronic Structure

Topological data for ICSD ID 618021 from Topological Materials Database
Topological Classification
SM*
Subclassification
ESFD
Crossing Type
Point
* Semimetal
Enforced Semimetal with Fermi point Degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
BN (mp-984) <0 0 1> <0 0 1> 0.000 38.3
GaSb (mp-1156) <1 1 1> <0 0 1> 0.000 66.9
LaF3 (mp-905) <0 0 1> <0 0 1> 0.001 181.7
WS2 (mp-224) <0 0 1> <0 0 1> 0.001 114.8
MoS2 (mp-1434) <0 0 1> <0 0 1> 0.001 114.8
CdSe (mp-2691) <1 1 1> <0 0 1> 0.002 66.9
MoSe2 (mp-1634) <0 0 1> <0 0 1> 0.005 9.6
DyScO3 (mp-31120) <1 0 0> <0 0 1> 0.005 229.5
WSe2 (mp-1821) <0 0 1> <0 0 1> 0.006 9.6
PbSe (mp-2201) <1 1 1> <0 0 1> 0.010 66.9
MoSe2 (mp-1634) <1 1 0> <0 0 1> 0.019 267.8
TbScO3 (mp-31119) <1 0 0> <0 0 1> 0.020 229.5
Bi2Se3 (mp-541837) <0 0 1> <0 0 1> 0.021 181.7
Mg (mp-153) <0 0 1> <0 0 1> 0.029 114.8
CdWO4 (mp-19387) <1 0 0> <0 0 1> 0.034 124.3
LiF (mp-1138) <1 1 1> <0 0 1> 0.042 28.7
GdScO3 (mp-5690) <0 0 1> <0 0 1> 0.048 95.6
TePb (mp-19717) <1 1 1> <0 0 1> 0.054 296.5
MgAl2O4 (mp-3536) <1 1 1> <0 0 1> 0.055 114.8
C (mp-66) <1 1 1> <0 0 1> 0.062 66.9
MoSe2 (mp-1634) <1 0 0> <0 0 1> 0.077 153.0
CaCO3 (mp-3953) <0 0 1> <0 0 1> 0.081 66.9
Al2O3 (mp-1143) <0 0 1> <0 0 1> 0.086 181.7
WS2 (mp-224) <1 1 1> <0 0 1> 0.087 239.1
MgO (mp-1265) <1 1 1> <0 0 1> 0.088 124.3
LiF (mp-1138) <1 0 0> <0 0 1> 0.089 181.7
CdTe (mp-406) <1 0 0> <0 0 1> 0.089 306.0
TiO2 (mp-390) <0 0 1> <0 0 1> 0.094 306.0
ZnSe (mp-1190) <1 0 0> <0 0 1> 0.095 229.5
GaSe (mp-1943) <0 0 1> <0 0 1> 0.096 38.3
ZnTe (mp-2176) <1 1 1> <0 0 1> 0.099 66.9
TeO2 (mp-2125) <1 0 0> <0 0 1> 0.100 210.4
InSb (mp-20012) <1 0 0> <0 0 1> 0.103 306.0
Ge(Bi3O5)4 (mp-23352) <1 1 1> <0 0 1> 0.113 181.7
InAs (mp-20305) <1 1 1> <0 0 1> 0.120 66.9
MgF2 (mp-1249) <0 0 1> <0 0 1> 0.125 153.0
GdScO3 (mp-5690) <1 0 0> <0 0 1> 0.128 229.5
GaAs (mp-2534) <1 0 0> <0 0 1> 0.132 229.5
CdS (mp-672) <0 0 1> <0 0 1> 0.137 181.7
TiO2 (mp-2657) <1 0 1> <0 0 1> 0.144 258.2
SiO2 (mp-6930) <1 0 0> <1 0 0> 0.145 247.7
Ga2O3 (mp-886) <1 0 1> <0 0 1> 0.149 325.1
TiO2 (mp-2657) <0 0 1> <0 0 1> 0.155 153.0
WSe2 (mp-1821) <1 0 1> <1 0 1> 0.159 50.5
WSe2 (mp-1821) <1 1 0> <1 1 0> 0.170 85.8
WSe2 (mp-1821) <1 0 0> <1 0 0> 0.170 49.5
ZnO (mp-2133) <1 1 0> <0 0 1> 0.176 153.0
TeO2 (mp-2125) <0 0 1> <0 0 1> 0.179 95.6
BaTiO3 (mp-5986) <1 0 1> <0 0 1> 0.196 114.8
Fe3O4 (mp-19306) <1 1 1> <0 0 1> 0.198 124.3
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
275 62 63 0 0 0
62 275 63 0 0 0
63 63 240 0 0 0
0 0 0 79 0 0
0 0 0 0 79 0
0 0 0 0 0 106
Compliance Tensor Sij (10-12Pa-1)
4 -0.7 -0.9 0 0 0
-0.7 4 -0.9 0 0 0
-0.9 -0.9 4.6 0 0 0
0 0 0 12.7 0 0
0 0 0 0 12.7 0
0 0 0 0 0 9.4
Shear Modulus GV
93 GPa
Bulk Modulus KV
130 GPa
Shear Modulus GR
91 GPa
Bulk Modulus KR
129 GPa
Shear Modulus GVRH
92 GPa
Bulk Modulus KVRH
130 GPa
Elastic Anisotropy
0.10
Poisson's Ratio
0.21

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Zr2TlC (mp-1025524) 0.0214 0.000 3
Zr2InC (mp-20004) 0.0204 0.000 3
Ti2AlC (mp-12990) 0.0726 0.000 3
Hf2TlC (mp-1078712) 0.0602 0.000 3
Nb2InC (mp-19835) 0.0485 0.000 3
Co3H (mp-1025425) 0.2848 0.182 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Hf_pv In_d C
Final Energy/Atom
-8.6828 eV
Corrected Energy
-69.4625 eV
-69.4625 eV = -69.4625 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 161970
  • 163521
  • 161969
  • 161971
  • 163520
  • 163508
  • 618021
Submitted by
User remarks:
  • High pressure experimental phase
  • Hafnium indium carbide (2/1/1)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)