material

InN

ID:

mp-22205

DOI:

10.17188/1183678


Tags: Indium nitride Indium nitride - wurtzite-type

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.090 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
6.64 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.478 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P63mc [186]
Hall
P 6c 2c
Point Group
6mm
Crystal System
hexagonal

Electronic Structure

Topological data for ICSD ID 25677 from Topological Materials Database
Topological Classification
SM*
Subclassification
ES
Crossing Type
Line
* Semimetal
Enforced Semimetal with Line or Plane degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
No elastic tensor calculated for this material, so elastic energies not avaialable. Sorting by MCIA instead.
substrate material substrate orientation film orientation MCIA [Å2]
LaAlO3 (mp-2920) <0 0 1> <0 0 1> 77.9
AlN (mp-661) <0 0 1> <0 0 1> 33.4
AlN (mp-661) <1 0 1> <1 0 0> 124.5
LaAlO3 (mp-2920) <1 0 1> <0 0 1> 300.3
AlN (mp-661) <1 1 0> <1 0 1> 211.9
CeO2 (mp-20194) <1 1 0> <0 0 1> 166.9
CeO2 (mp-20194) <1 1 1> <0 0 1> 211.3
AlN (mp-661) <1 0 0> <1 1 0> 107.8
AlN (mp-661) <1 1 1> <0 0 1> 255.8
CeO2 (mp-20194) <1 0 0> <1 1 1> 150.5
GaAs (mp-2534) <1 0 0> <1 0 0> 166.0
BaF2 (mp-1029) <1 1 0> <1 1 0> 107.8
GaAs (mp-2534) <1 1 0> <1 1 0> 143.8
GaAs (mp-2534) <1 1 1> <0 0 1> 178.0
BaF2 (mp-1029) <1 0 0> <0 0 1> 200.2
BaF2 (mp-1029) <1 1 1> <0 0 1> 211.3
GaN (mp-804) <0 0 1> <0 0 1> 77.9
GaN (mp-804) <1 0 0> <1 0 1> 70.6
GaN (mp-804) <1 0 1> <0 0 1> 133.5
GaN (mp-804) <1 1 0> <0 0 1> 233.6
GaN (mp-804) <1 1 1> <1 1 1> 150.5
SiO2 (mp-6930) <0 0 1> <0 0 1> 144.6
SiO2 (mp-6930) <1 0 0> <1 0 1> 211.9
SiO2 (mp-6930) <1 0 1> <1 0 0> 249.0
SiO2 (mp-6930) <1 1 0> <1 0 0> 186.8
SiO2 (mp-6930) <1 1 1> <1 1 1> 263.4
KCl (mp-23193) <1 0 0> <1 0 1> 259.0
KCl (mp-23193) <1 1 1> <0 0 1> 211.3
DyScO3 (mp-31120) <0 1 1> <1 0 1> 211.9
DyScO3 (mp-31120) <1 0 0> <1 1 0> 179.7
DyScO3 (mp-31120) <0 0 1> <1 0 0> 62.3
DyScO3 (mp-31120) <0 1 0> <0 0 1> 166.9
DyScO3 (mp-31120) <1 0 1> <1 0 0> 166.0
DyScO3 (mp-31120) <1 1 0> <1 0 0> 332.1
ZnSe (mp-1190) <1 1 0> <1 1 0> 143.8
InAs (mp-20305) <1 0 0> <1 0 0> 228.3
InAs (mp-20305) <1 1 0> <1 1 0> 107.8
InAs (mp-20305) <1 1 1> <0 0 1> 278.1
ZnSe (mp-1190) <1 0 0> <1 0 0> 166.0
ZnSe (mp-1190) <1 1 1> <0 0 1> 178.0
KTaO3 (mp-3614) <1 1 0> <1 1 0> 71.9
KTaO3 (mp-3614) <1 0 0> <1 1 1> 150.5
KTaO3 (mp-3614) <1 1 1> <1 0 0> 228.3
CdS (mp-672) <0 0 1> <0 0 1> 44.5
CdS (mp-672) <1 0 0> <1 0 0> 228.3
CdS (mp-672) <1 1 0> <1 0 0> 249.0
CdS (mp-672) <1 1 1> <0 0 1> 267.0
CdS (mp-672) <1 0 1> <1 1 0> 287.6
LiF (mp-1138) <1 0 0> <1 1 1> 150.5
LiF (mp-1138) <1 1 0> <1 1 0> 71.9
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
189 61 40 0 0 0
61 189 40 0 0 0
40 40 292 0 0 0
0 0 0 52 0 0
0 0 0 0 52 0
0 0 0 0 0 64
Compliance Tensor Sij (10-12Pa-1)
6 -1.8 -0.6 0 0 0
-1.8 6 -0.6 0 0 0
-0.6 -0.6 3.6 0 0 0
0 0 0 19.3 0 0
0 0 0 0 19.3 0
0 0 0 0 0 15.6
Shear Modulus GV
69 GPa
Bulk Modulus KV
106 GPa
Shear Modulus GR
63 GPa
Bulk Modulus KR
103 GPa
Shear Modulus GVRH
66 GPa
Bulk Modulus KVRH
104 GPa
Elastic Anisotropy
0.45
Poisson's Ratio
0.24

Piezoelectricity

Reference for tensor and properties: Methodology
Piezoelectric Tensor eij (C/m2)
0.00000 0.00000 0.00000 0.00000 -5.55115 0.00000
0.00000 0.00000 0.00000 -5.55115 0.00000 0.00000
-0.45301 -0.45301 0.87696 0.00000 0.00000 0.00000
Piezoelectric Modulus ‖eijmax
5.55115 C/m2
Crystallographic Direction vmax
0.00000
-1.00000
0.00000

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
2234.69 -0.00 0.00
-0.00 2234.69 0.00
0.00 0.00 9.65
Dielectric Tensor εij (total)
2248.69 -0.00 0.00
-0.00 2248.69 0.00
0.00 0.00 16.25
Polycrystalline dielectric constant εpoly
(electronic contribution)
1493.01
Polycrystalline dielectric constant εpoly
(total)
1504.54
Refractive Index n
38.64
Potentially ferroelectric?
Unknown

Equations of State

Reference:
Equation E0 (eV) V0 (Å3) B C
mie_gruneisen -5.443 16.128 6.697 6.828
pack_evans_james -5.443 16.130 0.742 3.612
vinet -5.444 16.117 6.830 5.539
tait -5.443 16.117 0.750 5.761
birch_euler -5.443 16.126 0.840 0.628
pourier_tarantola -5.446 16.112 0.130 2.676
birch_lagrange -5.452 16.121 0.485 6.277
murnaghan -5.442 16.147 0.723 3.467
Equations reference

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
BeSiN2 (mp-7913) 0.0869 0.000 3
LiInSe2 (mp-20310) 0.1222 0.001 3
MgSnN2 (mp-1029791) 0.0755 0.000 3
ZnSnN2 (mp-1029469) 0.0795 0.000 3
Zn2SbN3 (mp-1029334) 0.1344 0.004 3
LiCo7O7F (mp-764039) 0.2493 0.061 4
LiCo5O5F (mp-764225) 0.2822 0.069 4
Li2ZnSnS4 (mp-555186) 0.1975 0.000 4
ZnGaNO (mp-558481) 0.2625 0.058 4
ZnGa3N3O (mp-555777) 0.2897 0.025 4
MnS (mp-2562) 0.0109 0.810 2
AgI (mp-22894) 0.0047 0.001 2
ZnO (mp-2133) 0.0064 0.000 2
SmSe (mp-10643) 0.0211 0.536 2
AgH (mp-1096804) 0.0208 0.134 2
Ge (mp-1007760) 0.1170 0.121 1
Si (mp-165) 0.1242 0.011 1
C (mp-611426) 0.2893 0.146 1
C (mp-47) 0.1307 0.162 1
Ge (mp-1091415) 0.2961 0.008 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Synthesis Descriptions

For the preparation of pure GaN, Ga(NO3)3 (0.2g, Sigma Chemical Co.) was dissolved in methanol (2mL) at room temperature under fast stirring to form a clear and colorless solution, after which sol [...]
In this work, we report a systematic study on the growth temperature dependences of MOCVD-grown InN. Epitaxial 200-nm-thick InN films were grown on (0001) sapphire at the growth temperature range o [...]
chef hat mixing beaker

Explore more synthesis descriptions for materials of composition InN.

Text computed by synthesisproject.org.

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: In_d N
Final Energy/Atom
-5.4424 eV
Corrected Energy
-21.7697 eV
-21.7697 eV = -21.7697 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 184927
  • 162684
  • 157515
  • 67768
  • 181366
  • 41999
  • 640026
  • 191774
  • 41544
  • 190428
  • 25677
  • 109463
Submitted by
User remarks:
  • Indium nitride

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)