material

Zr2Ag

ID:

mp-2221

DOI:

10.17188/1197425


Tags: Zirconium silver (2/1) Silver zirconium (1/2)

Material Details

Final Magnetic Moment
0.002 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.106 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
7.43 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
I4/mmm [139]
Hall
-I 4 2
Point Group
4/mmm
Crystal System
tetragonal

Electronic Structure

Topological data for ICSD ID 58391 from Topological Materials Database
Topological Classification
SM*
Subclassification
ESFD
Crossing Type
Point
* Semimetal
Enforced Semimetal with Fermi point Degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
CsI (mp-614603) <1 0 0> <0 0 1> 0.000 308.6
SiC (mp-8062) <1 0 0> <0 0 1> 0.001 95.8
BaTiO3 (mp-5986) <1 1 0> <1 1 1> 0.002 286.3
Ge(Bi3O5)4 (mp-23352) <1 0 0> <0 0 1> 0.008 106.4
CdSe (mp-2691) <1 0 0> <0 0 1> 0.042 191.5
TiO2 (mp-2657) <1 0 1> <0 0 1> 0.049 127.7
TePb (mp-19717) <1 1 1> <1 1 0> 0.055 225.1
SrTiO3 (mp-4651) <1 1 0> <0 0 1> 0.060 308.6
NdGaO3 (mp-3196) <1 1 0> <0 0 1> 0.061 308.6
ZnO (mp-2133) <0 0 1> <0 0 1> 0.066 74.5
C (mp-48) <1 0 1> <0 0 1> 0.066 159.6
SiC (mp-11714) <1 1 1> <1 0 1> 0.067 164.8
GaSb (mp-1156) <1 0 0> <0 0 1> 0.067 191.5
LiGaO2 (mp-5854) <0 1 0> <1 0 1> 0.074 164.8
ZnO (mp-2133) <1 0 1> <1 0 0> 0.077 39.8
LiNbO3 (mp-3731) <1 0 1> <0 0 1> 0.078 308.6
KTaO3 (mp-3614) <1 1 1> <0 0 1> 0.078 223.5
KTaO3 (mp-3614) <1 1 0> <0 0 1> 0.079 159.6
MgF2 (mp-1249) <1 1 0> <0 0 1> 0.086 244.7
CeO2 (mp-20194) <1 0 0> <0 0 1> 0.092 266.0
LiGaO2 (mp-5854) <1 1 1> <0 0 1> 0.094 223.5
Si (mp-149) <1 0 0> <0 0 1> 0.100 266.0
LiAlO2 (mp-3427) <1 0 0> <1 0 0> 0.101 199.0
LiGaO2 (mp-5854) <1 0 0> <0 0 1> 0.101 106.4
PbSe (mp-2201) <1 0 0> <0 0 1> 0.106 191.5
LaAlO3 (mp-2920) <1 0 0> <0 0 1> 0.110 212.8
TePb (mp-19717) <1 0 0> <0 0 1> 0.120 42.6
BN (mp-984) <1 1 0> <0 0 1> 0.126 202.2
TbScO3 (mp-31119) <1 0 1> <0 0 1> 0.127 223.5
TiO2 (mp-2657) <1 1 0> <0 0 1> 0.130 138.3
CdS (mp-672) <1 0 0> <0 0 1> 0.133 287.3
DyScO3 (mp-31120) <1 0 1> <0 0 1> 0.133 223.5
Al (mp-134) <1 1 1> <0 0 1> 0.134 223.5
Al (mp-134) <1 1 0> <0 0 1> 0.136 159.6
LaF3 (mp-905) <1 0 0> <0 0 1> 0.138 53.2
AlN (mp-661) <1 1 1> <0 0 1> 0.141 287.3
LiGaO2 (mp-5854) <1 0 1> <0 0 1> 0.143 266.0
LiTaO3 (mp-3666) <1 0 1> <0 0 1> 0.145 308.6
TiO2 (mp-390) <1 1 1> <0 0 1> 0.148 329.9
TeO2 (mp-2125) <1 0 0> <1 0 0> 0.154 278.5
C (mp-48) <1 1 0> <1 0 0> 0.158 199.0
CdWO4 (mp-19387) <0 1 1> <0 0 1> 0.163 287.3
ZrO2 (mp-2858) <1 0 -1> <0 0 1> 0.163 287.3
TeO2 (mp-2125) <1 1 0> <1 0 0> 0.172 199.0
GdScO3 (mp-5690) <1 0 1> <0 0 1> 0.173 223.5
GaN (mp-804) <1 0 0> <0 0 1> 0.181 85.1
LaF3 (mp-905) <0 0 1> <1 0 0> 0.182 318.3
SrTiO3 (mp-4651) <1 0 0> <0 0 1> 0.186 223.5
CdWO4 (mp-19387) <1 1 1> <0 0 1> 0.191 255.4
SiC (mp-11714) <1 1 0> <0 0 1> 0.195 329.9
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
157 54 91 0 0 0
54 157 91 0 0 0
91 91 126 0 0 0
0 0 0 63 0 0
0 0 0 0 63 0
0 0 0 0 0 32
Compliance Tensor Sij (10-12Pa-1)
11.2 1.4 -9.1 0 0 0
1.4 11.2 -9.1 0 0 0
-9.1 -9.1 21.1 0 0 0
0 0 0 15.8 0 0
0 0 0 0 15.8 0
0 0 0 0 0 30.8
Shear Modulus GV
45 GPa
Bulk Modulus KV
101 GPa
Shear Modulus GR
35 GPa
Bulk Modulus KR
101 GPa
Shear Modulus GVRH
40 GPa
Bulk Modulus KVRH
101 GPa
Elastic Anisotropy
1.47
Poisson's Ratio
0.32

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
GaCuPt2 (mp-644280) 0.1734 0.000 3
MnSbRh2 (mp-571163) 0.1079 0.094 3
CoSnRh2 (mp-1018085) 0.0989 0.060 3
CrSnRh2 (mp-1018066) 0.1762 0.000 3
AlCuPt2 (mp-12550) 0.1200 0.000 3
Yb3Tc (mp-979938) 0.0961 0.411 2
PmF3 (mp-862901) 0.0989 0.000 2
HgPd (mp-2685) 0.1015 0.000 2
Hf2Ag (mp-13155) 0.0848 0.000 2
Hf2Cd (mp-1018156) 0.0900 0.000 2
Hg (mp-975272) 0.6508 0.001 1
K (mp-972981) 0.6544 0.008 1
Hg (mp-569360) 0.5733 0.001 1
W (mp-1065340) 0.6233 0.491 1
Eu (mp-1057315) 0.6511 0.000 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Zr_sv Ag
Final Energy/Atom
-6.7485 eV
Corrected Energy
-20.2454 eV
Uncorrected energy = -20.2454 eV Corrected energy = -20.2454 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 58391
  • 163153
  • 605999
Submitted by
User remarks:
  • Silver zirconium (1/2)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)