material

SrInPt

ID:

mp-22284

DOI:

10.17188/1197506


Tags: Strontium platinum indium High pressure experimental phase

Material Details

Final Magnetic Moment
-0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
Non-magnetic
Formation Energy / Atom
-0.781 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
8.75 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Pnma [62]
Hall
-P 2ac 2n
Point Group
mmm
Crystal System
orthorhombic

Band Structure

Density of States
Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

sign indicates spin ↑ ↓

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
MoSe2 (mp-1634) <0 0 1> <0 1 0> 0.007 315.2
WSe2 (mp-1821) <0 0 1> <0 1 0> 0.007 315.2
ZnSe (mp-1190) <1 0 0> <0 1 1> 0.016 263.5
GaAs (mp-2534) <1 0 0> <0 1 1> 0.023 263.5
ZrO2 (mp-2858) <1 0 0> <0 0 1> 0.026 315.0
GdScO3 (mp-5690) <1 0 1> <1 0 1> 0.027 224.3
GaN (mp-804) <0 0 1> <1 1 1> 0.028 169.1
TiO2 (mp-390) <0 0 1> <0 0 1> 0.030 175.0
TbScO3 (mp-31119) <1 0 1> <1 0 1> 0.033 224.3
GaN (mp-804) <1 1 0> <0 1 1> 0.034 263.5
AlN (mp-661) <1 1 1> <0 0 1> 0.037 315.0
TiO2 (mp-2657) <1 1 0> <0 0 1> 0.038 175.0
LiAlO2 (mp-3427) <1 0 1> <1 0 1> 0.040 299.1
CeO2 (mp-20194) <1 1 0> <0 0 1> 0.047 210.0
Si (mp-149) <1 1 0> <0 0 1> 0.050 210.0
SiC (mp-8062) <1 1 0> <0 0 1> 0.051 245.0
WS2 (mp-224) <0 0 1> <1 1 1> 0.052 169.1
Ge (mp-32) <1 0 0> <0 1 1> 0.052 263.5
MoS2 (mp-1434) <0 0 1> <1 1 1> 0.052 169.1
TiO2 (mp-390) <1 0 0> <1 0 1> 0.056 74.8
MgF2 (mp-1249) <1 1 1> <0 0 1> 0.062 210.0
BaTiO3 (mp-5986) <0 0 1> <0 1 0> 0.062 354.7
C (mp-48) <1 0 1> <1 0 1> 0.064 299.1
MoSe2 (mp-1634) <1 1 0> <1 0 0> 0.064 264.3
WSe2 (mp-1821) <1 1 1> <1 0 0> 0.066 264.3
Al (mp-134) <1 0 0> <0 1 1> 0.066 263.5
DyScO3 (mp-31120) <1 0 1> <1 0 1> 0.066 224.3
LiGaO2 (mp-5854) <0 1 0> <1 0 1> 0.068 299.1
CdWO4 (mp-19387) <0 0 1> <0 0 1> 0.075 245.0
CaCO3 (mp-3953) <1 0 0> <1 0 0> 0.078 264.3
CdWO4 (mp-19387) <1 1 0> <1 0 0> 0.080 330.4
NdGaO3 (mp-3196) <0 0 1> <1 1 0> 0.083 153.9
KTaO3 (mp-3614) <1 1 1> <1 0 1> 0.095 224.3
LiF (mp-1138) <1 0 0> <0 1 1> 0.100 263.5
CdS (mp-672) <1 0 1> <0 1 0> 0.107 197.0
C (mp-48) <0 0 1> <1 1 0> 0.113 230.8
MgAl2O4 (mp-3536) <1 0 0> <0 1 1> 0.114 263.5
Te2Mo (mp-602) <1 1 0> <0 0 1> 0.115 280.0
KTaO3 (mp-3614) <1 0 0> <0 1 1> 0.117 263.5
KCl (mp-23193) <1 1 0> <1 1 0> 0.121 230.8
ZrO2 (mp-2858) <1 1 0> <0 1 1> 0.121 158.1
BN (mp-984) <1 1 0> <1 0 0> 0.122 66.1
Al (mp-134) <1 1 1> <1 0 1> 0.127 224.3
LiTaO3 (mp-3666) <0 0 1> <0 1 1> 0.127 210.8
SiC (mp-11714) <1 0 0> <0 0 1> 0.131 280.0
SiC (mp-7631) <1 0 0> <0 0 1> 0.136 140.0
PbS (mp-21276) <1 1 0> <1 1 0> 0.137 153.9
Mg (mp-153) <0 0 1> <1 0 0> 0.140 330.4
BN (mp-984) <0 0 1> <1 0 0> 0.144 66.1
ZnO (mp-2133) <1 0 0> <0 1 0> 0.149 354.7
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
89 42 46 0 0 0
42 94 57 0 0 0
46 57 89 0 0 0
0 0 0 37 0 0
0 0 0 0 25 0
0 0 0 0 0 23
Compliance Tensor Sij (10-12Pa-1)
16.1 -3.7 -5.9 0 0 0
-3.7 18.2 -9.8 0 0 0
-5.9 -9.8 20.6 0 0 0
0 0 0 26.7 0 0
0 0 0 0 39.7 0
0 0 0 0 0 42.6
Shear Modulus GV
26 GPa
Bulk Modulus KV
62 GPa
Shear Modulus GR
24 GPa
Bulk Modulus KR
62 GPa
Shear Modulus GVRH
25 GPa
Bulk Modulus KVRH
62 GPa
Elastic Anisotropy
0.34
Poisson's Ratio
0.32

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Na2LiGaAs2 (mp-9722) 0.4699 0.000 4
K2LiInAs2 (mp-505431) 0.4135 0.000 4
K2LiGaAs2 (mp-9703) 0.5899 0.000 4
KNa4SnSb3 (mp-6758) 0.5491 0.004 4
Na2LiAlP2 (mp-9719) 0.5722 0.000 4
SrH2 (mp-23714) 0.6043 0.000 2
BaH2 (mp-23715) 0.5488 0.000 2
Cr2As (mp-22064) 0.5769 0.107 2
YbH2 (mp-864603) 0.5749 0.000 2
Fe3P (mp-18708) 0.6124 0.000 2
TmAlRh (mp-568685) 0.2416 0.000 3
ZrPRu (mp-22268) 0.2504 0.000 3
CaInRh (mp-20220) 0.1377 0.000 3
EuInPd (mp-22322) 0.2198 0.000 3
EuInPt (mp-21051) 0.2087 0.000 3
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Sr_sv In_d Pt
Final Energy/Atom
-4.2706 eV
Corrected Energy
-51.2471 eV
-51.2471 eV = -51.2471 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 410704
Submitted by
User remarks:
  • Strontium platinum indium
  • High pressure experimental phase

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)