material

HfCoSn

ID:

mp-22315

DOI:

10.17188/1197548


Tags: Hafnium cobalt tin (1/1/1) - supercell Hafnium cobalt stannide (1/1/1)

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.444 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
11.31 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P62c [190]
Hall
P 6c 2c
Point Group
6m2
Crystal System
hexagonal

Electronic Structure

Topological data for ICSD ID 107472 from Topological Materials Database
Topological Classification
SM*
Subclassification
ESFD
Crossing Type
Point
* Semimetal
Enforced Semimetal with Fermi point Degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
KP(HO2)2 (mp-23959) <0 1 0> <1 0 0> 0.000 152.8
Te2Mo (mp-602) <0 0 1> <0 0 1> 0.004 43.8
LiNbO3 (mp-3731) <0 0 1> <0 0 1> 0.004 306.5
Te2Mo (mp-602) <1 0 0> <0 0 1> 0.010 218.9
C (mp-48) <0 0 1> <0 0 1> 0.011 131.3
LiTaO3 (mp-3666) <0 0 1> <0 0 1> 0.011 306.5
TbScO3 (mp-31119) <1 1 0> <1 0 0> 0.018 254.7
InSb (mp-20012) <1 1 1> <0 0 1> 0.026 306.5
C (mp-66) <1 0 0> <1 0 0> 0.031 50.9
KCl (mp-23193) <1 0 0> <1 0 0> 0.032 203.8
LiF (mp-1138) <1 0 0> <0 0 1> 0.039 350.3
CdTe (mp-406) <1 1 1> <0 0 1> 0.040 306.5
ZnTe (mp-2176) <1 0 0> <0 0 1> 0.040 306.5
DyScO3 (mp-31120) <1 1 0> <1 0 0> 0.051 254.7
TiO2 (mp-390) <1 0 0> <1 1 1> 0.059 295.5
KP(HO2)2 (mp-23959) <0 0 1> <1 0 0> 0.070 152.8
GdScO3 (mp-5690) <1 1 0> <1 0 0> 0.072 254.7
Ga2O3 (mp-886) <1 0 0> <0 0 1> 0.076 218.9
SiC (mp-11714) <0 0 1> <0 0 1> 0.090 131.3
CdSe (mp-2691) <1 0 0> <0 0 1> 0.093 306.5
SiC (mp-11714) <1 1 0> <1 0 1> 0.100 268.7
SiC (mp-7631) <0 0 1> <0 0 1> 0.100 131.3
SiC (mp-8062) <1 1 1> <0 0 1> 0.126 131.3
BaTiO3 (mp-5986) <1 1 0> <0 0 1> 0.147 262.7
GaSb (mp-1156) <1 1 0> <0 0 1> 0.152 218.9
CdWO4 (mp-19387) <0 1 0> <1 1 0> 0.154 264.7
CdSe (mp-2691) <1 1 0> <0 0 1> 0.156 218.9
PbSe (mp-2201) <1 1 0> <0 0 1> 0.157 218.9
SiO2 (mp-6930) <1 1 1> <0 0 1> 0.166 262.7
LaAlO3 (mp-2920) <0 0 1> <0 0 1> 0.171 175.1
AlN (mp-661) <1 0 0> <1 0 0> 0.171 254.7
GaN (mp-804) <1 0 1> <1 1 0> 0.187 264.7
C (mp-48) <1 0 1> <1 1 1> 0.190 98.5
Ge (mp-32) <1 1 1> <0 0 1> 0.195 175.1
SiC (mp-8062) <1 1 0> <0 0 1> 0.214 218.9
C (mp-66) <1 1 0> <0 0 1> 0.227 218.9
LiGaO2 (mp-5854) <0 1 1> <1 0 0> 0.239 254.7
ZnO (mp-2133) <0 0 1> <0 0 1> 0.247 175.1
AlN (mp-661) <0 0 1> <0 0 1> 0.248 175.1
LiF (mp-1138) <1 1 0> <0 0 1> 0.248 350.3
ZnTe (mp-2176) <1 1 0> <0 0 1> 0.264 218.9
Al (mp-134) <1 1 0> <0 0 1> 0.277 350.3
InAs (mp-20305) <1 1 0> <0 0 1> 0.287 218.9
Te2W (mp-22693) <0 1 0> <0 0 1> 0.291 218.9
Mg (mp-153) <0 0 1> <1 0 0> 0.296 305.6
NaCl (mp-22862) <1 0 0> <1 0 0> 0.299 254.7
GaAs (mp-2534) <1 1 1> <0 0 1> 0.328 175.1
Cu (mp-30) <1 1 0> <0 0 1> 0.339 218.9
MoS2 (mp-1434) <0 0 1> <1 0 0> 0.340 305.6
WS2 (mp-224) <0 0 1> <1 0 0> 0.341 305.6
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
235 101 101 0 0 0
101 235 101 0 0 0
101 101 188 0 0 0
0 0 0 93 0 0
0 0 0 0 93 0
0 0 0 0 0 67
Compliance Tensor Sij (10-12Pa-1)
5.9 -1.5 -2.4 0 0 0
-1.5 5.9 -2.4 0 0 0
-2.4 -2.4 7.9 0 0 0
0 0 0 10.8 0 0
0 0 0 0 10.8 0
0 0 0 0 0 14.9
Shear Modulus GV
74 GPa
Bulk Modulus KV
141 GPa
Shear Modulus GR
70 GPa
Bulk Modulus KR
139 GPa
Shear Modulus GVRH
72 GPa
Bulk Modulus KVRH
140 GPa
Elastic Anisotropy
0.29
Poisson's Ratio
0.28

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
ScSnPt (mp-18198) 0.2244 0.000 3
ZrSnIr (mp-607139) 0.2439 0.000 3
ZrGaPt (mp-601253) 0.2298 0.000 3
HfAlPt (mp-571619) 0.2052 0.000 3
ZrSnRh (mp-4667) 0.2486 0.000 3
TaNi2TeSe (mp-622009) 0.7187 0.000 4
Mg3Al8FeSi6 (mp-571315) 0.7329 0.141 4
GePt2 (mp-20061) 0.6057 0.032 2
GePd2 (mp-423) 0.5275 0.000 2
UPt2 (mp-30854) 0.6250 0.000 2
K2Re (mp-1080778) 0.6177 1.993 2
K2Tc (mp-1084834) 0.5815 1.575 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Hf_pv Co Sn_d
Final Energy/Atom
-7.4633 eV
Corrected Energy
-134.3398 eV
Uncorrected energy = -134.3398 eV Corrected energy = -134.3398 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 408899
  • 107472
Submitted by
User remarks:
  • Hafnium cobalt stannide (1/1/1)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)