Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.463 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.12 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap1.469 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/m [11] |
Hall-P 2yb |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | elastic energy [meV] | MCIA† [Å2] |
---|---|---|---|---|
BN (mp-984) | <1 0 1> | <1 0 -1> | 0.008 | 301.8 |
TiO2 (mp-2657) | <1 0 1> | <0 0 1> | 0.023 | 282.8 |
BaTiO3 (mp-5986) | <1 0 1> | <1 0 0> | 0.025 | 70.1 |
ZrO2 (mp-2858) | <0 1 0> | <1 1 1> | 0.039 | 195.4 |
SiC (mp-11714) | <1 1 0> | <0 0 1> | 0.041 | 161.6 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 0.050 | 282.8 |
NaCl (mp-22862) | <1 0 0> | <0 0 1> | 0.055 | 161.6 |
GdScO3 (mp-5690) | <1 1 0> | <0 0 1> | 0.060 | 323.2 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 0.062 | 323.2 |
CdWO4 (mp-19387) | <0 0 1> | <0 0 1> | 0.067 | 121.2 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 0.068 | 80.8 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 0.073 | 282.8 |
GdScO3 (mp-5690) | <1 0 0> | <1 0 0> | 0.075 | 140.1 |
AlN (mp-661) | <1 1 0> | <1 0 -1> | 0.085 | 301.8 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 -1> | 0.086 | 301.8 |
TiO2 (mp-390) | <0 0 1> | <1 0 -1> | 0.089 | 301.8 |
TiO2 (mp-390) | <1 1 1> | <0 0 1> | 0.091 | 161.6 |
SiO2 (mp-6930) | <1 1 1> | <1 0 0> | 0.097 | 210.2 |
Al (mp-134) | <1 0 0> | <0 0 1> | 0.101 | 80.8 |
BaTiO3 (mp-5986) | <0 0 1> | <0 0 1> | 0.104 | 80.8 |
Mg (mp-153) | <1 0 1> | <1 0 0> | 0.126 | 280.3 |
Cu (mp-30) | <1 0 0> | <0 0 1> | 0.128 | 323.2 |
C (mp-66) | <1 0 0> | <0 0 1> | 0.134 | 202.0 |
TbScO3 (mp-31119) | <1 0 0> | <1 0 0> | 0.148 | 140.1 |
Cu (mp-30) | <1 1 0> | <1 0 0> | 0.165 | 280.3 |
BaTiO3 (mp-5986) | <1 1 1> | <0 0 1> | 0.171 | 282.8 |
TbScO3 (mp-31119) | <0 1 0> | <1 0 -1> | 0.172 | 301.8 |
ZnO (mp-2133) | <1 1 1> | <0 0 1> | 0.172 | 282.8 |
TbScO3 (mp-31119) | <1 1 0> | <0 0 1> | 0.178 | 323.2 |
Au (mp-81) | <1 1 1> | <0 0 1> | 0.200 | 121.2 |
ZrO2 (mp-2858) | <1 0 -1> | <0 0 1> | 0.214 | 323.2 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 0.221 | 323.2 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 0.221 | 140.1 |
Fe2O3 (mp-24972) | <1 0 0> | <0 0 1> | 0.228 | 282.8 |
Ga2O3 (mp-886) | <1 0 1> | <0 0 1> | 0.233 | 323.2 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 0.239 | 121.2 |
SiC (mp-11714) | <1 1 1> | <0 0 1> | 0.239 | 161.6 |
C (mp-48) | <1 1 1> | <1 0 -1> | 0.240 | 301.8 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 0.264 | 280.3 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 0.271 | 323.2 |
Ga2O3 (mp-886) | <1 0 0> | <1 0 1> | 0.279 | 257.9 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 0.287 | 161.6 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 -1> | 0.289 | 226.4 |
SiC (mp-8062) | <1 0 0> | <0 0 1> | 0.298 | 282.8 |
GdScO3 (mp-5690) | <0 0 1> | <0 0 1> | 0.298 | 282.8 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 0.299 | 140.1 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 0.301 | 282.8 |
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 0.305 | 140.1 |
AlN (mp-661) | <1 1 1> | <1 0 -1> | 0.306 | 226.4 |
C (mp-48) | <1 0 1> | <1 0 1> | 0.311 | 257.9 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
104 | 43 | 54 | 0 | -1 | 0 |
43 | 116 | 40 | 0 | 1 | 0 |
54 | 40 | 130 | 0 | 0 | 0 |
0 | 0 | 0 | 24 | 0 | 0 |
-1 | 1 | 0 | 0 | 33 | 0 |
0 | 0 | 0 | 0 | 0 | 39 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
13.3 | -3.3 | -4.5 | 0 | 0.7 | 0 |
-3.3 | 10.5 | -1.9 | 0 | -0.4 | 0 |
-4.5 | -1.9 | 10.1 | 0 | -0.2 | 0 |
0 | 0 | 0 | 41.9 | 0 | -0.1 |
0.7 | -0.4 | -0.2 | 0 | 30.4 | 0 |
0 | 0 | 0 | -0.1 | 0 | 25.9 |
Shear Modulus GV33 GPa |
Bulk Modulus KV69 GPa |
Shear Modulus GR32 GPa |
Bulk Modulus KR69 GPa |
Shear Modulus GVRH33 GPa |
Bulk Modulus KVRH69 GPa |
Elastic Anisotropy0.22 |
Poisson's Ratio0.30 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Hf2N2O (mp-780169) | 0.5685 | 0.079 | 3 |
Hf2N2O (mp-780050) | 0.4843 | 0.087 | 3 |
Li2FeF4 (mp-777665) | 0.6243 | 0.531 | 3 |
Ce2SnSe4 (mp-1006368) | 0.5935 | 0.077 | 3 |
Ce2Sb2Se5 (mp-1080287) | 0.5819 | 0.127 | 3 |
Cs2Li14Tb3O14 (mp-8711) | 0.6272 | 0.043 | 4 |
Li4Co3OF8 (mp-763942) | 0.6237 | 0.072 | 4 |
Li7V(O2F)2 (mp-765831) | 0.6145 | 0.103 | 4 |
Li4Fe3OF8 (mp-764594) | 0.6192 | 0.078 | 4 |
Rb2Li14Tb3O14 (mp-556675) | 0.6546 | 0.041 | 4 |
Y2O3 (mp-775907) | 0.5100 | 0.053 | 2 |
Ho2S3 (mp-878) | 0.0170 | 0.000 | 2 |
V2O3 (mp-776630) | 0.4617 | 0.086 | 2 |
Ti2O3 (mp-776456) | 0.3243 | 0.074 | 2 |
Y2S3 (mp-541289) | 0.0565 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Er_3 S |
Final Energy/Atom-6.3736 eV |
Corrected Energy-203.1500 eV
-203.1500 eV = -191.2077 eV (uncorrected energy) - 11.9423 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)