material

Sn7Ru3

ID:

mp-22344

DOI:

10.17188/1197574


Tags: Ruthenium stannide (3/7)

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.222 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
8.85 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Im3m [229]
Hall
-I 4 2 3
Point Group
m3m
Crystal System
cubic

Electronic Structure

Topological data for ICSD ID 54510 from Topological Materials Database
Topological Classification
SM*
Subclassification
ESFD
Crossing Type
Point
* Semimetal
Enforced Semimetal with Fermi point Degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Si (mp-149) <1 1 1> <1 1 1> 0.001 155.6
Al (mp-134) <1 1 0> <1 1 0> 0.001 254.1
Si (mp-149) <1 1 0> <1 1 0> 0.001 127.1
CeO2 (mp-20194) <1 1 1> <1 1 1> 0.002 155.6
CeO2 (mp-20194) <1 1 0> <1 1 0> 0.003 127.1
PbS (mp-21276) <1 0 0> <1 0 0> 0.007 179.7
C (mp-66) <1 1 1> <1 1 1> 0.015 155.6
KTaO3 (mp-3614) <1 1 0> <1 1 0> 0.023 254.1
CaCO3 (mp-3953) <0 0 1> <1 1 1> 0.024 155.6
Bi2Te3 (mp-34202) <0 0 1> <1 1 1> 0.055 155.6
MgO (mp-1265) <1 0 0> <1 0 0> 0.060 89.8
NdGaO3 (mp-3196) <0 1 0> <1 1 0> 0.067 127.1
GaP (mp-2490) <1 1 1> <1 1 1> 0.123 155.6
GaP (mp-2490) <1 1 0> <1 1 0> 0.125 127.1
InP (mp-20351) <1 0 0> <1 0 0> 0.136 179.7
NdGaO3 (mp-3196) <1 0 1> <1 0 0> 0.166 269.5
YAlO3 (mp-3792) <0 0 1> <1 1 0> 0.168 254.1
LiGaO2 (mp-5854) <0 0 1> <1 1 0> 0.182 254.1
CaF2 (mp-2741) <1 1 1> <1 1 1> 0.203 155.6
CaF2 (mp-2741) <1 1 0> <1 1 0> 0.208 127.1
MgF2 (mp-1249) <0 0 1> <1 0 0> 0.308 89.8
ZrO2 (mp-2858) <1 0 0> <1 1 0> 0.319 254.1
InSb (mp-20012) <1 1 0> <1 1 0> 0.337 127.1
InSb (mp-20012) <1 0 0> <1 0 0> 0.359 89.8
MgF2 (mp-1249) <1 0 1> <1 0 0> 0.371 269.5
CdTe (mp-406) <1 1 0> <1 1 0> 0.379 127.1
CdTe (mp-406) <1 0 0> <1 0 0> 0.403 89.8
Al2O3 (mp-1143) <1 0 0> <1 1 0> 0.438 127.1
GaN (mp-804) <1 0 0> <1 1 0> 0.556 254.1
LaAlO3 (mp-2920) <1 1 0> <1 1 0> 0.585 127.1
SrTiO3 (mp-4651) <1 0 1> <1 0 0> 0.663 269.5
CsI (mp-614603) <1 1 0> <1 1 0> 0.789 254.1
DyScO3 (mp-31120) <1 0 1> <1 0 0> 0.887 269.5
YVO4 (mp-19133) <1 0 1> <1 0 0> 0.956 269.5
TiO2 (mp-390) <1 1 0> <1 1 0> 0.972 254.1
NdGaO3 (mp-3196) <0 1 1> <1 1 0> 0.974 254.1
TiO2 (mp-390) <1 0 0> <1 0 0> 0.980 179.7
C (mp-48) <1 0 0> <1 0 0> 1.083 269.5
TbScO3 (mp-31119) <1 0 1> <1 0 0> 1.171 269.5
SiC (mp-7631) <1 1 0> <1 1 0> 1.224 254.1
TePb (mp-19717) <1 1 0> <1 1 0> 1.298 127.1
TePb (mp-19717) <1 0 0> <1 0 0> 1.381 89.8
GdScO3 (mp-5690) <1 0 1> <1 0 0> 1.822 269.5
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
188 71 71 0 0 0
71 188 71 0 0 0
71 71 188 0 0 0
0 0 0 28 0 0
0 0 0 0 28 0
0 0 0 0 0 28
Compliance Tensor Sij (10-12Pa-1)
6.7 -1.8 -1.8 0 0 0
-1.8 6.7 -1.8 0 0 0
-1.8 -1.8 6.7 0 0 0
0 0 0 35.4 0 0
0 0 0 0 35.4 0
0 0 0 0 0 35.4
Shear Modulus GV
40 GPa
Bulk Modulus KV
110 GPa
Shear Modulus GR
36 GPa
Bulk Modulus KR
110 GPa
Shear Modulus GVRH
38 GPa
Bulk Modulus KVRH
110 GPa
Elastic Anisotropy
0.67
Poisson's Ratio
0.34

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
NbCoTe2 (mp-5603) 0.7468 0.000 3
NbNiTe2 (mp-20506) 0.7327 0.000 3
NbFeTe2 (mp-616481) 0.7315 0.057 3
Nb3Sb2Te5 (mp-569571) 0.2059 0.000 3
TaNiTe2 (mp-19810) 0.7349 0.000 3
In7Pt3 (mp-22075) 0.1269 0.000 2
In7Pd3 (mp-568655) 0.1093 0.000 2
Sb7Mo3 (mp-1521) 0.1071 0.000 2
Sn7Os3 (mp-2729) 0.0384 0.008 2
Ga7Ni3 (mp-16852) 0.1572 0.000 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Sn_d Ru_pv
Final Energy/Atom
-5.7992 eV
Corrected Energy
-115.9848 eV
-115.9848 eV = -115.9848 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 150763
  • 54510
  • 54511
Submitted by
User remarks:
  • Ruthenium stannide (3/7)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)