Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.286 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.65 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.065 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI42d [122] |
HallI 4 2bw |
Point Group42m |
Crystal Systemtetragonal |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 1 1> | 128.1 |
LaAlO3 (mp-2920) | <1 1 0> | <1 1 0> | 120.5 |
LaAlO3 (mp-2920) | <1 1 1> | <1 1 1> | 128.1 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 260.7 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 347.6 |
AlN (mp-661) | <1 1 1> | <1 0 1> | 287.0 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 170.5 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 347.6 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 217.2 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 304.1 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 170.5 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 43.4 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 120.5 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 217.2 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 1> | 287.0 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 347.6 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 170.5 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 217.2 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 347.6 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 217.2 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 217.2 |
Te2W (mp-22693) | <0 0 1> | <1 1 0> | 241.1 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 217.2 |
YVO4 (mp-19133) | <1 0 1> | <1 0 1> | 287.0 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 43.4 |
TePb (mp-19717) | <1 1 0> | <1 1 0> | 120.5 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 86.9 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 255.7 |
BN (mp-984) | <0 0 1> | <0 0 1> | 347.6 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 217.2 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 347.6 |
Al (mp-134) | <1 0 0> | <0 0 1> | 217.2 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 304.1 |
LiGaO2 (mp-5854) | <1 0 0> | <0 0 1> | 217.2 |
LiGaO2 (mp-5854) | <1 1 0> | <1 0 1> | 95.7 |
CdTe (mp-406) | <1 0 0> | <0 0 1> | 43.4 |
CdTe (mp-406) | <1 1 0> | <1 1 0> | 120.5 |
LiTaO3 (mp-3666) | <1 1 1> | <1 0 0> | 255.7 |
MgO (mp-1265) | <1 1 0> | <1 0 1> | 287.0 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 43.4 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 217.2 |
TiO2 (mp-2657) | <1 0 1> | <0 0 1> | 304.1 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 173.8 |
TiO2 (mp-2657) | <1 1 1> | <1 0 1> | 287.0 |
Ge3(BiO3)4 (mp-23560) | <1 0 0> | <0 0 1> | 217.2 |
C (mp-66) | <1 0 0> | <0 0 1> | 217.2 |
C (mp-66) | <1 1 0> | <0 0 1> | 217.2 |
GdScO3 (mp-5690) | <1 1 1> | <1 0 1> | 287.0 |
Mg (mp-153) | <1 0 0> | <0 0 1> | 347.6 |
Mg (mp-153) | <1 0 1> | <1 0 0> | 170.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Piezoelectric Tensor eij (C/m2) |
|||||
---|---|---|---|---|---|
0.00000 | 0.00000 | 0.00000 | -0.05160 | 0.00000 | 0.00000 |
0.00000 | 0.00000 | 0.00000 | 0.00000 | -0.05160 | 0.00000 |
0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.03053 |
Piezoelectric Modulus ‖eij‖max0.05160 C/m2 |
Crystallographic Direction vmax |
---|
0.00000 |
1.00000 |
0.00000 |
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
12.61 | 0.00 | 0.00 |
0.00 | 12.61 | 0.00 |
0.00 | 0.00 | 12.80 |
Dielectric Tensor εij (total) |
||
---|---|---|
15.30 | 0.00 | 0.00 |
0.00 | 15.30 | 0.00 |
0.00 | 0.00 | 16.01 |
Polycrystalline dielectric constant
εpoly∞
12.68
|
Polycrystalline dielectric constant
εpoly
15.54
|
Refractive Index n3.56 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CdSnAs2 (mp-3829) | 0.0127 | 0.000 | 3 |
CdSnP2 (mp-5213) | 0.0171 | 0.000 | 3 |
LiInSe2 (mp-20187) | 0.0191 | 0.000 | 3 |
ZnGeP2 (mp-4524) | 0.0098 | 0.000 | 3 |
AlCuS2 (mp-4979) | 0.0164 | 0.000 | 3 |
FeCu2GeS4 (mp-917359) | 0.0267 | 0.185 | 4 |
CoCu2GeS4 (mp-6498) | 0.0329 | 0.055 | 4 |
CoCu2GeS4 (mp-560428) | 0.0349 | 0.055 | 4 |
FeCu2GeS4 (mp-22053) | 0.0291 | 0.185 | 4 |
ZnCu2GeTe4 (mp-1078420) | 0.0563 | 0.005 | 4 |
Si7Ge (mp-1094056) | 0.0389 | 0.006 | 2 |
CuS (mp-760381) | 0.0476 | 0.013 | 2 |
LiN (mp-1059612) | 0.0497 | 1.430 | 2 |
CoO (mp-24864) | 0.0500 | 0.000 | 2 |
CoO (mp-715460) | 0.0482 | 0.000 | 2 |
Si (mp-149) | 0.0500 | 0.000 | 1 |
Sn (mp-117) | 0.0500 | 0.000 | 1 |
C (mp-66) | 0.0500 | 0.136 | 1 |
Ge (mp-32) | 0.0500 | 0.000 | 1 |
Se (mp-12771) | 0.0500 | 0.514 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: In_d Ag Te |
Final Energy/Atom-3.2542 eV |
Corrected Energy-27.7214 eV
Uncorrected energy = -26.0334 eV
Composition-based energy adjustment (-0.422 eV/atom x 4.0 atoms) = -1.6880 eV
Corrected energy = -27.7214 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)