Final Magnetic Moment2.998 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-1.618 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.006 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density11.35 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToU16N25 + UN |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinIa3 [206] |
Hall-I 2b 2c 3 |
Point Groupm3 |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 0> | <1 1 0> | 160.8 |
SiO2 (mp-6930) | <0 0 1> | <1 1 1> | 196.9 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 113.7 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 160.8 |
InAs (mp-20305) | <1 1 1> | <1 1 1> | 196.9 |
KTaO3 (mp-3614) | <1 1 1> | <1 1 1> | 196.9 |
Te2W (mp-22693) | <0 1 0> | <1 1 0> | 160.8 |
Te2Mo (mp-602) | <1 0 0> | <1 1 0> | 160.8 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 227.4 |
BN (mp-984) | <0 0 1> | <1 1 1> | 196.9 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 1 1> | 196.9 |
Al (mp-134) | <1 1 1> | <1 1 1> | 196.9 |
LiGaO2 (mp-5854) | <1 1 0> | <1 1 1> | 196.9 |
CdTe (mp-406) | <1 0 0> | <1 0 0> | 227.4 |
SiC (mp-7631) | <1 0 0> | <1 0 0> | 227.4 |
SiC (mp-7631) | <1 1 0> | <1 1 0> | 160.8 |
Ge3(BiO3)4 (mp-23560) | <1 0 0> | <1 0 0> | 113.7 |
Ge3(BiO3)4 (mp-23560) | <1 1 0> | <1 1 0> | 160.8 |
Ge3(BiO3)4 (mp-23560) | <1 1 1> | <1 1 1> | 196.9 |
KP(HO2)2 (mp-23959) | <0 0 1> | <1 0 0> | 227.4 |
KP(HO2)2 (mp-23959) | <0 1 0> | <1 0 0> | 227.4 |
KP(HO2)2 (mp-23959) | <1 0 0> | <1 0 0> | 113.7 |
InSb (mp-20012) | <1 0 0> | <1 0 0> | 227.4 |
PbSe (mp-2201) | <1 1 0> | <1 1 0> | 160.8 |
PbSe (mp-2201) | <1 1 1> | <1 1 1> | 196.9 |
Ga2O3 (mp-886) | <1 0 1> | <1 0 0> | 227.4 |
Au (mp-81) | <1 0 0> | <1 0 0> | 227.4 |
CdSe (mp-2691) | <1 1 0> | <1 1 0> | 160.8 |
CdSe (mp-2691) | <1 1 1> | <1 1 1> | 196.9 |
C (mp-48) | <0 0 1> | <1 0 0> | 227.4 |
ZrO2 (mp-2858) | <1 0 0> | <1 0 0> | 113.7 |
YAlO3 (mp-3792) | <0 0 1> | <1 0 0> | 113.7 |
YAlO3 (mp-3792) | <1 0 0> | <1 1 0> | 160.8 |
YAlO3 (mp-3792) | <1 1 0> | <1 0 0> | 113.7 |
SiC (mp-8062) | <1 1 0> | <1 1 0> | 160.8 |
TiO2 (mp-390) | <1 0 1> | <1 1 0> | 160.8 |
ZnO (mp-2133) | <0 0 1> | <1 1 1> | 196.9 |
GaSb (mp-1156) | <1 1 0> | <1 1 0> | 160.8 |
GaSb (mp-1156) | <1 1 1> | <1 1 1> | 196.9 |
GaTe (mp-542812) | <1 0 0> | <1 0 0> | 227.4 |
ZnTe (mp-2176) | <1 1 0> | <1 1 0> | 160.8 |
ZnTe (mp-2176) | <1 1 1> | <1 1 1> | 196.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li5FeS4 (mp-776781) | 0.3964 | 0.057 | 3 |
Y7HoO12 (mp-762307) | 0.4291 | 0.001 | 3 |
Dy11Y5O24 (mp-766279) | 0.4283 | 0.000 | 3 |
Sm27Y5O48 (mp-861145) | 0.4224 | 0.020 | 3 |
Sm3Y5O12 (mp-860969) | 0.4188 | 0.015 | 3 |
LiMnOF2 (mp-766924) | 0.6969 | 0.097 | 4 |
Li3Nb4NiO12 (mp-772009) | 0.7033 | 0.089 | 4 |
Li3Nb4FeO12 (mp-771984) | 0.7103 | 0.030 | 4 |
TiFe(BiO3)2 (mp-560185) | 0.6765 | 0.015 | 4 |
InNi2SbO6 (mp-1078367) | 0.6800 | 0.000 | 4 |
Pu2O3 (mp-637224) | 0.2371 | 0.000 | 2 |
Ce2O3 (mp-542313) | 0.1376 | 0.000 | 2 |
Mg3P2 (mp-2514) | 0.1396 | 0.000 | 2 |
Mg3As2 (mp-1990) | 0.0837 | 0.000 | 2 |
Be3N2 (mp-18337) | 0.0891 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: U N |
Final Energy/Atom-10.9063 eV |
Corrected Energy-436.2537 eV
-436.2537 eV = -436.2537 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)