material

Ta4FeP

ID:

mp-22444

DOI:

10.17188/1197652


Tags: Tantalum iron phosphide (4/1/1)

Material Details

Final Magnetic Moment
0.001 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.407 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.055 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
14.16 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Ta3P + Ta7Fe6 + TaFeP
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P4/mcc [124]
Hall
-P 4 2c
Point Group
4/mmm
Crystal System
tetragonal

Electronic Structure

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Ge (mp-32) <1 0 0> <0 0 1> 0.003 298.4
CeO2 (mp-20194) <1 0 0> <0 0 1> 0.004 149.2
Si (mp-149) <1 0 0> <0 0 1> 0.006 149.2
GaAs (mp-2534) <1 0 0> <0 0 1> 0.010 298.4
LiGaO2 (mp-5854) <0 1 0> <1 1 0> 0.021 132.0
LiGaO2 (mp-5854) <1 0 1> <0 0 1> 0.030 223.8
ZnSe (mp-1190) <1 0 0> <0 0 1> 0.039 298.4
YVO4 (mp-19133) <1 1 1> <1 0 0> 0.039 249.0
LiF (mp-1138) <1 0 0> <0 0 1> 0.043 149.2
WS2 (mp-224) <1 0 1> <1 1 1> 0.082 230.8
YVO4 (mp-19133) <1 0 0> <1 1 1> 0.082 230.8
SiO2 (mp-6930) <1 1 1> <0 0 1> 0.097 261.1
CaCO3 (mp-3953) <1 0 0> <1 1 0> 0.130 88.0
TiO2 (mp-2657) <1 0 1> <1 0 0> 0.149 280.1
TeO2 (mp-2125) <1 0 1> <1 1 1> 0.169 230.8
CdWO4 (mp-19387) <1 1 0> <1 1 1> 0.173 288.5
KTaO3 (mp-3614) <1 1 0> <1 0 0> 0.186 342.4
GaSe (mp-1943) <0 0 1> <1 0 1> 0.204 291.5
CdWO4 (mp-19387) <0 1 0> <1 0 0> 0.226 186.7
Te2Mo (mp-602) <1 1 0> <1 0 0> 0.233 93.4
GdScO3 (mp-5690) <1 1 1> <1 1 1> 0.233 288.5
InAs (mp-20305) <1 1 1> <1 1 0> 0.249 132.0
Mg (mp-153) <1 1 1> <0 0 1> 0.258 149.2
Cu (mp-30) <1 1 0> <1 0 0> 0.258 93.4
MgF2 (mp-1249) <1 0 1> <1 0 0> 0.260 186.7
BN (mp-984) <0 0 1> <1 1 0> 0.260 44.0
SiC (mp-11714) <1 0 0> <0 0 1> 0.261 186.5
ZnTe (mp-2176) <1 1 1> <1 1 0> 0.262 132.0
C (mp-66) <1 0 0> <1 0 0> 0.262 155.6
ZnO (mp-2133) <0 0 1> <1 1 0> 0.263 132.0
Cu (mp-30) <1 0 0> <1 1 0> 0.267 132.0
Al (mp-134) <1 1 0> <1 0 0> 0.268 342.4
SiC (mp-7631) <1 0 0> <1 0 0> 0.270 93.4
TeO2 (mp-2125) <1 1 0> <1 0 1> 0.270 97.2
CaCO3 (mp-3953) <0 0 1> <1 1 0> 0.275 44.0
BN (mp-984) <1 0 0> <1 0 0> 0.278 155.6
SiO2 (mp-6930) <0 0 1> <1 1 0> 0.290 44.0
C (mp-66) <1 1 1> <1 1 0> 0.294 44.0
BaTiO3 (mp-5986) <1 0 1> <1 1 0> 0.296 352.1
YVO4 (mp-19133) <0 0 1> <1 1 0> 0.299 264.1
GdScO3 (mp-5690) <1 1 0> <1 0 1> 0.302 194.3
ZrO2 (mp-2858) <1 0 0> <1 0 0> 0.304 311.2
CaCO3 (mp-3953) <1 1 0> <0 0 1> 0.309 149.2
Al2O3 (mp-1143) <1 1 0> <1 0 0> 0.309 217.9
BN (mp-984) <1 1 0> <1 1 0> 0.316 132.0
MgO (mp-1265) <1 1 0> <1 0 0> 0.328 155.6
Ga2O3 (mp-886) <1 0 0> <1 0 1> 0.331 145.7
GaP (mp-2490) <1 0 0> <0 0 1> 0.331 149.2
Al (mp-134) <1 0 0> <0 0 1> 0.331 149.2
MgF2 (mp-1249) <1 1 0> <1 0 1> 0.362 242.9
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
326 150 150 0 0 0
150 366 157 0 0 0
150 157 366 0 0 0
0 0 0 114 0 0
0 0 0 0 97 0
0 0 0 0 0 97
Compliance Tensor Sij (10-12Pa-1)
4.2 -1.2 -1.2 0 0 0
-1.2 3.7 -1.1 0 0 0
-1.2 -1.1 3.7 0 0 0
0 0 0 8.8 0 0
0 0 0 0 10.4 0
0 0 0 0 0 10.4
Shear Modulus GV
102 GPa
Bulk Modulus KV
219 GPa
Shear Modulus GR
101 GPa
Bulk Modulus KR
218 GPa
Shear Modulus GVRH
101 GPa
Bulk Modulus KVRH
219 GPa
Elastic Anisotropy
0.03
Poisson's Ratio
0.30

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Nb4CoP (mp-21447) 0.1311 0.053 3
Nb4SiNi (mp-22396) 0.2594 0.004 3
Nb4FeSi (mp-22312) 0.1236 0.048 3
Nb4CoSi (mp-10003) 0.1851 0.013 3
Zr4CuP (mp-581733) 0.2028 0.063 3
Ti2B (mp-1025149) 0.1893 0.160 2
PdPb2 (mp-20599) 0.1806 0.000 2
CoSn2 (mp-20155) 0.1988 0.013 2
Tl2Pd (mp-570896) 0.1984 0.000 2
Zr2Rh (mp-571664) 0.2031 0.000 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ta_pv Fe_pv P
Final Energy/Atom
-10.6259 eV
Corrected Energy
-127.5107 eV
Uncorrected energy = -127.5107 eV Corrected energy = -127.5107 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 86378
Submitted by
User remarks:
  • Tantalum iron phosphide (4/1/1)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)