material

YInAu2

ID:

mp-22493

DOI:

10.17188/1198738


Tags: Yttrium gold indide (1/2/1) Gold indium yttrium (2/1/1)

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.705 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
11.44 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Fm3m [225]
Hall
-F 4 2 3
Point Group
m3m
Crystal System
cubic

Electronic Structure

Topological data for ICSD ID 58514 from Topological Materials Database
Topological Classification
TI*
Subclassification
SEBR
* Topological insulator
Split Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
CsI (mp-614603) <1 0 0> <1 0 0> 0.000 246.9
BaF2 (mp-1029) <1 0 0> <1 0 0> 0.000 197.5
SiC (mp-11714) <0 0 1> <1 1 1> 0.002 256.6
ZnSe (mp-1190) <1 1 0> <1 1 0> 0.002 139.7
SiC (mp-7631) <0 0 1> <1 1 1> 0.003 256.6
TiO2 (mp-390) <0 0 1> <1 0 0> 0.004 246.9
LiAlO2 (mp-3427) <0 0 1> <1 0 0> 0.005 246.9
Ni (mp-23) <1 0 0> <1 0 0> 0.006 49.4
Ni (mp-23) <1 1 0> <1 1 0> 0.007 69.8
Ni (mp-23) <1 1 1> <1 1 1> 0.007 85.5
MgF2 (mp-1249) <0 0 1> <1 0 0> 0.010 197.5
SrTiO3 (mp-4651) <0 0 1> <1 0 0> 0.012 246.9
GaAs (mp-2534) <1 1 0> <1 1 0> 0.013 139.7
ZrO2 (mp-2858) <0 0 1> <1 0 0> 0.024 246.9
SrTiO3 (mp-4651) <1 1 0> <1 0 0> 0.050 246.9
MoSe2 (mp-1634) <0 0 1> <1 1 1> 0.051 85.5
Ge (mp-32) <1 1 0> <1 1 0> 0.052 139.7
WSe2 (mp-1821) <0 0 1> <1 1 1> 0.052 85.5
Al (mp-134) <1 1 0> <1 1 0> 0.054 69.8
Al (mp-134) <1 1 1> <1 1 1> 0.055 85.5
NdGaO3 (mp-3196) <1 1 0> <1 0 0> 0.056 246.9
SiO2 (mp-6930) <1 1 1> <1 1 0> 0.067 209.5
NaCl (mp-22862) <1 1 1> <1 1 0> 0.069 279.3
DyScO3 (mp-31120) <0 0 1> <1 1 0> 0.077 279.3
KTaO3 (mp-3614) <1 1 0> <1 1 0> 0.112 69.8
LiF (mp-1138) <1 1 0> <1 1 0> 0.113 69.8
AlN (mp-661) <0 0 1> <1 0 0> 0.113 296.3
KTaO3 (mp-3614) <1 1 1> <1 1 1> 0.114 85.5
LiF (mp-1138) <1 1 1> <1 1 1> 0.115 85.5
Al2O3 (mp-1143) <0 0 1> <1 1 1> 0.115 256.6
C (mp-48) <0 0 1> <1 1 0> 0.124 209.5
TiO2 (mp-2657) <0 0 1> <1 0 0> 0.125 197.5
CaF2 (mp-2741) <1 0 0> <1 0 0> 0.127 246.9
MgAl2O4 (mp-3536) <1 1 0> <1 1 0> 0.130 279.3
TiO2 (mp-2657) <1 0 0> <1 0 0> 0.139 345.7
Te2Mo (mp-602) <0 0 1> <1 0 0> 0.157 345.7
NaCl (mp-22862) <1 1 0> <1 1 0> 0.171 139.7
Mg (mp-153) <0 0 1> <1 0 0> 0.178 345.7
SiC (mp-11714) <1 0 0> <1 1 0> 0.183 279.3
AlN (mp-661) <1 0 0> <1 0 0> 0.186 246.9
Fe3O4 (mp-19306) <1 1 0> <1 1 0> 0.192 209.5
TbScO3 (mp-31119) <0 0 1> <1 1 0> 0.193 279.3
GaP (mp-2490) <1 0 0> <1 0 0> 0.197 246.9
TiO2 (mp-390) <1 1 0> <1 1 0> 0.212 209.5
PbSe (mp-2201) <1 0 0> <1 0 0> 0.217 197.5
GdScO3 (mp-5690) <1 0 1> <1 1 1> 0.227 171.1
Mg (mp-153) <1 1 1> <1 0 0> 0.254 246.9
Cu (mp-30) <1 1 0> <1 0 0> 0.259 148.1
MgF2 (mp-1249) <1 0 0> <1 0 0> 0.259 148.1
C (mp-66) <1 0 0> <1 1 1> 0.269 256.6
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
105 82 82 0 0 0
82 105 82 0 0 0
82 82 105 0 0 0
0 0 0 34 0 0
0 0 0 0 34 0
0 0 0 0 0 34
Compliance Tensor Sij (10-12Pa-1)
30.6 -13.4 -13.4 0 0 0
-13.4 30.6 -13.4 0 0 0
-13.4 -13.4 30.6 0 0 0
0 0 0 29.8 0 0
0 0 0 0 29.8 0
0 0 0 0 0 29.8
Shear Modulus GV
25 GPa
Bulk Modulus KV
89 GPa
Shear Modulus GR
19 GPa
Bulk Modulus KR
89 GPa
Shear Modulus GVRH
22 GPa
Bulk Modulus KVRH
89 GPa
Elastic Anisotropy
1.55
Poisson's Ratio
0.39

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Mn2GaCo (mp-20160) 0.0000 0.147 3
LiGa2Pd (mp-5159) 0.0000 0.000 3
Li2GaPd (mp-3201) 0.0000 0.000 3
AlVNi2 (mp-10899) 0.0000 0.046 3
ScGaNi2 (mp-11400) 0.0000 0.000 3
LiMgSnPd (mp-7555) 0.0000 0.000 4
LiMgSnAu (mp-7554) 0.0000 0.088 4
VFeCoGe (mp-1063914) 0.0000 0.000 4
LiMgSbPd (mp-10179) 0.0000 0.096 4
LiMgSnPt (mp-11806) 0.0000 0.000 4
SmMg3 (mp-30779) 0.0000 0.065 2
Ni3Sb (mp-10260) 0.0000 0.044 2
LiZn (mp-1934) 0.0000 0.000 2
LaF3 (mp-13181) 0.0000 0.181 2
CeCd3 (mp-2863) 0.0000 0.000 2
Pr (mp-63) 0.0000 0.136 1
Se (mp-119) 0.0000 0.602 1
Mo (mp-129) 0.0000 0.000 1
Nd (mp-4) 0.0000 0.140 1
Tb (mp-11446) 0.0000 0.148 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Y_sv In_d Au
Final Energy/Atom
-4.6463 eV
Corrected Energy
-18.5850 eV
-18.5850 eV = -18.5850 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 612079
  • 612077
  • 58514
  • 612080
Submitted by
User remarks:
  • Gold indium yttrium (2/1/1)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)