Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom0.043 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.114 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.72 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToFe3Ge + Ge |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/m [12] |
Hall-C 2y |
Point Group2/m |
Crystal Systemmonoclinic |
Topological ClassificationTI*
|
SubclassificationNLC†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
KP(HO2)2 (mp-23959) | <1 0 1> | <1 0 0> | 134.3 |
ZnTe (mp-2176) | <1 0 0> | <1 0 -1> | 229.4 |
InAs (mp-20305) | <1 0 0> | <1 0 -1> | 229.4 |
ZrO2 (mp-2858) | <0 0 1> | <1 0 -1> | 137.6 |
SiC (mp-8062) | <1 0 0> | <1 0 -1> | 229.4 |
LiTaO3 (mp-3666) | <1 0 0> | <1 0 1> | 218.0 |
BN (mp-984) | <1 1 1> | <1 0 0> | 307.0 |
CaF2 (mp-2741) | <1 0 0> | <1 0 -1> | 91.8 |
Ag (mp-124) | <1 0 0> | <1 0 -1> | 137.6 |
NdGaO3 (mp-3196) | <1 1 0> | <1 0 -1> | 183.5 |
LiAlO2 (mp-3427) | <0 0 1> | <1 0 -1> | 137.6 |
GaP (mp-2490) | <1 0 0> | <1 0 -1> | 91.8 |
CdSe (mp-2691) | <1 0 0> | <1 0 -1> | 229.4 |
CsI (mp-614603) | <1 0 0> | <1 0 -1> | 183.5 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 268.6 |
GaTe (mp-542812) | <1 0 1> | <0 1 1> | 292.5 |
SrTiO3 (mp-4651) | <1 0 0> | <1 0 1> | 218.0 |
TbScO3 (mp-31119) | <0 1 1> | <1 0 0> | 268.6 |
LiAlO2 (mp-3427) | <1 1 1> | <1 0 0> | 326.2 |
ZrO2 (mp-2858) | <1 0 -1> | <1 0 0> | 287.8 |
Au (mp-81) | <1 0 0> | <1 0 -1> | 137.6 |
Mg (mp-153) | <1 0 0> | <1 0 0> | 134.3 |
NdGaO3 (mp-3196) | <1 0 0> | <1 0 1> | 218.0 |
GaSb (mp-1156) | <1 0 0> | <1 0 -1> | 229.4 |
Te2W (mp-22693) | <0 1 0> | <1 1 -1> | 218.0 |
C (mp-48) | <0 0 1> | <1 1 0> | 178.6 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 268.6 |
CaF2 (mp-2741) | <1 1 0> | <1 0 1> | 218.0 |
PbSe (mp-2201) | <1 1 0> | <0 1 1> | 219.4 |
GaSb (mp-1156) | <1 1 0> | <0 1 1> | 219.4 |
SrTiO3 (mp-4651) | <0 0 1> | <1 0 -1> | 91.8 |
Te2W (mp-22693) | <1 0 0> | <1 1 -1> | 290.7 |
CdSe (mp-2691) | <1 1 0> | <0 1 1> | 219.4 |
Au (mp-81) | <1 1 0> | <1 0 0> | 268.6 |
PbSe (mp-2201) | <1 0 0> | <1 0 -1> | 229.4 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 134.3 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 326.2 |
C (mp-48) | <1 0 1> | <0 1 0> | 281.8 |
ZnO (mp-2133) | <1 1 1> | <1 1 1> | 156.8 |
ZnO (mp-2133) | <1 0 1> | <1 0 1> | 218.0 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 134.3 |
GaP (mp-2490) | <1 1 0> | <1 0 1> | 218.0 |
BaTiO3 (mp-5986) | <1 1 0> | <1 1 1> | 235.2 |
YAlO3 (mp-3792) | <1 1 0> | <1 0 -1> | 275.3 |
CdWO4 (mp-19387) | <1 0 0> | <1 0 1> | 218.0 |
ZrO2 (mp-2858) | <1 1 -1> | <1 0 0> | 230.2 |
GdScO3 (mp-5690) | <1 0 1> | <1 0 -1> | 229.4 |
SiC (mp-8062) | <1 1 0> | <0 1 1> | 219.4 |
YAlO3 (mp-3792) | <1 0 1> | <1 0 0> | 345.4 |
MgO (mp-1265) | <1 1 1> | <1 0 1> | 218.0 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
194 | 90 | 75 | 0 | -0 | 0 |
90 | 243 | 83 | 0 | 20 | 0 |
75 | 83 | 320 | 0 | 6 | 0 |
0 | 0 | 0 | 75 | 0 | -1 |
-0 | 20 | 6 | 0 | 64 | 0 |
0 | 0 | 0 | -1 | 0 | 79 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
6.5 | -2.2 | -1 | 0 | 0.8 | 0 |
-2.2 | 5.3 | -0.8 | 0 | -1.6 | 0 |
-1 | -0.8 | 3.6 | 0 | -0.1 | 0 |
0 | 0 | 0 | 13.3 | 0 | 0.2 |
0.8 | -1.6 | -0.1 | 0 | 16.2 | 0 |
0 | 0 | 0 | 0.2 | 0 | 12.6 |
Shear Modulus GV78 GPa |
Bulk Modulus KV139 GPa |
Shear Modulus GR74 GPa |
Bulk Modulus KR134 GPa |
Shear Modulus GVRH76 GPa |
Bulk Modulus KVRH136 GPa |
Elastic Anisotropy0.32 |
Poisson's Ratio0.27 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ga8Cu3Mo2 (mp-567502) | 0.5693 | 0.000 | 3 |
Ga8Cu3W2 (mp-568017) | 0.5240 | 0.000 | 3 |
Nb4Cr2Si5 (mp-3276) | 0.6555 | 0.034 | 3 |
Nb2Cr4Si5 (mp-29645) | 0.6953 | 0.000 | 3 |
V6Si5 (mp-976) | 0.6468 | 0.014 | 2 |
NiSn (mp-680646) | 0.7186 | 0.008 | 2 |
UIr (mp-644899) | 0.7084 | 0.401 | 2 |
Ti6Ge5 (mp-1365) | 0.7210 | 0.011 | 2 |
CoGe (mp-21237) | 0.6730 | 0.000 | 2 |
Si (mp-1079649) | 0.7396 | 0.426 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Fe_pv Ge_d |
Final Energy/Atom-6.5004 eV |
Corrected Energy-52.0034 eV
-52.0034 eV = -52.0034 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)