material

CoAsRh

ID:

mp-22546

DOI:

10.17188/1198780


Tags: Cobalt rhodium arsenide (1/1/1)

Material Details

Final Magnetic Moment
0.357 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
FM
Formation Energy / Atom
-0.309 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.021 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
9.89 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
CoAs + AsRh2 + Co
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Pnma [62]
Hall
-P 2ac 2n
Point Group
mmm
Crystal System
orthorhombic
We have not yet calculated a detailed bandstructure for this material

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
SrTiO3 (mp-4651) <0 0 1> <1 1 0> 0.012 248.1
SiO2 (mp-6930) <1 1 0> <0 1 0> 0.022 240.1
ZrO2 (mp-2858) <1 1 -1> <0 1 0> 0.026 320.1
TbScO3 (mp-31119) <1 1 0> <1 0 1> 0.031 190.3
GaSe (mp-1943) <1 0 0> <0 0 1> 0.035 67.9
InP (mp-20351) <1 0 0> <1 0 1> 0.035 142.7
GdScO3 (mp-5690) <0 0 1> <0 1 0> 0.036 160.1
BaF2 (mp-1029) <1 0 0> <1 1 0> 0.038 198.5
GaN (mp-804) <1 0 1> <1 0 1> 0.042 95.2
DyScO3 (mp-31120) <1 1 0> <1 0 1> 0.045 190.3
PbS (mp-21276) <1 1 0> <0 0 1> 0.046 203.8
Al (mp-134) <1 1 0> <1 0 0> 0.051 209.2
GaN (mp-804) <0 0 1> <0 0 1> 0.053 249.1
AlN (mp-661) <1 0 1> <1 0 0> 0.053 125.5
Mg (mp-153) <1 0 1> <1 0 1> 0.056 95.2
BN (mp-984) <1 0 1> <0 0 1> 0.058 181.2
MgF2 (mp-1249) <1 1 0> <0 1 1> 0.062 244.9
LaAlO3 (mp-2920) <1 0 1> <0 0 1> 0.064 226.5
Ni (mp-23) <1 0 0> <1 1 0> 0.068 49.6
SiC (mp-7631) <1 0 0> <0 1 1> 0.069 140.0
CdS (mp-672) <1 0 1> <1 1 1> 0.072 163.6
ZnO (mp-2133) <1 1 0> <0 1 0> 0.073 240.1
TiO2 (mp-390) <1 0 1> <0 1 0> 0.074 80.0
WS2 (mp-224) <0 0 1> <0 0 1> 0.085 249.1
MoS2 (mp-1434) <0 0 1> <0 0 1> 0.086 249.1
PbS (mp-21276) <1 0 0> <1 0 1> 0.087 142.7
GaSe (mp-1943) <0 0 1> <0 1 1> 0.089 175.0
MgO (mp-1265) <1 1 1> <1 0 0> 0.098 125.5
MoSe2 (mp-1634) <0 0 1> <1 1 1> 0.098 218.2
WSe2 (mp-1821) <0 0 1> <1 1 1> 0.100 218.2
SiO2 (mp-6930) <1 0 1> <0 1 0> 0.103 106.7
Cu (mp-30) <1 1 1> <0 1 0> 0.115 293.4
NaCl (mp-22862) <1 1 1> <1 0 1> 0.117 333.1
LiNbO3 (mp-3731) <1 0 0> <0 1 0> 0.119 293.4
KTaO3 (mp-3614) <1 1 0> <1 0 0> 0.119 209.2
GdScO3 (mp-5690) <1 1 0> <1 0 1> 0.126 190.3
BN (mp-984) <0 0 1> <0 1 1> 0.131 175.0
ZnO (mp-2133) <0 0 1> <1 1 1> 0.140 218.2
Ga2O3 (mp-886) <0 1 0> <1 0 1> 0.142 142.7
BaTiO3 (mp-5986) <1 0 0> <1 1 1> 0.153 218.2
CdWO4 (mp-19387) <1 1 0> <1 1 0> 0.156 248.1
YAlO3 (mp-3792) <1 0 1> <0 1 1> 0.157 244.9
CdWO4 (mp-19387) <0 0 1> <0 0 1> 0.162 90.6
Al2O3 (mp-1143) <0 0 1> <0 0 1> 0.167 339.7
KP(HO2)2 (mp-23959) <0 1 1> <0 1 0> 0.167 106.7
Te2Mo (mp-602) <1 1 0> <0 1 1> 0.180 279.9
Ga2O3 (mp-886) <1 0 0> <0 0 1> 0.183 90.6
LiF (mp-1138) <1 1 0> <1 0 0> 0.185 209.2
TiO2 (mp-2657) <1 1 0> <0 0 1> 0.187 158.5
Ga2O3 (mp-886) <1 0 1> <0 1 1> 0.192 140.0
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
245 156 154 0 0 0
156 306 154 0 0 0
154 154 282 0 0 0
0 0 0 60 0 0
0 0 0 0 75 0
0 0 0 0 0 59
Compliance Tensor Sij (10-12Pa-1)
7.3 -2.4 -2.7 0 0 0
-2.4 5.3 -1.6 0 0 0
-2.7 -1.6 5.9 0 0 0
0 0 0 16.6 0 0
0 0 0 0 13.4 0
0 0 0 0 0 16.9
Shear Modulus GV
63 GPa
Bulk Modulus KV
196 GPa
Shear Modulus GR
62 GPa
Bulk Modulus KR
194 GPa
Shear Modulus GVRH
63 GPa
Bulk Modulus KVRH
195 GPa
Elastic Anisotropy
0.10
Poisson's Ratio
0.35

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
TaGeRh (mp-972224) 0.2446 0.000 3
CrFeP (mp-21495) 0.2311 0.000 3
CoMoP (mp-22262) 0.1778 0.000 3
NbGeIr (mp-22287) 0.2315 0.000 3
TiSiNi (mp-510409) 0.2359 0.000 3
Yb3In3Ge2Au (mp-981207) 0.5541 0.000 4
Na2LiGaAs2 (mp-9722) 0.5502 0.000 4
Na2LiAlP2 (mp-9719) 0.5774 0.000 4
KNa4SnSb3 (mp-6758) 0.5350 0.005 4
K3Na2SnBi3 (mp-568329) 0.5702 0.000 4
YbH2 (mp-864603) 0.2642 0.000 2
CaH2 (mp-23713) 0.2954 0.000 2
SrH2 (mp-23714) 0.2810 0.000 2
Co2P (mp-22204) 0.3037 0.000 2
BaH2 (mp-23715) 0.2509 0.000 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Co As Rh_pv
Final Energy/Atom
-6.6864 eV
Corrected Energy
-80.2362 eV
-80.2362 eV = -80.2362 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 43896
Submitted by
User remarks:
  • Cobalt rhodium arsenide (1/1/1)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)