Final Magnetic Moment0.021 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.119 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.180 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.44 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCu5Sn2Se7 + FeSe2 + Cu + SnSe |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI42m [121] |
HallI 4 2 |
Point Group42m |
Crystal Systemtetragonal |
Topological ClassificationTI*
|
SubclassificationSEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 33.3 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 92.4 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 166.3 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 266.1 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 33.3 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 92.4 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 232.9 |
Te2W (mp-22693) | <0 0 1> | <1 0 1> | 220.0 |
Te2W (mp-22693) | <0 1 0> | <1 0 0> | 326.7 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 266.1 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 166.3 |
TePb (mp-19717) | <1 1 0> | <1 1 0> | 184.8 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 33.3 |
Ag (mp-124) | <1 1 0> | <1 0 1> | 73.3 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 232.9 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 261.4 |
BN (mp-984) | <0 0 1> | <1 0 1> | 220.0 |
BN (mp-984) | <1 0 0> | <1 1 1> | 98.2 |
BN (mp-984) | <1 0 1> | <0 0 1> | 266.1 |
BN (mp-984) | <1 1 0> | <1 0 1> | 293.3 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 299.4 |
MoS2 (mp-1434) | <0 0 1> | <1 0 0> | 326.7 |
Al (mp-134) | <1 0 0> | <0 0 1> | 33.3 |
Al (mp-134) | <1 1 0> | <1 1 0> | 92.4 |
Al (mp-134) | <1 1 1> | <0 0 1> | 166.3 |
LiGaO2 (mp-5854) | <1 0 1> | <0 0 1> | 133.1 |
CdTe (mp-406) | <1 0 0> | <0 0 1> | 166.3 |
CdTe (mp-406) | <1 1 0> | <1 1 0> | 184.8 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 33.3 |
TeO2 (mp-2125) | <0 1 0> | <1 1 0> | 277.2 |
TeO2 (mp-2125) | <0 1 1> | <0 0 1> | 232.9 |
TeO2 (mp-2125) | <1 0 0> | <1 1 0> | 277.2 |
TeO2 (mp-2125) | <1 0 1> | <0 0 1> | 232.9 |
AlN (mp-661) | <0 0 1> | <1 1 1> | 294.7 |
AlN (mp-661) | <1 0 0> | <1 0 1> | 220.0 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 199.6 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 299.4 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 196.0 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 266.1 |
Fe3O4 (mp-19306) | <1 0 0> | <0 0 1> | 299.4 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 33.3 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 92.4 |
GaAs (mp-2534) | <1 1 1> | <1 1 1> | 294.7 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 166.3 |
BaF2 (mp-1029) | <1 1 0> | <1 0 1> | 220.0 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 166.3 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 166.3 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 196.0 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 232.9 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 332.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CaZn3Se4 (mp-1084796) | 0.1527 | 0.130 | 3 |
AlB3N4 (mp-1019379) | 0.1462 | 0.361 | 3 |
Cu3SbSe4 (mp-9814) | 0.0561 | 0.000 | 3 |
Cu3SbS4 (mp-5702) | 0.1374 | 0.000 | 3 |
Cu3SbS4 (mp-22171) | 0.1490 | 0.009 | 3 |
CdCu2SiTe4 (mp-1087540) | 0.0208 | 0.000 | 4 |
CoCu2SnS4 (mp-11770) | 0.0482 | 0.053 | 4 |
CoCu2SnSe4 (mp-1001058) | 0.0454 | 0.055 | 4 |
CoCu2SnS4 (mp-556504) | 0.0539 | 0.053 | 4 |
CoCu2SnSe4 (mp-11771) | 0.0491 | 0.055 | 4 |
FeO (mp-781777) | 0.2190 | 0.947 | 2 |
BC7 (mp-1080030) | 0.2254 | 0.243 | 2 |
BC5 (mp-1018649) | 0.2205 | 0.271 | 2 |
BC7 (mp-1079661) | 0.2323 | 0.239 | 2 |
BC5 (mp-1095514) | 0.1770 | 0.295 | 2 |
Sn (mp-949028) | 0.2198 | 0.012 | 1 |
Si (mp-971662) | 0.2180 | 0.062 | 1 |
C (mp-569517) | 0.3261 | 0.145 | 1 |
C (mp-569567) | 0.3282 | 0.144 | 1 |
Ge (mp-1091415) | 0.3216 | 0.008 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Fe_pv Cu_pv Sn_d Se |
Final Energy/Atom-4.4494 eV |
Corrected Energy-37.4829 eV
Uncorrected energy = -35.5949 eV
Composition-based energy adjustment (-0.472 eV/atom x 4.0 atoms) = -1.8880 eV
Corrected energy = -37.4829 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)