Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-1.025 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
9.89 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Pnma [62]
Hall
-P 2ac 2n
Point Group
mmm
Crystal System
orthorhombic

Electronic Structure

Topological data for ICSD ID 75009 from Topological Materials Database
Topological Classification
TI*
Subclassification
NLC
* Topological insulator
No Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Au (mp-81) <1 1 0> <0 1 0> 0.010 147.3
Ag (mp-124) <1 1 0> <0 1 0> 0.013 147.3
WS2 (mp-224) <1 1 0> <0 1 0> 0.023 235.7
KP(HO2)2 (mp-23959) <1 0 0> <0 1 1> 0.040 114.8
KP(HO2)2 (mp-23959) <0 1 0> <0 1 1> 0.043 76.5
Bi2Te3 (mp-34202) <0 0 1> <0 0 1> 0.044 292.7
BaTiO3 (mp-5986) <1 1 0> <0 1 1> 0.065 191.3
ZrO2 (mp-2858) <0 1 1> <1 0 1> 0.070 311.5
Ag (mp-124) <1 0 0> <1 0 0> 0.072 172.0
ZrO2 (mp-2858) <1 0 0> <0 1 1> 0.073 114.8
BN (mp-984) <1 0 0> <1 1 0> 0.084 193.4
TbScO3 (mp-31119) <1 1 0> <0 1 1> 0.089 191.3
Mg (mp-153) <1 0 1> <0 0 1> 0.094 243.9
LiTaO3 (mp-3666) <0 0 1> <1 0 1> 0.100 186.9
GaP (mp-2490) <1 1 0> <1 1 0> 0.110 128.9
CaF2 (mp-2741) <1 1 0> <1 1 0> 0.110 128.9
C (mp-66) <1 0 0> <0 1 1> 0.115 38.3
SiC (mp-11714) <1 1 1> <0 0 1> 0.115 219.5
Te2Mo (mp-602) <1 0 0> <0 0 1> 0.116 219.5
WSe2 (mp-1821) <1 0 0> <1 0 1> 0.123 249.2
BN (mp-984) <0 0 1> <0 0 1> 0.129 292.7
AlN (mp-661) <1 1 1> <0 1 1> 0.129 114.8
BaTiO3 (mp-5986) <0 0 1> <0 1 1> 0.137 191.3
GdScO3 (mp-5690) <1 1 0> <0 1 1> 0.137 191.3
DyScO3 (mp-31120) <1 1 0> <0 1 1> 0.137 191.3
SiO2 (mp-6930) <1 0 0> <1 0 1> 0.141 249.2
SiC (mp-8062) <1 1 1> <0 1 0> 0.147 265.2
LaAlO3 (mp-2920) <1 0 0> <1 0 0> 0.159 286.6
WSe2 (mp-1821) <1 0 1> <1 1 0> 0.169 257.8
Au (mp-81) <1 0 0> <1 0 0> 0.170 172.0
Te2W (mp-22693) <0 1 1> <0 1 0> 0.185 58.9
Ge3(BiO3)4 (mp-23560) <1 0 0> <0 1 1> 0.197 114.8
LiNbO3 (mp-3731) <0 0 1> <1 0 1> 0.201 186.9
Mg (mp-153) <1 0 0> <0 1 0> 0.203 265.2
LiTaO3 (mp-3666) <1 1 0> <1 0 1> 0.204 124.6
CdWO4 (mp-19387) <1 0 1> <0 0 1> 0.218 268.3
CdS (mp-672) <1 0 0> <1 0 0> 0.218 57.3
Te2Mo (mp-602) <0 0 1> <0 1 0> 0.218 88.4
TiO2 (mp-390) <0 0 1> <0 1 1> 0.219 114.8
KP(HO2)2 (mp-23959) <0 0 1> <0 1 1> 0.219 76.5
ZrO2 (mp-2858) <1 0 -1> <0 0 1> 0.241 73.2
C (mp-48) <1 0 0> <1 1 0> 0.251 193.4
AlN (mp-661) <0 0 1> <0 0 1> 0.260 170.7
NdGaO3 (mp-3196) <0 0 1> <0 0 1> 0.264 122.0
TiO2 (mp-2657) <1 0 1> <1 0 0> 0.266 229.3
Ni (mp-23) <1 1 0> <0 1 0> 0.269 88.4
Mg (mp-153) <1 1 1> <0 0 1> 0.271 268.3
Te2Mo (mp-602) <1 0 1> <0 0 1> 0.278 219.5
TiO2 (mp-2657) <0 0 1> <0 0 1> 0.288 195.1
LiAlO2 (mp-3427) <0 0 1> <0 0 1> 0.291 219.5
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
309 80 149 0 0 0
80 324 121 0 0 0
149 121 276 0 0 0
0 0 0 122 0 0
0 0 0 0 129 0
0 0 0 0 0 78
Compliance Tensor Sij (10-12Pa-1)
4.4 -0.2 -2.3 0 0 0
-0.2 3.7 -1.5 0 0 0
-2.3 -1.5 5.5 0 0 0
0 0 0 8.2 0 0
0 0 0 0 7.8 0
0 0 0 0 0 12.7
Shear Modulus GV
103 GPa
Bulk Modulus KV
179 GPa
Shear Modulus GR
96 GPa
Bulk Modulus KR
179 GPa
Shear Modulus GVRH
99 GPa
Bulk Modulus KVRH
179 GPa
Elastic Anisotropy
0.38
Poisson's Ratio
0.27

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
HfSiMo (mp-22258) 0.2965 0.000 3
YbFeGe (mp-628705) 0.4328 0.205 3
ZrNbP (mp-4500) 0.1346 0.000 3
HfVP (mp-1095442) 0.3797 0.000 3
HfGeMo (mp-1095449) 0.2983 0.000 3
KSr2Cd2Sb3 (mp-866639) 0.7373 0.000 4
US2 (mp-669500) 0.4446 0.000 2
PbCl2 (mp-619071) 0.4502 0.023 2
NaGe (mp-29657) 0.4588 0.000 2
Lu5Ga3 (mp-1094132) 0.4161 0.009 2
V2P (mp-20541) 0.3079 0.000 2
Rb (mp-640416) 0.4523 0.057 1
U (mp-1077335) 0.7482 0.282 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Hf_pv Nb_pv P
Final Energy/Atom
-9.5159 eV
Corrected Energy
-114.1912 eV
-114.1912 eV = -114.1912 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 75009
Submitted by
User remarks:
  • Hafnium niobium phosphide (1/1/1)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)