Final Magnetic Moment0.015 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.804 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.020 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density8.96 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToEr11Ge10 + Er3Ge4 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCmcm [63] |
Hall-C 2c 2 |
Point Groupmmm |
Crystal Systemorthorhombic |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 293.0 |
LaAlO3 (mp-2920) | <1 0 1> | <1 0 0> | 293.0 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 135.8 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 150.4 |
AlN (mp-661) | <1 0 1> | <1 0 1> | 123.3 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 209.3 |
CeO2 (mp-20194) | <1 1 0> | <0 1 0> | 300.7 |
CeO2 (mp-20194) | <1 1 1> | <0 1 0> | 267.3 |
GaAs (mp-2534) | <1 0 0> | <1 1 0> | 135.2 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 226.3 |
GaAs (mp-2534) | <1 1 0> | <0 1 0> | 183.8 |
CeO2 (mp-20194) | <1 0 0> | <1 1 0> | 90.1 |
GaN (mp-804) | <0 0 1> | <0 1 1> | 144.7 |
GaN (mp-804) | <1 1 0> | <0 1 1> | 241.2 |
BaF2 (mp-1029) | <1 0 0> | <0 1 0> | 367.5 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 167.4 |
SiO2 (mp-6930) | <1 0 0> | <1 1 1> | 255.5 |
SiO2 (mp-6930) | <1 1 1> | <0 1 0> | 217.2 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 135.8 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 150.4 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 293.0 |
SiO2 (mp-6930) | <0 0 1> | <0 1 1> | 193.0 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 250.6 |
SiO2 (mp-6930) | <1 1 0> | <1 1 1> | 191.6 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 1> | 61.6 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 0> | 300.7 |
DyScO3 (mp-31120) | <1 0 1> | <1 1 0> | 225.3 |
ZnSe (mp-1190) | <1 1 0> | <0 1 0> | 183.8 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 200.5 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 45.1 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 209.3 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 0> | 133.6 |
DyScO3 (mp-31120) | <1 1 1> | <0 1 0> | 284.0 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 181.0 |
InAs (mp-20305) | <1 1 0> | <0 1 0> | 217.2 |
InAs (mp-20305) | <1 1 1> | <0 1 1> | 193.0 |
CdS (mp-672) | <0 0 1> | <0 1 0> | 150.4 |
CdS (mp-672) | <1 0 0> | <0 1 0> | 116.9 |
CdS (mp-672) | <1 1 0> | <1 0 1> | 308.2 |
ZnSe (mp-1190) | <1 0 0> | <1 1 0> | 135.2 |
KTaO3 (mp-3614) | <1 1 1> | <0 1 0> | 200.5 |
Te2W (mp-22693) | <0 1 0> | <1 0 0> | 167.4 |
Te2W (mp-22693) | <0 1 1> | <0 0 1> | 181.0 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 135.8 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 209.3 |
LiF (mp-1138) | <1 0 0> | <1 1 0> | 135.2 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 183.8 |
LiF (mp-1138) | <1 1 1> | <0 1 0> | 200.5 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 316.8 |
Te2Mo (mp-602) | <0 0 1> | <0 1 0> | 250.6 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
152 | 34 | 73 | 0 | 0 | 0 |
34 | 189 | 20 | 0 | 0 | 0 |
73 | 20 | 149 | 0 | 0 | 0 |
0 | 0 | 0 | 32 | 0 | 0 |
0 | 0 | 0 | 0 | 96 | 0 |
0 | 0 | 0 | 0 | 0 | 48 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
8.8 | -1.2 | -4.2 | 0 | 0 | 0 |
-1.2 | 5.5 | -0.2 | 0 | 0 | 0 |
-4.2 | -0.2 | 8.8 | 0 | 0 | 0 |
0 | 0 | 0 | 30.9 | 0 | 0 |
0 | 0 | 0 | 0 | 10.4 | 0 |
0 | 0 | 0 | 0 | 0 | 20.7 |
Shear Modulus GV60 GPa |
Bulk Modulus KV82 GPa |
Shear Modulus GR50 GPa |
Bulk Modulus KR82 GPa |
Shear Modulus GVRH55 GPa |
Bulk Modulus KVRH82 GPa |
Elastic Anisotropy0.97 |
Poisson's Ratio0.23 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Hf2NiP (mp-5918) | 0.5253 | 0.000 | 3 |
Zr2CoP (mp-29152) | 0.5952 | 0.000 | 3 |
Zr2NiP (mp-29153) | 0.5935 | 0.000 | 3 |
Hf2CoP (mp-29154) | 0.5010 | 0.000 | 3 |
Ba2PtAu (mp-675690) | 0.6998 | 0.003 | 3 |
SrCa2In2Ge (mp-619206) | 0.5357 | 0.106 | 4 |
YGe (mp-9971) | 0.0562 | 0.004 | 2 |
DyGe (mp-20122) | 0.0539 | 0.000 | 2 |
TmGe (mp-998911) | 0.0270 | 0.025 | 2 |
TbGe (mp-1405) | 0.0632 | 0.000 | 2 |
HoGe (mp-16342) | 0.0183 | 0.017 | 2 |
Si (mp-1001113) | 0.6382 | 0.488 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Er_3 Ge_d |
Final Energy/Atom-5.3961 eV |
Corrected Energy-21.5844 eV
-21.5844 eV = -21.5844 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)