Final Magnetic Moment0.356 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-0.136 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.224 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.02 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToBaSn2 + Mn |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI4/mmm [139] |
Hall-I 4 2 |
Point Group4/mmm |
Crystal Systemtetragonal |
Topological ClassificationSM*
|
SubclassificationES†
|
Crossing TypeLine
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 178.5 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 283.2 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 290.1 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 178.5 |
LaAlO3 (mp-2920) | <1 1 0> | <1 0 1> | 121.7 |
AlN (mp-661) | <1 0 0> | <1 1 1> | 249.4 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 111.6 |
GaN (mp-804) | <0 0 1> | <1 0 1> | 243.5 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 290.1 |
GaAs (mp-2534) | <1 1 0> | <1 0 1> | 182.6 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 200.9 |
GaN (mp-804) | <1 0 0> | <1 0 1> | 182.6 |
GaN (mp-804) | <1 0 1> | <1 0 1> | 304.4 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 290.1 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 178.5 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 245.5 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 200.9 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 200.9 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 290.1 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 312.4 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 200.9 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 223.2 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 283.2 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 283.2 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 1> | 182.6 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 267.8 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 200.9 |
ZnSe (mp-1190) | <1 1 0> | <1 0 1> | 182.6 |
Te2W (mp-22693) | <0 1 1> | <0 0 1> | 290.1 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 200.9 |
YVO4 (mp-19133) | <1 1 0> | <1 1 1> | 249.4 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 312.4 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 223.2 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 1> | 182.6 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 283.2 |
CdS (mp-672) | <1 1 0> | <1 1 0> | 240.3 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 334.8 |
Ag (mp-124) | <1 1 1> | <1 1 0> | 240.3 |
Te2W (mp-22693) | <0 0 1> | <1 0 1> | 182.6 |
YVO4 (mp-19133) | <1 0 0> | <1 0 1> | 182.6 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 1 0> | 240.3 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 111.6 |
GaSe (mp-1943) | <1 1 1> | <1 1 0> | 240.3 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 44.6 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 226.5 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 89.3 |
BN (mp-984) | <1 1 0> | <1 0 1> | 304.4 |
GaSe (mp-1943) | <1 1 0> | <1 1 0> | 240.3 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 290.1 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 334.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Eu(CoSi)2 (mp-672294) | 0.0084 | 0.000 | 3 |
Pr(CoSi)2 (mp-5112) | 0.0534 | 0.000 | 3 |
Ce(CoAs)2 (mp-568182) | 0.0436 | 0.000 | 3 |
Nd(CoSi)2 (mp-4228) | 0.0104 | 0.000 | 3 |
Ca(CoSi)2 (mp-1070152) | 0.0226 | 0.000 | 3 |
La3Cu4(P2O)2 (mp-6309) | 0.4740 | 0.000 | 4 |
SrIn4 (mp-22466) | 0.3236 | 0.010 | 2 |
YbGa4 (mp-1088) | 0.3252 | 0.000 | 2 |
CaGa4 (mp-1976) | 0.3184 | 0.000 | 2 |
SrAl4 (mp-2775) | 0.2764 | 0.000 | 2 |
BaAl4 (mp-1903) | 0.2500 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ba_sv Mn_pv Sn_d |
Final Energy/Atom-5.7794 eV |
Corrected Energy-28.8969 eV
Uncorrected energy = -28.8969 eV
Corrected energy = -28.8969 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)