material

CaIn2Pd

ID:

mp-22717

DOI:

10.17188/1198920


Tags: Calcium palladium indium (1/1/2)

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.616 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
6.67 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Cmcm [63]
Hall
-C 2c 2
Point Group
mmm
Crystal System
orthorhombic

Electronic Structure

Topological data for ICSD ID 408881 from Topological Materials Database
Topological Classification
TI*
Subclassification
SEBR
* Topological insulator
Split Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
LiAlO2 (mp-3427) <1 0 0> <0 0 1> 0.003 331.1
GaN (mp-804) <1 0 0> <0 0 1> 0.003 236.5
Te2W (mp-22693) <0 0 1> <0 0 1> 0.011 331.1
SrTiO3 (mp-4651) <0 0 1> <1 0 0> 0.020 249.2
SrTiO3 (mp-4651) <1 1 0> <1 0 0> 0.022 249.2
WSe2 (mp-1821) <0 0 1> <0 1 0> 0.029 250.2
MoSe2 (mp-1634) <0 0 1> <0 1 0> 0.029 250.2
BN (mp-984) <0 0 1> <0 1 0> 0.038 71.5
CsI (mp-614603) <1 0 0> <1 0 0> 0.043 249.2
YAlO3 (mp-3792) <0 1 1> <1 0 1> 0.048 95.6
LiNbO3 (mp-3731) <0 0 1> <0 1 0> 0.057 71.5
ZrO2 (mp-2858) <1 0 0> <1 0 1> 0.058 286.8
AlN (mp-661) <1 1 1> <1 0 1> 0.060 286.8
Fe3O4 (mp-19306) <1 1 1> <0 1 0> 0.061 250.2
KCl (mp-23193) <1 1 1> <0 1 0> 0.062 71.5
MgO (mp-1265) <1 1 1> <1 0 0> 0.077 249.2
MgF2 (mp-1249) <1 1 0> <1 0 1> 0.078 286.8
Ni (mp-23) <1 0 0> <1 0 0> 0.080 249.2
TiO2 (mp-390) <1 0 1> <0 0 1> 0.083 236.5
Bi2Se3 (mp-541837) <0 0 1> <0 1 0> 0.089 286.0
Mg (mp-153) <1 0 1> <0 1 0> 0.093 286.0
GaN (mp-804) <1 1 0> <0 0 1> 0.100 236.5
YAlO3 (mp-3792) <1 1 0> <0 0 1> 0.100 331.1
ZrO2 (mp-2858) <0 1 1> <0 0 1> 0.100 236.5
Si (mp-149) <1 1 0> <0 1 0> 0.110 214.5
DyScO3 (mp-31120) <1 0 0> <1 1 0> 0.110 90.4
TePb (mp-19717) <1 1 0> <1 1 0> 0.110 180.9
CeO2 (mp-20194) <1 1 0> <0 1 0> 0.117 214.5
LiTaO3 (mp-3666) <0 0 1> <0 1 0> 0.122 71.5
DyScO3 (mp-31120) <0 1 0> <0 1 0> 0.127 214.5
NaCl (mp-22862) <1 1 0> <1 1 0> 0.132 90.4
BaF2 (mp-1029) <1 0 0> <0 1 1> 0.134 118.6
InP (mp-20351) <1 0 0> <0 1 1> 0.136 177.9
ZrO2 (mp-2858) <1 0 -1> <0 0 1> 0.140 141.9
ZrO2 (mp-2858) <0 1 0> <0 0 1> 0.148 331.1
BaTiO3 (mp-5986) <1 0 0> <0 1 0> 0.151 250.2
DyScO3 (mp-31120) <1 1 0> <1 0 0> 0.153 249.2
ZnO (mp-2133) <0 0 1> <0 1 0> 0.158 286.0
MgF2 (mp-1249) <1 0 0> <0 0 1> 0.158 236.5
BaF2 (mp-1029) <1 1 0> <0 0 1> 0.163 283.8
CaF2 (mp-2741) <1 1 1> <0 1 0> 0.168 107.2
Al (mp-134) <1 0 0> <0 1 0> 0.169 321.7
MgF2 (mp-1249) <0 0 1> <0 1 1> 0.170 177.9
GdScO3 (mp-5690) <0 1 0> <0 1 0> 0.174 178.7
KTaO3 (mp-3614) <1 1 0> <1 1 0> 0.175 90.4
TbScO3 (mp-31119) <1 0 0> <1 1 0> 0.178 90.4
TiO2 (mp-390) <1 1 1> <0 0 1> 0.178 331.1
C (mp-48) <1 1 0> <1 0 0> 0.184 166.2
InSb (mp-20012) <1 0 0> <0 1 1> 0.184 177.9
AlN (mp-661) <0 0 1> <0 0 1> 0.189 236.5
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
84 42 56 0 0 0
42 82 42 0 0 0
56 42 91 0 0 0
0 0 0 22 0 0
0 0 0 0 46 0
0 0 0 0 0 27
Compliance Tensor Sij (10-12Pa-1)
22.2 -5.7 -11.1 0 0 0
-5.7 17.4 -4.6 0 0 0
-11.1 -4.6 19.9 0 0 0
0 0 0 44.8 0 0
0 0 0 0 21.8 0
0 0 0 0 0 37.6
Shear Modulus GV
27 GPa
Bulk Modulus KV
60 GPa
Shear Modulus GR
24 GPa
Bulk Modulus KR
59 GPa
Shear Modulus GVRH
25 GPa
Bulk Modulus KVRH
59 GPa
Elastic Anisotropy
0.68
Poisson's Ratio
0.31

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
YbIn2Pd (mp-20240) 0.1904 0.000 3
CaIn2Pt (mp-21027) 0.1693 0.000 3
YbIn2Ni (mp-21223) 0.1807 0.000 3
EuIn2Pd (mp-21258) 0.1557 0.000 3
MgAl2Cu (mp-3034) 0.1516 0.000 3
Na2LiGaAs2 (mp-9722) 0.5524 0.000 4
LiYb2InGe2 (mp-977355) 0.6962 0.000 4
K3Na2SnBi3 (mp-568329) 0.6580 0.000 4
K2NaInSb2 (mp-505767) 0.6849 0.000 4
LiCa2InGe2 (mp-570850) 0.6865 0.000 4
ThSe2 (mp-7951) 0.6385 0.000 2
MgH2 (mp-23712) 0.5423 0.082 2
CaH2 (mp-23713) 0.6400 0.000 2
YbF3 (mp-22072) 0.6122 0.000 2
Li2S (mp-1125) 0.6149 0.056 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ca_sv In_d Pd
Final Energy/Atom
-3.7859 eV
Corrected Energy
-30.2876 eV
Uncorrected energy = -30.2876 eV Corrected energy = -30.2876 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 408881
Submitted by
User remarks:
  • Calcium palladium indium (1/1/2)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)