Final Magnetic Moment2.526 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom0.379 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.568 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.14 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCoGe2 + CoGe |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI4mm [107] |
HallI 4 2 |
Point Group4mm |
Crystal Systemtetragonal |
Topological ClassificationSM*
|
SubclassificationESFD†
|
Crossing TypePoint
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <1 0 0> | 327.4 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 63.9 |
GaN (mp-804) | <0 0 1> | <1 0 1> | 316.6 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 255.4 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 93.6 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 264.6 |
SiO2 (mp-6930) | <1 1 0> | <1 1 0> | 198.5 |
AlN (mp-661) | <1 0 0> | <1 1 0> | 330.8 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 191.6 |
AlN (mp-661) | <1 1 1> | <1 1 0> | 198.5 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 93.6 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 1> | 158.3 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 63.9 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 319.3 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 46.8 |
ZnSe (mp-1190) | <1 1 1> | <1 0 0> | 327.4 |
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 46.8 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 319.3 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 46.8 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 233.9 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 319.3 |
CdS (mp-672) | <1 0 0> | <1 0 1> | 316.6 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 233.9 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 255.4 |
LiF (mp-1138) | <1 0 0> | <1 1 0> | 66.2 |
SiO2 (mp-6930) | <1 0 0> | <1 1 1> | 275.8 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 319.3 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 127.7 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 46.8 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 280.7 |
Te2W (mp-22693) | <0 1 0> | <1 1 0> | 330.8 |
TePb (mp-19717) | <1 1 0> | <1 1 1> | 183.9 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 63.9 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 63.9 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 46.8 |
LiF (mp-1138) | <1 1 1> | <1 0 0> | 233.9 |
Ag (mp-124) | <1 1 1> | <1 0 0> | 233.9 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 255.4 |
YVO4 (mp-19133) | <1 1 0> | <1 0 1> | 316.6 |
BN (mp-984) | <0 0 1> | <0 0 1> | 191.6 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 140.3 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 198.5 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 319.3 |
Al (mp-134) | <1 1 0> | <1 0 0> | 46.8 |
GaSe (mp-1943) | <0 0 1> | <1 1 0> | 264.6 |
BN (mp-984) | <1 0 0> | <0 0 1> | 191.6 |
BN (mp-984) | <1 0 1> | <0 0 1> | 255.4 |
BN (mp-984) | <1 1 1> | <1 0 0> | 233.9 |
LiGaO2 (mp-5854) | <1 0 0> | <1 0 1> | 316.6 |
TeO2 (mp-2125) | <0 1 0> | <1 1 1> | 275.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Co Ge_d |
Final Energy/Atom-5.2761 eV |
Corrected Energy-63.3127 eV
-63.3127 eV = -63.3127 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)