material

TiCoGe

ID:

mp-22769

DOI:

10.17188/1198962


Tags: Titanium cobalt germanide (1/1/1) Cobalt germanium titanium (1/1/1)

Material Details

Final Magnetic Moment
0.317 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
FM
Formation Energy / Atom
-0.598 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
7.19 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P62m [189]
Hall
P 6 2
Point Group
6m2
Crystal System
hexagonal

Electronic Structure

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
SiC (mp-11714) <0 0 1> <0 0 1> 0.001 33.1
MgF2 (mp-1249) <1 0 0> <1 0 0> 0.002 116.1
SiC (mp-7631) <0 0 1> <0 0 1> 0.003 33.1
SiC (mp-8062) <1 1 1> <0 0 1> 0.008 33.1
Fe2O3 (mp-24972) <0 0 1> <0 0 1> 0.008 298.1
Ge3(BiO3)4 (mp-23560) <1 1 0> <1 1 0> 0.021 160.8
LiGaO2 (mp-5854) <1 1 0> <1 1 0> 0.023 241.2
C (mp-48) <1 1 0> <1 0 0> 0.027 301.7
GaN (mp-804) <1 0 0> <1 0 0> 0.030 185.7
GaSb (mp-1156) <1 0 0> <1 0 0> 0.034 116.1
Te2Mo (mp-602) <0 0 1> <0 0 1> 0.034 33.1
KTaO3 (mp-3614) <1 1 1> <1 1 0> 0.034 281.4
CdSe (mp-2691) <1 0 0> <1 0 0> 0.037 116.1
Ga2O3 (mp-886) <1 0 0> <1 0 0> 0.038 255.3
PbSe (mp-2201) <1 0 0> <1 0 0> 0.039 116.1
Ge (mp-32) <1 1 1> <0 0 1> 0.045 231.8
ZrO2 (mp-2858) <1 1 0> <0 0 1> 0.049 198.7
Al (mp-134) <1 1 1> <1 1 0> 0.050 281.4
C (mp-48) <0 0 1> <0 0 1> 0.053 99.4
SrTiO3 (mp-4651) <1 1 1> <1 1 1> 0.058 208.4
CdS (mp-672) <1 1 0> <1 0 0> 0.060 348.2
Ni (mp-23) <1 0 0> <1 0 0> 0.061 185.7
Ni (mp-23) <1 1 1> <1 1 0> 0.061 321.6
SiC (mp-7631) <1 0 0> <1 1 0> 0.068 281.4
TbScO3 (mp-31119) <1 0 1> <1 0 0> 0.070 278.5
DyScO3 (mp-31120) <1 0 1> <1 0 0> 0.071 278.5
InAs (mp-20305) <1 1 0> <1 1 0> 0.076 160.8
SiC (mp-8062) <1 0 0> <1 0 0> 0.091 116.1
ZnTe (mp-2176) <1 1 0> <1 1 0> 0.092 160.8
LiAlO2 (mp-3427) <1 0 1> <1 0 0> 0.092 255.3
TiO2 (mp-390) <1 1 1> <1 0 0> 0.096 162.5
TePb (mp-19717) <1 0 0> <1 0 0> 0.104 348.2
YAlO3 (mp-3792) <1 1 0> <1 0 0> 0.108 278.5
GaAs (mp-2534) <1 1 1> <0 0 1> 0.113 231.8
Cu (mp-30) <1 1 1> <0 0 1> 0.116 298.1
CdTe (mp-406) <1 0 0> <1 0 0> 0.119 348.2
ZnO (mp-2133) <1 1 0> <1 1 0> 0.121 120.6
TePb (mp-19717) <1 1 0> <1 1 0> 0.125 120.6
C (mp-66) <1 1 0> <1 1 0> 0.129 160.8
ZrO2 (mp-2858) <0 0 1> <1 0 0> 0.133 139.3
ZnTe (mp-2176) <1 0 0> <1 0 0> 0.136 116.1
InSb (mp-20012) <1 0 0> <1 0 0> 0.142 348.2
SiC (mp-8062) <1 1 0> <1 1 0> 0.144 80.4
InSb (mp-20012) <1 1 1> <0 0 1> 0.153 231.8
Te2Mo (mp-602) <1 0 1> <0 0 1> 0.155 165.6
InAs (mp-20305) <1 0 0> <1 0 0> 0.157 116.1
YVO4 (mp-19133) <1 0 1> <1 1 1> 0.162 208.4
ZnSe (mp-1190) <1 1 1> <0 0 1> 0.170 231.8
ZnO (mp-2133) <1 0 1> <1 0 0> 0.177 139.3
CdTe (mp-406) <1 1 1> <0 0 1> 0.181 231.8
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
263 106 138 0 0 0
106 263 138 0 0 0
138 138 253 0 0 0
0 0 0 94 0 0
0 0 0 0 94 0
0 0 0 0 0 79
Compliance Tensor Sij (10-12Pa-1)
5.5 -0.9 -2.5 0 0 0
-0.9 5.5 -2.5 0 0 0
-2.5 -2.5 6.7 0 0 0
0 0 0 10.7 0 0
0 0 0 0 10.7 0
0 0 0 0 0 12.7
Shear Modulus GV
80 GPa
Bulk Modulus KV
172 GPa
Shear Modulus GR
76 GPa
Bulk Modulus KR
171 GPa
Shear Modulus GVRH
78 GPa
Bulk Modulus KVRH
171 GPa
Elastic Anisotropy
0.21
Poisson's Ratio
0.30

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
ErAgPb (mp-16745) 0.0717 0.000 3
LuAgPb (mp-16747) 0.0814 0.000 3
TmAgSn (mp-2990) 0.0835 0.012 3
ErAgSn (mp-13265) 0.0767 0.012 3
ScCuGe (mp-1078430) 0.0756 0.000 3
Yb3In3Ge2Au (mp-981207) 0.2786 0.000 4
LiYb2InGe2 (mp-977355) 0.4659 0.000 4
Sr2LiInGe2 (mp-571617) 0.4501 0.000 4
LiCa2InGe2 (mp-570850) 0.4699 0.000 4
U3Al3NiRu2 (mp-1080528) 0.4446 0.087 4
Fe2P (mp-778) 0.4690 0.000 2
Pu2Co (mp-20026) 0.4913 0.060 2
BaI2 (mp-568536) 0.5789 0.006 2
BaCl2 (mp-567680) 0.5469 0.030 2
Co2As (mp-1079254) 0.5839 0.071 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ti_pv Co Ge_d
Final Energy/Atom
-7.1383 eV
Corrected Energy
-64.2449 eV
Uncorrected energy = -64.2449 eV Corrected energy = -64.2449 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 42943
  • 623629
Submitted by
User remarks:
  • Titanium cobalt germanide (1/1/1)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)