Final Magnetic Moment0.005 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.401 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.009 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.93 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToTe2Rh |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP3m1 [164] |
Hall-P 3 2" |
Point Group3m |
Crystal Systemtrigonal |
Topological ClassificationSM*
|
SubclassificationESFD†
|
Crossing TypePoint
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 153.0 |
LaAlO3 (mp-2920) | <1 1 0> | <1 0 0> | 131.1 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 153.0 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 109.3 |
AlN (mp-661) | <1 1 1> | <1 1 0> | 113.6 |
CeO2 (mp-20194) | <1 0 0> | <1 1 0> | 151.4 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 43.7 |
GaAs (mp-2534) | <1 1 0> | <1 1 1> | 281.6 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 54.4 |
LaAlO3 (mp-2920) | <1 0 0> | <1 0 1> | 205.9 |
LaAlO3 (mp-2920) | <1 0 1> | <1 0 0> | 153.0 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 174.8 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 217.6 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 153.0 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 87.4 |
GaN (mp-804) | <1 1 1> | <1 1 0> | 151.4 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 136.0 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 109.3 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 54.4 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 163.2 |
SiO2 (mp-6930) | <1 0 1> | <1 0 1> | 283.1 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 312.7 |
KCl (mp-23193) | <1 0 0> | <1 0 1> | 334.6 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 174.8 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 109.3 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 196.7 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 189.3 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 43.7 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 109.3 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 1> | 281.6 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 1> | 231.7 |
DyScO3 (mp-31120) | <1 1 0> | <1 1 0> | 302.8 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 0> | 284.1 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 258.4 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 109.3 |
SiO2 (mp-6930) | <1 1 0> | <1 1 0> | 189.3 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 217.6 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 339.9 |
InAs (mp-20305) | <1 1 0> | <1 0 1> | 334.6 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 258.4 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 163.2 |
ZnSe (mp-1190) | <1 1 0> | <1 1 1> | 281.6 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 54.4 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 65.6 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 1> | 154.4 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 258.4 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 176.8 |
CdS (mp-672) | <1 0 1> | <1 1 0> | 340.7 |
CdS (mp-672) | <1 1 0> | <1 1 0> | 151.4 |
CdS (mp-672) | <1 0 0> | <1 1 0> | 113.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Sb2TeSe2 (mp-571550) | 0.4547 | 0.037 | 3 |
Ge2Sb2Te5 (mp-3534) | 0.4203 | 0.023 | 3 |
Ca(InN)2 (mp-1029479) | 0.3192 | 0.012 | 3 |
GeBi4Te7 (mp-29644) | 0.4566 | 0.003 | 3 |
Ge3(BiTe3)2 (mp-540687) | 0.4459 | 0.023 | 3 |
Li2VO2F (mp-763844) | 0.6266 | 0.131 | 4 |
Na3Co2SbO6 (mp-561940) | 0.6992 | 0.015 | 4 |
Li2VO2F (mp-763174) | 0.6157 | 0.150 | 4 |
Li2VO2F (mp-763177) | 0.6791 | 0.146 | 4 |
Li2VO2F (mp-763175) | 0.6070 | 0.174 | 4 |
Bi2Pt (mp-569581) | 0.1225 | 0.037 | 2 |
CoTe2 (mp-1009641) | 0.2466 | 0.000 | 2 |
Te2Ir (mp-2285) | 0.0681 | 0.027 | 2 |
NiTe2 (mp-2578) | 0.1430 | 0.000 | 2 |
Te2Pt (mp-399) | 0.2009 | 0.000 | 2 |
Na6MnNi3(SbO6)2 (mp-1094109) | 0.6922 | 0.139 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Te Rh_pv |
Final Energy/Atom-4.9423 eV |
Corrected Energy-14.8269 eV
-14.8269 eV = -14.8269 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)