Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.652 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.079 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.55 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToInS + In |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPa3 [205] |
Hall-P 2ac 2ab 3 |
Point Groupm3 |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
In4SnSe4 (mp-628768) | 0.2909 | 0.000 | 3 |
Ga4GeS4 (mp-531297) | 0.2689 | 0.030 | 3 |
In4SnS4 (mp-646878) | 0.0542 | 0.000 | 3 |
In4GeS4 (mp-556528) | 0.2377 | 0.000 | 3 |
In4GeSe4 (mp-530545) | 0.4204 | 0.035 | 3 |
Li2Ga2GeS6 (mp-554782) | 0.6305 | 0.035 | 4 |
ZnAgPS4 (mp-558807) | 0.6279 | 0.000 | 4 |
In2Ag2GeSe6 (mp-505607) | 0.7224 | 0.018 | 4 |
In2Ag2GeS6 (mp-560386) | 0.7248 | 0.010 | 4 |
LiZnPS4 (mp-11175) | 0.7193 | 0.000 | 4 |
SiP2 (mp-9996) | 0.5317 | 0.000 | 2 |
GaTe (mp-542812) | 0.6101 | 0.003 | 2 |
GaS (mp-556742) | 0.6276 | 0.000 | 2 |
SiP (mp-2798) | 0.5623 | 0.000 | 2 |
SiAs (mp-1863) | 0.5657 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: In_d S |
Final Energy/Atom-3.7245 eV |
Corrected Energy-289.3934 eV
-289.3934 eV = -268.1626 eV (uncorrected energy) - 21.2307 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)