material

CsCl

ID:

mp-22865

DOI:

10.17188/1199031


Tags: Cesium chloride Cesium cjloride

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-2.207 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.048 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
3.75 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
CsCl
Band Gap
5.483 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Pm3m [221]
Hall
-P 4 2 3
Point Group
m3m
Crystal System
cubic

Electronic Structure

Topological data for ICSD ID 22173 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

Vibrational Properties

Reference for phonon calculations and visualization: Visualize with phononwebsite

Phonon dispersion

Density of States
Warning! These calculations were performed using a PBEsol exchange correlation functional in the framework of DFPT using the Abinit code. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
InP (mp-20351) <1 1 0> <1 1 0> 0.000 50.1
InP (mp-20351) <1 0 0> <1 0 0> 0.000 35.4
Ge(Bi3O5)4 (mp-23352) <1 1 0> <1 1 0> 0.001 150.3
NaCl (mp-22862) <1 1 0> <1 1 0> 0.001 275.6
Ni (mp-23) <1 0 0> <1 0 0> 0.003 159.4
MgF2 (mp-1249) <0 0 1> <1 0 0> 0.006 88.6
CdS (mp-672) <1 0 1> <1 0 0> 0.008 194.9
Fe2O3 (mp-24972) <0 0 1> <1 1 1> 0.009 92.1
InSb (mp-20012) <1 0 0> <1 0 0> 0.010 88.6
GdScO3 (mp-5690) <1 1 0> <1 0 0> 0.011 318.9
BN (mp-984) <0 0 1> <1 1 1> 0.011 214.8
ZnO (mp-2133) <0 0 1> <1 1 1> 0.012 122.7
MgF2 (mp-1249) <1 1 0> <1 1 0> 0.012 225.5
LiAlO2 (mp-3427) <1 0 0> <1 0 0> 0.014 265.7
CdTe (mp-406) <1 0 0> <1 0 0> 0.014 88.6
Te2W (mp-22693) <1 1 0> <1 1 0> 0.018 225.5
KP(HO2)2 (mp-23959) <1 0 0> <1 0 0> 0.018 230.3
AlN (mp-661) <1 1 1> <1 1 0> 0.019 200.4
BaF2 (mp-1029) <1 1 0> <1 1 0> 0.019 225.5
BaF2 (mp-1029) <1 0 0> <1 0 0> 0.021 159.4
ZrO2 (mp-2858) <0 1 0> <1 1 0> 0.022 225.5
KCl (mp-23193) <1 1 1> <1 1 1> 0.022 214.8
BaTiO3 (mp-5986) <1 0 0> <1 1 0> 0.024 50.1
Y3Fe5O12 (mp-19648) <1 0 0> <1 0 0> 0.026 159.4
Al2O3 (mp-1143) <1 0 1> <1 1 0> 0.029 200.4
BaTiO3 (mp-5986) <1 1 0> <1 0 0> 0.031 70.9
Ge3(BiO3)4 (mp-23560) <1 0 0> <1 0 0> 0.037 230.3
GaN (mp-804) <1 0 1> <1 0 0> 0.037 212.6
CdWO4 (mp-19387) <1 0 1> <1 1 0> 0.039 175.4
LiGaO2 (mp-5854) <0 0 1> <1 1 0> 0.040 225.5
Ga2O3 (mp-886) <0 1 0> <1 1 1> 0.042 214.8
LiGaO2 (mp-5854) <0 1 1> <1 0 0> 0.045 212.6
MoSe2 (mp-1634) <0 0 1> <1 1 1> 0.045 122.7
CdWO4 (mp-19387) <0 1 1> <1 1 0> 0.045 200.4
WSe2 (mp-1821) <0 0 1> <1 1 1> 0.046 122.7
CdS (mp-672) <0 0 1> <1 0 0> 0.046 124.0
ZnSe (mp-1190) <1 1 0> <1 1 0> 0.048 275.6
Cu (mp-30) <1 1 1> <1 1 1> 0.048 92.1
Cu (mp-30) <1 1 0> <1 1 0> 0.051 75.2
YAlO3 (mp-3792) <0 0 1> <1 1 0> 0.055 225.5
Mg (mp-153) <0 0 1> <1 1 0> 0.056 175.4
NdGaO3 (mp-3196) <1 1 0> <1 0 0> 0.058 301.2
MoS2 (mp-1434) <0 0 1> <1 1 0> 0.058 175.4
WS2 (mp-224) <0 0 1> <1 1 0> 0.058 175.4
NaCl (mp-22862) <1 0 0> <1 0 0> 0.058 159.4
Te2Mo (mp-602) <0 0 1> <1 0 0> 0.058 194.9
Al2O3 (mp-1143) <0 0 1> <1 1 0> 0.059 100.2
PbS (mp-21276) <1 1 0> <1 1 0> 0.060 50.1
CdWO4 (mp-19387) <1 0 0> <1 1 0> 0.062 125.3
Au (mp-81) <1 1 1> <1 1 1> 0.062 30.7
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
34 6 6 0 0 0
6 34 6 0 0 0
6 6 34 0 0 0
0 0 0 5 0 0
0 0 0 0 5 0
0 0 0 0 0 5
Compliance Tensor Sij (10-12Pa-1)
31.4 -4.7 -4.7 0 0 0
-4.7 31.4 -4.7 0 0 0
-4.7 -4.7 31.4 0 0 0
0 0 0 197.9 0 0
0 0 0 0 197.9 0
0 0 0 0 0 197.9
Shear Modulus GV
9 GPa
Bulk Modulus KV
15 GPa
Shear Modulus GR
7 GPa
Bulk Modulus KR
15 GPa
Shear Modulus GVRH
8 GPa
Bulk Modulus KVRH
15 GPa
Elastic Anisotropy
1.33
Poisson's Ratio
0.28

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
DyYHg2 (mp-971799) 0.0000 0.007 3
Si2HgTe (mp-631331) 0.0000 0.720 3
NpSnRh2 (mp-864834) 0.0000 0.127 3
TmCdPd2 (mp-865982) 0.0000 0.000 3
ErSnRu2 (mp-866285) 0.0000 0.000 3
TiFeCoAs (mp-998974) 0.0000 0.134 4
TiGaFeCo (mp-998964) 0.0000 0.000 4
TiFeCoSb (mp-998973) 0.0000 0.186 4
TiAlFeCo (mp-998980) 0.0000 0.000 4
MnGaFeCo (mp-999552) 0.0000 0.044 4
CeHg (mp-702) 0.0000 0.000 2
TmCu (mp-985) 0.0000 0.000 2
SrCd (mp-30496) 0.0000 0.000 2
HfIr (mp-1002122) 0.0000 0.042 2
DyAs (mp-1010161) 0.0000 0.476 2
Cu (mp-998890) 0.0000 0.037 1
Kr (mp-974400) 0.0000 0.002 1
H2 (mp-632250) 0.0000 2.271 1
Ge (mp-998883) 0.0000 0.339 1
U (mp-108) 0.0000 0.269 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Cs_sv Cl
Final Energy/Atom
-3.2722 eV
Corrected Energy
-7.1584 eV
Uncorrected energy = -6.5444 eV Composition-based energy adjustment (-0.614 eV/atom x 1.0 atoms) = -0.6140 eV Corrected energy = -7.1584 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 622366
  • 53847
  • 22173
  • 655032
  • 44289
  • 622367
Submitted by
User remarks:
  • Cesium chloride

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)