Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.803 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.87 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap2.824 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI4/mmm [139] |
Hall-I 4 2 |
Point Group4/mmm |
Crystal Systemtetragonal |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
DyScO3 (mp-31120) | <1 0 0> | <1 0 1> | 228.7 |
DyScO3 (mp-31120) | <1 1 0> | <1 1 1> | 250.1 |
DyScO3 (mp-31120) | <1 1 1> | <1 1 0> | 137.4 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 40.2 |
InAs (mp-20305) | <1 1 0> | <1 0 1> | 266.9 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 201.0 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 160.8 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 80.4 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 1> | 114.4 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 291.5 |
CdS (mp-672) | <0 0 1> | <1 0 1> | 190.6 |
CdS (mp-672) | <1 0 0> | <1 0 1> | 114.4 |
CdS (mp-672) | <1 0 1> | <1 0 1> | 266.9 |
CdS (mp-672) | <1 1 0> | <1 0 0> | 97.2 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 259.2 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 80.4 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 356.3 |
LiF (mp-1138) | <1 1 1> | <1 0 0> | 291.5 |
Te2W (mp-22693) | <0 0 1> | <1 1 1> | 200.1 |
Te2W (mp-22693) | <0 1 1> | <1 0 1> | 305.0 |
Te2W (mp-22693) | <1 0 0> | <1 1 1> | 100.1 |
Te2W (mp-22693) | <1 0 1> | <1 1 1> | 100.1 |
Te2W (mp-22693) | <1 1 0> | <1 0 0> | 226.8 |
Te2W (mp-22693) | <1 1 1> | <1 1 0> | 229.1 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 100.5 |
YVO4 (mp-19133) | <1 0 0> | <1 1 0> | 45.8 |
YVO4 (mp-19133) | <1 0 1> | <1 1 0> | 137.4 |
YVO4 (mp-19133) | <1 1 0> | <1 1 1> | 200.1 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 180.9 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 100.5 |
Te2Mo (mp-602) | <1 0 0> | <1 0 0> | 226.8 |
Te2Mo (mp-602) | <1 0 1> | <1 0 0> | 226.8 |
Te2Mo (mp-602) | <1 1 0> | <1 1 1> | 100.1 |
Te2Mo (mp-602) | <1 1 1> | <0 0 1> | 100.5 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 160.8 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 226.8 |
Ag (mp-124) | <1 1 1> | <1 0 0> | 291.5 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 140.7 |
Bi2Te3 (mp-34202) | <1 0 0> | <0 0 1> | 140.7 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 221.1 |
BN (mp-984) | <0 0 1> | <0 0 1> | 100.5 |
LaAlO3 (mp-2920) | <0 0 1> | <1 1 0> | 183.2 |
LaAlO3 (mp-2920) | <1 0 0> | <1 0 0> | 291.5 |
BN (mp-984) | <1 0 0> | <1 1 1> | 250.1 |
BN (mp-984) | <1 0 1> | <1 0 1> | 305.0 |
BN (mp-984) | <1 1 0> | <0 0 1> | 140.7 |
BN (mp-984) | <1 1 1> | <0 0 1> | 140.7 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 120.6 |
LiNbO3 (mp-3731) | <1 1 0> | <1 0 0> | 129.6 |
LiNbO3 (mp-3731) | <1 1 1> | <1 0 0> | 129.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
1.99 | -0.00 | 0.00 |
-0.00 | 1.99 | -0.00 |
0.00 | -0.00 | 3.31 |
Dielectric Tensor εij (total) |
||
---|---|---|
2.65 | -0.00 | 0.00 |
-0.00 | 2.65 | -0.00 |
0.00 | -0.00 | 4.67 |
Polycrystalline dielectric constant
εpoly∞
2.43
|
Polycrystalline dielectric constant
εpoly
3.32
|
Refractive Index n1.56 |
Potentially ferroelectric?Unknown |
Run TypeGGA |
Energy Cutoff700 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Xe F |
Final Energy/Atom-1.7618 eV |
Corrected Energy-5.2853 eV
-5.2853 eV = -5.2853 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)