Material Details

Final Magnetic Moment
7.001 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
FM
Formation Energy / Atom
-2.752 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.003 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
4.76 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
EuCl2
Band Gap
1.216 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Pnma [62]
Hall
-P 2ac 2n
Point Group
mmm
Crystal System
orthorhombic

Electronic Structure

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
KCl (mp-23193) <1 1 0> <0 1 0> 0.002 288.5
BN (mp-984) <1 0 1> <0 0 1> 0.004 240.8
Te2W (mp-22693) <0 0 1> <0 1 0> 0.006 288.5
C (mp-48) <0 0 1> <0 1 0> 0.007 247.3
ZnSe (mp-1190) <1 0 0> <0 1 0> 0.007 164.8
SrTiO3 (mp-4651) <1 0 0> <0 0 1> 0.009 309.6
GaAs (mp-2534) <1 0 0> <0 1 0> 0.010 164.8
BN (mp-984) <0 0 1> <0 1 1> 0.013 214.7
ZnO (mp-2133) <0 0 1> <0 0 1> 0.020 343.9
Ge (mp-32) <1 0 0> <0 1 0> 0.020 164.8
GaN (mp-804) <0 0 1> <0 1 0> 0.021 288.5
C (mp-66) <1 0 0> <0 1 0> 0.021 164.8
KCl (mp-23193) <1 1 1> <0 1 1> 0.025 214.7
Al (mp-134) <1 0 0> <0 1 0> 0.029 82.4
YAlO3 (mp-3792) <0 0 1> <0 0 1> 0.030 309.6
MgO (mp-1265) <1 0 0> <0 1 0> 0.030 164.8
TeO2 (mp-2125) <0 0 1> <1 1 0> 0.037 159.4
LiTaO3 (mp-3666) <0 0 1> <0 1 0> 0.037 164.8
LiF (mp-1138) <1 0 0> <0 1 0> 0.038 82.4
TiO2 (mp-390) <0 0 1> <0 0 1> 0.041 172.0
CdWO4 (mp-19387) <0 0 1> <1 0 0> 0.041 272.9
LiNbO3 (mp-3731) <0 0 1> <0 1 0> 0.041 164.8
LiGaO2 (mp-5854) <1 1 0> <0 0 1> 0.045 240.8
GdScO3 (mp-5690) <0 0 1> <1 1 0> 0.048 159.4
KTaO3 (mp-3614) <1 0 0> <0 1 0> 0.049 82.4
SiC (mp-8062) <1 1 0> <0 0 1> 0.050 240.8
SiO2 (mp-6930) <1 0 0> <1 0 1> 0.053 305.6
YVO4 (mp-19133) <0 0 1> <0 1 0> 0.054 206.1
TbScO3 (mp-31119) <1 1 0> <1 1 0> 0.056 318.8
DyScO3 (mp-31120) <1 1 0> <1 1 0> 0.058 318.8
Cu (mp-30) <1 0 0> <0 1 0> 0.062 206.1
CaCO3 (mp-3953) <1 0 1> <1 0 0> 0.067 272.9
NaCl (mp-22862) <1 0 0> <0 1 0> 0.069 164.8
WSe2 (mp-1821) <1 0 0> <1 0 1> 0.069 152.8
NdGaO3 (mp-3196) <0 0 1> <0 0 1> 0.075 309.6
Mg (mp-153) <0 0 1> <1 0 0> 0.078 272.9
TiO2 (mp-390) <1 0 1> <0 0 1> 0.078 240.8
CdWO4 (mp-19387) <0 1 0> <1 1 1> 0.078 260.4
MoS2 (mp-1434) <0 0 1> <1 0 0> 0.081 272.9
WS2 (mp-224) <0 0 1> <1 0 0> 0.081 272.9
InP (mp-20351) <1 0 0> <1 1 0> 0.082 318.8
Mg (mp-153) <1 1 1> <0 1 0> 0.084 329.7
GdScO3 (mp-5690) <1 1 0> <1 1 0> 0.085 318.8
AlN (mp-661) <1 1 1> <0 0 1> 0.085 309.6
Fe2O3 (mp-24972) <1 1 0> <0 1 0> 0.087 123.6
BaF2 (mp-1029) <1 0 0> <1 1 0> 0.088 79.7
BaTiO3 (mp-5986) <0 0 1> <1 1 0> 0.091 79.7
MgAl2O4 (mp-3536) <1 0 0> <0 1 1> 0.092 268.4
ZrO2 (mp-2858) <1 1 -1> <1 0 1> 0.092 229.2
TeO2 (mp-2125) <0 1 1> <0 0 1> 0.096 309.6
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
53 19 21 0 0 0
19 42 13 0 0 0
21 13 37 0 0 0
0 0 0 8 0 0
0 0 0 0 19 0
0 0 0 0 0 6
Compliance Tensor Sij (10-12Pa-1)
26.7 -8.7 -11.7 0 0 0
-8.7 29.5 -5.6 0 0 0
-11.7 -5.6 35.2 0 0 0
0 0 0 125.2 0 0
0 0 0 0 53.5 0
0 0 0 0 0 156.6
Shear Modulus GV
12 GPa
Bulk Modulus KV
26 GPa
Shear Modulus GR
10 GPa
Bulk Modulus KR
25 GPa
Shear Modulus GVRH
11 GPa
Bulk Modulus KVRH
26 GPa
Elastic Anisotropy
0.89
Poisson's Ratio
0.31

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
KRbS (mp-28760) 0.5228 0.008 3
MoPRu (mp-22451) 0.5508 0.000 3
PbBrCl (mp-22997) 0.3938 0.010 3
VAsRh (mp-934092) 0.4453 0.002 3
VAsRh (mp-20395) 0.4228 0.002 3
Na2LiGaAs2 (mp-9722) 0.7445 0.000 4
BaI2 (mp-23260) 0.1529 0.000 2
BaBr2 (mp-27456) 0.1951 0.000 2
ZrO2 (mp-963) 0.1961 0.103 2
CaF2 (mp-10464) 0.1473 0.052 2
HfO2 (mp-741) 0.1754 0.139 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Eu Cl
Final Energy/Atom
-7.0182 eV
Corrected Energy
-89.1303 eV
Uncorrected energy = -84.2183 eV Composition-based energy adjustment (-0.614 eV/atom x 8.0 atoms) = -4.9120 eV Corrected energy = -89.1303 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 22039
  • 60318
Submitted by
User remarks:
  • Europium(II) chloride

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)