Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.676 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.20 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap2.030 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP4/mmm [123] |
Hall-P 4 2 |
Point Group4/mmm |
Crystal Systemtetragonal |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | elastic energy [meV] | MCIA† [Å2] |
---|---|---|---|---|
WS2 (mp-224) | <1 1 0> | <1 0 1> | 0.000 | 235.5 |
KP(HO2)2 (mp-23959) | <0 0 1> | <1 0 0> | 0.000 | 151.4 |
MoS2 (mp-1434) | <1 0 0> | <1 0 0> | 0.001 | 272.5 |
MgO (mp-1265) | <1 1 0> | <1 1 0> | 0.001 | 128.5 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 0.001 | 90.8 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 0.005 | 242.2 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 0.006 | 252.5 |
Mg (mp-153) | <1 0 0> | <1 0 0> | 0.006 | 151.4 |
WS2 (mp-224) | <1 1 1> | <1 0 1> | 0.008 | 235.5 |
YAlO3 (mp-3792) | <0 1 0> | <1 0 0> | 0.008 | 272.5 |
PbS (mp-21276) | <1 1 0> | <1 1 0> | 0.009 | 256.9 |
NdGaO3 (mp-3196) | <1 1 1> | <1 0 0> | 0.009 | 272.5 |
PbS (mp-21276) | <1 0 0> | <1 0 0> | 0.010 | 181.7 |
BaTiO3 (mp-5986) | <0 0 1> | <1 0 0> | 0.010 | 242.2 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 0.010 | 212.0 |
TbScO3 (mp-31119) | <1 1 0> | <0 0 1> | 0.011 | 252.5 |
AlN (mp-661) | <0 0 1> | <1 1 1> | 0.011 | 264.8 |
ZnO (mp-2133) | <0 0 1> | <1 0 1> | 0.012 | 235.5 |
Te2Mo (mp-602) | <0 0 1> | <1 0 1> | 0.013 | 176.6 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 0.014 | 151.4 |
Al (mp-134) | <1 0 0> | <1 0 0> | 0.015 | 242.2 |
KP(HO2)2 (mp-23959) | <0 1 0> | <1 0 0> | 0.015 | 151.4 |
C (mp-48) | <0 0 1> | <1 0 0> | 0.015 | 212.0 |
Mg (mp-153) | <0 0 1> | <1 0 1> | 0.016 | 235.5 |
WSe2 (mp-1821) | <1 0 0> | <1 1 1> | 0.017 | 198.6 |
C (mp-66) | <1 0 0> | <0 0 1> | 0.022 | 50.5 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 0.023 | 202.0 |
SiC (mp-11714) | <1 1 0> | <1 1 0> | 0.025 | 214.1 |
CdWO4 (mp-19387) | <0 0 1> | <1 1 0> | 0.025 | 214.1 |
ZnO (mp-2133) | <1 0 0> | <1 0 0> | 0.026 | 121.1 |
BaTiO3 (mp-5986) | <1 1 1> | <1 1 1> | 0.026 | 198.6 |
MoS2 (mp-1434) | <0 0 1> | <1 0 1> | 0.028 | 235.5 |
WS2 (mp-224) | <0 0 1> | <1 0 1> | 0.028 | 235.5 |
SiC (mp-8062) | <1 1 1> | <1 0 1> | 0.028 | 235.5 |
SrTiO3 (mp-4651) | <1 1 0> | <0 0 1> | 0.028 | 252.5 |
BaTiO3 (mp-5986) | <1 0 0> | <1 1 0> | 0.033 | 85.6 |
TiO2 (mp-390) | <1 1 0> | <1 0 0> | 0.033 | 212.0 |
MgF2 (mp-1249) | <1 1 0> | <1 1 1> | 0.034 | 331.0 |
MgF2 (mp-1249) | <1 0 1> | <1 0 0> | 0.034 | 212.0 |
BaTiO3 (mp-5986) | <1 1 0> | <1 0 0> | 0.034 | 121.1 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 0.036 | 212.0 |
Al (mp-134) | <1 1 1> | <1 1 1> | 0.042 | 198.6 |
GdScO3 (mp-5690) | <1 1 0> | <0 0 1> | 0.043 | 252.5 |
Ni (mp-23) | <1 1 0> | <1 0 1> | 0.043 | 176.6 |
GaSe (mp-1943) | <0 0 1> | <1 1 1> | 0.044 | 198.6 |
MoSe2 (mp-1634) | <0 0 1> | <1 0 0> | 0.044 | 333.1 |
WSe2 (mp-1821) | <0 0 1> | <1 0 0> | 0.044 | 333.1 |
C (mp-48) | <1 0 1> | <1 1 1> | 0.045 | 198.6 |
KP(HO2)2 (mp-23959) | <0 1 1> | <1 0 0> | 0.045 | 212.0 |
BN (mp-984) | <1 0 1> | <1 1 1> | 0.046 | 198.6 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
22 | 6 | 6 | 0 | 0 | 0 |
6 | 26 | 4 | 0 | 0 | 0 |
6 | 4 | 26 | 0 | 0 | 0 |
0 | 0 | 0 | 5 | 0 | 0 |
0 | 0 | 0 | 0 | 5 | 0 |
0 | 0 | 0 | 0 | 0 | 5 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
50.1 | -9.2 | -9.2 | 0 | 0 | 0 |
-9.2 | 40.6 | -4.8 | 0 | 0 | 0 |
-9.2 | -4.8 | 40.6 | 0 | 0 | 0 |
0 | 0 | 0 | 196.5 | 0 | 0 |
0 | 0 | 0 | 0 | 192.8 | 0 |
0 | 0 | 0 | 0 | 0 | 192.8 |
Shear Modulus GV7 GPa |
Bulk Modulus KV12 GPa |
Shear Modulus GR6 GPa |
Bulk Modulus KR12 GPa |
Shear Modulus GVRH7 GPa |
Bulk Modulus KVRH12 GPa |
Elastic Anisotropy0.55 |
Poisson's Ratio0.26 |
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
2.86 | 0.00 | 0.00 |
0.00 | 3.57 | 0.00 |
0.00 | 0.00 | 3.57 |
Dielectric Tensor εij (total) |
||
---|---|---|
2.86 | 0.00 | 0.00 |
0.00 | 18.99 | 0.00 |
0.00 | 0.00 | 18.99 |
Polycrystalline dielectric constant
εpoly∞
3.34
|
Polycrystalline dielectric constant
εpoly
13.61
|
Refractive Index n1.83 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
K2PtBr4 (mp-27243) | 0.0320 | 0.006 | 3 |
Tl2PdCl4 (mp-29889) | 0.0863 | 0.000 | 3 |
K2PdBr4 (mp-27138) | 0.0745 | 0.000 | 3 |
Rb2PdCl4 (mp-1025201) | 0.1646 | 0.000 | 3 |
K2PdCl4 (mp-22956) | 0.0807 | 0.000 | 3 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: K_sv Pt Cl |
Final Energy/Atom-3.5769 eV |
Corrected Energy-27.4946 eV
Uncorrected energy = -25.0386 eV
Composition-based energy adjustment (-0.614 eV/atom x 4.0 atoms) = -2.4560 eV
Corrected energy = -27.4946 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)