Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.796 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.52 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap1.496 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCmcm [63] |
Hall-C 2c 2 |
Point Groupmmm |
Crystal Systemorthorhombic |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CeO2 (mp-20194) | <1 0 0> | <1 1 0> | 92.4 |
CeO2 (mp-20194) | <1 1 0> | <0 1 0> | 169.1 |
GaN (mp-804) | <1 1 1> | <0 1 0> | 338.1 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 56.4 |
SiO2 (mp-6930) | <1 0 1> | <0 1 1> | 142.1 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 92.4 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 0> | 56.4 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 0> | 92.4 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 219.5 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 92.4 |
KTaO3 (mp-3614) | <1 0 0> | <1 1 0> | 277.1 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 92.4 |
KTaO3 (mp-3614) | <1 1 1> | <0 1 0> | 56.4 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 92.4 |
LiF (mp-1138) | <1 1 1> | <0 1 0> | 56.4 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 281.8 |
Te2Mo (mp-602) | <1 0 1> | <1 1 0> | 277.1 |
Ag (mp-124) | <1 0 0> | <1 1 0> | 277.1 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 338.1 |
GaAs (mp-2534) | <1 0 0> | <0 1 0> | 225.4 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 92.4 |
BN (mp-984) | <1 0 1> | <0 0 1> | 260.9 |
BN (mp-984) | <1 1 0> | <0 1 0> | 225.4 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 146.4 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 146.4 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 219.5 |
MoS2 (mp-1434) | <0 0 1> | <0 1 0> | 281.8 |
Al (mp-134) | <1 1 1> | <0 1 0> | 56.4 |
ZnSe (mp-1190) | <1 0 0> | <0 1 0> | 225.4 |
LiGaO2 (mp-5854) | <0 0 1> | <0 1 0> | 56.4 |
LiGaO2 (mp-5854) | <0 1 1> | <0 1 0> | 169.1 |
LiGaO2 (mp-5854) | <1 0 0> | <1 0 0> | 73.2 |
LiGaO2 (mp-5854) | <1 0 1> | <1 1 0> | 92.4 |
TeO2 (mp-2125) | <0 1 0> | <1 1 0> | 277.1 |
TeO2 (mp-2125) | <0 1 1> | <0 1 0> | 225.4 |
TeO2 (mp-2125) | <1 0 0> | <1 1 0> | 277.1 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 130.5 |
TePb (mp-19717) | <1 1 0> | <1 1 0> | 184.7 |
TeO2 (mp-2125) | <1 0 1> | <0 1 0> | 225.4 |
SiC (mp-7631) | <0 0 1> | <0 1 0> | 338.1 |
Al (mp-134) | <1 0 0> | <1 1 0> | 277.1 |
Al (mp-134) | <1 1 0> | <1 1 0> | 92.4 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 130.5 |
MgO (mp-1265) | <1 0 0> | <0 1 0> | 338.1 |
LiGaO2 (mp-5854) | <1 1 0> | <0 1 0> | 338.1 |
CdTe (mp-406) | <1 1 0> | <1 1 0> | 184.7 |
TeO2 (mp-2125) | <0 0 1> | <1 0 0> | 219.5 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 260.9 |
TiO2 (mp-2657) | <0 0 1> | <1 1 0> | 277.1 |
TiO2 (mp-2657) | <1 0 1> | <0 1 0> | 281.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ca3SnH2 (mp-984605) | 0.3514 | 0.000 | 3 |
CsCu2I3 (mp-23431) | 0.3296 | 0.011 | 3 |
KFe2S3 (mp-22035) | 0.4400 | 0.000 | 3 |
BaFe2S3 (mp-22739) | 0.4601 | 0.055 | 3 |
KFe2Se3 (mp-1095516) | 0.3920 | 0.027 | 3 |
Cs2MnSnTe4 (mp-22235) | 0.6632 | 0.000 | 4 |
CsCu2ICl2 (mp-579536) | 0.6336 | 0.000 | 4 |
Ba2V(CuS2)3 (mp-560493) | 0.5612 | 0.038 | 4 |
Rb2TaCuS4 (mp-11923) | 0.6726 | 0.000 | 4 |
Rb2NbCuS4 (mp-15221) | 0.6741 | 0.000 | 4 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Cs_sv Cu_pv Br |
Final Energy/Atom-3.1300 eV |
Corrected Energy-40.7637 eV
Uncorrected energy = -37.5597 eV
Composition-based energy adjustment (-0.534 eV/atom x 6.0 atoms) = -3.2040 eV
Corrected energy = -40.7637 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)