Final Magnetic Moment0.004 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.332 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.071 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.13 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCsAuCl3 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPm3m [221] |
Hall-P 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Topological ClassificationTI*
|
SubclassificationSEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <1 0 0> | 244.2 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 307.0 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 244.2 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 135.7 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 115.1 |
LaAlO3 (mp-2920) | <0 0 1> | <1 1 1> | 329.0 |
AlN (mp-661) | <0 0 1> | <1 1 1> | 329.0 |
AlN (mp-661) | <1 0 1> | <1 1 0> | 191.9 |
AlN (mp-661) | <1 1 1> | <1 1 0> | 307.0 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 345.4 |
BaF2 (mp-1029) | <1 0 0> | <1 1 1> | 235.0 |
GaN (mp-804) | <0 0 1> | <1 1 1> | 141.0 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 81.4 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 115.1 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 307.0 |
SiO2 (mp-6930) | <1 0 1> | <1 1 0> | 307.0 |
SiO2 (mp-6930) | <1 1 1> | <1 1 0> | 153.5 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 217.1 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 115.1 |
DyScO3 (mp-31120) | <0 1 0> | <1 1 0> | 345.4 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 244.2 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 352.8 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 153.5 |
InAs (mp-20305) | <1 1 1> | <1 1 1> | 188.0 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 135.7 |
GdScO3 (mp-5690) | <0 0 1> | <1 1 0> | 191.9 |
GdScO3 (mp-5690) | <0 1 0> | <1 1 0> | 345.4 |
GdScO3 (mp-5690) | <1 1 0> | <1 0 0> | 135.7 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 298.5 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 135.7 |
KTaO3 (mp-3614) | <1 1 1> | <1 1 1> | 188.0 |
Mg (mp-153) | <0 0 1> | <1 1 1> | 141.0 |
Mg (mp-153) | <1 0 0> | <1 0 0> | 81.4 |
Mg (mp-153) | <1 1 0> | <1 1 0> | 115.1 |
Mg (mp-153) | <1 1 1> | <1 0 0> | 244.2 |
KP(HO2)2 (mp-23959) | <0 0 1> | <1 0 0> | 217.1 |
CdS (mp-672) | <0 0 1> | <1 1 1> | 47.0 |
CdS (mp-672) | <1 0 0> | <1 1 0> | 268.6 |
CdS (mp-672) | <1 0 1> | <1 1 0> | 191.9 |
CdS (mp-672) | <1 1 0> | <1 1 0> | 153.5 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 135.7 |
LaF3 (mp-905) | <0 0 1> | <1 1 1> | 47.0 |
LaF3 (mp-905) | <1 0 0> | <1 0 0> | 54.3 |
LaF3 (mp-905) | <1 1 0> | <1 1 1> | 94.0 |
PbS (mp-21276) | <1 0 0> | <1 0 0> | 352.8 |
PbS (mp-21276) | <1 1 0> | <1 1 0> | 153.5 |
PbS (mp-21276) | <1 1 1> | <1 1 1> | 188.0 |
LiF (mp-1138) | <1 1 1> | <1 1 1> | 329.0 |
Te2W (mp-22693) | <0 0 1> | <1 1 1> | 329.0 |
Te2W (mp-22693) | <1 1 0> | <1 1 0> | 115.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
InBiO3 (mp-545379) | 0.0025 | 0.496 | 3 |
BaIrO3 (mp-5660) | 0.0021 | 0.143 | 3 |
SrTcO3 (mp-1068333) | 0.0021 | 0.000 | 3 |
LaFeO3 (mp-556561) | 0.0025 | 0.130 | 3 |
SrMoO3 (mp-1068267) | 0.0025 | 0.087 | 3 |
Ba2ScSbO6 (mp-20709) | 0.0033 | 2.196 | 4 |
Cs2LiYCl6 (mp-567652) | 0.0024 | 0.000 | 4 |
Sr2GaSbO6 (mp-6065) | 0.0000 | 0.039 | 4 |
Ba2YSbO6 (mp-14226) | 0.0033 | 2.082 | 4 |
Cs2NaLaBr6 (mp-1079096) | 0.0026 | 0.007 | 4 |
Ca3Sb2 (mp-1013546) | 0.0033 | 0.421 | 2 |
Ba3Sb2 (mp-1013582) | 0.0033 | 0.409 | 2 |
Ca3Bi2 (mp-1013735) | 0.0033 | 0.366 | 2 |
Sr3Sb2 (mp-1013583) | 0.0033 | 0.381 | 2 |
Ni4N (mp-20839) | 0.0033 | 2.021 | 2 |
BaLaMgBiO6 (mp-41414) | 0.0465 | 0.096 | 5 |
BaLaMgNbO6 (mp-39288) | 0.0694 | 0.090 | 5 |
SrLaNbZnO6 (mp-41918) | 0.0643 | 0.126 | 5 |
SrLaMnCoO6 (mp-40761) | 0.0381 | 0.247 | 5 |
Sr6Ca2MnFe7O24 (mp-1075969) | 0.0468 | 0.021 | 5 |
Na5Ca2Ce3Ti8Nb2O30 (mp-721094) | 0.7376 | 0.065 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Cs_sv Au Cl |
Final Energy/Atom-2.9179 eV |
Corrected Energy-16.4316 eV
Uncorrected energy = -14.5896 eV
Composition-based energy adjustment (-0.614 eV/atom x 3.0 atoms) = -1.8420 eV
Corrected energy = -16.4316 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)