material

CsPbCl3

ID:

mp-23037

DOI:

10.17188/1199184


Tags: High pressure experimental phase Cesium lead(II) trichloride Cesium lead chloride Cesium lead trichloride

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-1.869 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.007 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
3.93 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
CsPbCl3
Band Gap
2.395 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Pm3m [221]
Hall
-P 4 2 3
Point Group
m3m
Crystal System
cubic

Electronic Structure

Topological data for ICSD ID 29072 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Ni (mp-23) <1 1 0> <1 1 0> 0.001 139.5
CdTe (mp-406) <1 1 1> <1 1 1> 0.002 227.8
CdTe (mp-406) <1 1 0> <1 1 0> 0.002 186.0
ZnSe (mp-1190) <1 1 1> <1 1 1> 0.002 56.9
ZnSe (mp-1190) <1 1 0> <1 1 0> 0.002 46.5
ZnSe (mp-1190) <1 0 0> <1 0 0> 0.003 32.9
InSb (mp-20012) <1 1 1> <1 1 1> 0.004 227.8
InSb (mp-20012) <1 1 0> <1 1 0> 0.004 186.0
LaAlO3 (mp-2920) <1 0 1> <1 1 1> 0.004 227.8
AlN (mp-661) <0 0 1> <1 1 1> 0.006 227.8
KCl (mp-23193) <1 0 0> <1 0 0> 0.008 164.4
GaAs (mp-2534) <1 1 1> <1 1 1> 0.009 56.9
GaAs (mp-2534) <1 1 0> <1 1 0> 0.009 46.5
Cu (mp-30) <1 0 0> <1 0 0> 0.010 65.8
GaAs (mp-2534) <1 0 0> <1 0 0> 0.011 32.9
YVO4 (mp-19133) <0 0 1> <1 0 0> 0.015 263.0
CdWO4 (mp-19387) <0 1 1> <1 1 0> 0.017 325.5
Al (mp-134) <1 1 0> <1 1 0> 0.017 46.5
BN (mp-984) <0 0 1> <1 1 1> 0.018 170.8
AlN (mp-661) <1 0 1> <1 0 0> 0.018 197.3
Al (mp-134) <1 0 0> <1 0 0> 0.020 32.9
MgF2 (mp-1249) <1 1 0> <1 1 0> 0.021 186.0
MgO (mp-1265) <1 0 0> <1 0 0> 0.022 164.4
TiO2 (mp-390) <0 0 1> <1 0 0> 0.025 131.5
WSe2 (mp-1821) <0 0 1> <1 0 0> 0.026 230.1
MoSe2 (mp-1634) <0 0 1> <1 0 0> 0.026 230.1
Ge (mp-32) <1 1 1> <1 1 1> 0.028 56.9
Ge (mp-32) <1 1 0> <1 1 0> 0.029 46.5
MgO (mp-1265) <1 1 0> <1 1 0> 0.030 279.0
LiF (mp-1138) <1 1 1> <1 0 0> 0.031 230.1
Te2Mo (mp-602) <0 0 1> <1 1 1> 0.034 227.8
Ge (mp-32) <1 0 0> <1 0 0> 0.034 32.9
SiO2 (mp-6930) <1 0 1> <1 1 0> 0.037 139.5
DyScO3 (mp-31120) <0 0 1> <1 1 0> 0.038 93.0
KTaO3 (mp-3614) <1 1 0> <1 1 0> 0.039 46.5
TbScO3 (mp-31119) <0 1 0> <1 0 0> 0.042 131.5
AlN (mp-661) <1 0 0> <1 1 1> 0.043 284.7
KTaO3 (mp-3614) <1 0 0> <1 0 0> 0.045 32.9
DyScO3 (mp-31120) <0 1 0> <1 0 0> 0.046 131.5
TeO2 (mp-2125) <1 0 0> <1 1 0> 0.047 139.5
TeO2 (mp-2125) <1 0 1> <1 0 0> 0.055 230.1
NaCl (mp-22862) <1 1 1> <1 1 1> 0.058 56.9
LiF (mp-1138) <1 1 0> <1 1 0> 0.059 46.5
NaCl (mp-22862) <1 1 0> <1 1 0> 0.062 46.5
C (mp-48) <1 0 1> <1 0 0> 0.065 263.0
TiO2 (mp-2657) <1 1 1> <1 1 0> 0.066 325.5
MgAl2O4 (mp-3536) <1 1 0> <1 1 0> 0.067 93.0
LiF (mp-1138) <1 0 0> <1 0 0> 0.069 32.9
ZnO (mp-2133) <1 0 0> <1 0 0> 0.070 263.0
GdScO3 (mp-5690) <1 0 0> <1 1 0> 0.071 46.5
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
49 8 8 0 0 0
8 49 8 0 0 0
8 8 49 0 0 0
0 0 0 5 0 0
0 0 0 0 5 0
0 0 0 0 0 5
Compliance Tensor Sij (10-12Pa-1)
21.5 -2.9 -2.9 0 0 0
-2.9 21.5 -2.9 0 0 0
-2.9 -2.9 21.5 0 0 0
0 0 0 189.3 0 0
0 0 0 0 189.3 0
0 0 0 0 0 189.3
Shear Modulus GV
11 GPa
Bulk Modulus KV
21 GPa
Shear Modulus GR
8 GPa
Bulk Modulus KR
21 GPa
Shear Modulus GVRH
9 GPa
Bulk Modulus KVRH
21 GPa
Elastic Anisotropy
2.56
Poisson's Ratio
0.31

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Ca3BiSb (mp-1013733) 0.0000 0.320 3
Sr3SbAs (mp-1013541) 0.0000 0.619 3
Ba3SbAs (mp-1013562) 0.0000 0.229 3
Lu3AlN (mp-1017627) 0.0000 0.000 3
Sr3SbAs (mp-1013561) 0.0000 0.186 3
Ba2VFeO6 (mp-1096778) 0.0000 2.272 4
Ba2ScSbO6 (mp-20709) 0.0000 2.196 4
Ba2YbSbO6 (mp-14223) 0.0000 1.747 4
Ba2YSbO6 (mp-14226) 0.0000 2.082 4
Ba2NbFeO6 (mp-1096853) 0.0000 2.749 4
Sr3Sb2 (mp-1013583) 0.0000 0.381 2
Ba3Bi2 (mp-1013736) 0.0000 0.388 2
Sr3P2 (mp-1013552) 0.0000 0.403 2
Sr3As2 (mp-1013559) 0.0000 0.367 2
Ba3As2 (mp-1013560) 0.0000 0.418 2
BaLaMgBiO6 (mp-41414) 0.0488 0.096 5
BaLaMgNbO6 (mp-39288) 0.0712 0.090 5
SrLaNbZnO6 (mp-41918) 0.0665 0.126 5
SrLaMnCoO6 (mp-40761) 0.0404 0.247 5
Sr6Ca2MnFe7O24 (mp-1075969) 0.0482 0.021 5
Na5Ca2Ce3Ti8Nb2O30 (mp-721094) 0.7380 0.065 6
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Cs_sv Pb_d Cl
Final Energy/Atom
-3.5434 eV
Corrected Energy
-19.5588 eV
Uncorrected energy = -17.7168 eV Composition-based energy adjustment (-0.614 eV/atom x 3.0 atoms) = -1.8420 eV Corrected energy = -19.5588 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 201250
  • 181780
  • 181286
  • 201251
  • 181779
  • 181781
  • 29072
Submitted by
User remarks:
  • Cesium lead(II) trichloride