Final Magnetic Moment
3.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
FM
Formation Energy / Atom
-1.265 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
4.13 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.687 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P63/mmc [194]
Hall
-P 6c 2c
Point Group
6/mmm
Crystal System
hexagonal

Electronic Structure

Topological data for ICSD ID 201829 from Topological Materials Database
Topological Classification
SM*
Subclassification
ESFD
Crossing Type
Point
* Semimetal
Enforced Semimetal with Fermi point Degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
CeO2 (mp-20194) <1 1 1> <0 0 1> 0.000 51.8
Si (mp-149) <1 1 1> <0 0 1> 0.000 51.8
SiC (mp-7631) <0 0 1> <0 0 1> 0.000 207.1
TePb (mp-19717) <1 1 0> <1 0 0> 0.001 305.0
C (mp-66) <1 1 1> <0 0 1> 0.001 155.3
CaCO3 (mp-3953) <0 0 1> <0 0 1> 0.002 155.3
ZnO (mp-2133) <1 0 1> <1 0 1> 0.004 217.7
Te2Mo (mp-602) <0 0 1> <0 0 1> 0.006 207.1
Bi2Te3 (mp-34202) <0 0 1> <0 0 1> 0.006 51.8
C (mp-48) <0 0 1> <0 0 1> 0.007 207.1
ZnO (mp-2133) <0 0 1> <1 1 0> 0.011 264.1
BaF2 (mp-1029) <1 1 1> <0 0 1> 0.013 207.1
CdS (mp-672) <1 0 1> <1 0 1> 0.017 290.2
C (mp-48) <1 0 0> <1 0 0> 0.019 152.5
BN (mp-984) <1 1 0> <1 0 0> 0.021 101.7
Ag (mp-124) <1 1 1> <0 0 1> 0.028 207.1
Te2W (mp-22693) <1 0 0> <1 0 1> 0.029 290.2
NdGaO3 (mp-3196) <1 1 0> <1 0 0> 0.030 305.0
C (mp-66) <1 1 0> <1 0 0> 0.030 305.0
SiC (mp-11714) <0 0 1> <0 0 1> 0.030 155.3
GaP (mp-2490) <1 1 1> <0 0 1> 0.031 51.8
MgF2 (mp-1249) <1 1 0> <1 0 0> 0.034 101.7
SiO2 (mp-6930) <0 0 1> <0 0 1> 0.040 155.3
GaSe (mp-1943) <0 0 1> <1 0 0> 0.042 50.8
CdTe (mp-406) <1 0 0> <1 1 0> 0.042 88.0
BaTiO3 (mp-5986) <1 0 0> <1 0 1> 0.043 290.2
InSb (mp-20012) <1 0 0> <1 1 0> 0.044 88.0
MgF2 (mp-1249) <0 0 1> <1 1 0> 0.046 88.0
AlN (mp-661) <1 0 1> <1 0 0> 0.046 305.0
CaF2 (mp-2741) <1 1 1> <0 0 1> 0.049 51.8
BN (mp-984) <0 0 1> <1 0 0> 0.052 152.5
Au (mp-81) <1 1 1> <0 0 1> 0.053 207.1
BaTiO3 (mp-5986) <1 1 0> <1 0 0> 0.054 305.0
Ga2O3 (mp-886) <1 0 0> <1 0 0> 0.054 254.2
Ni (mp-23) <1 0 0> <1 0 0> 0.055 305.0
MoSe2 (mp-1634) <0 0 1> <1 0 0> 0.058 152.5
WSe2 (mp-1821) <0 0 1> <1 0 0> 0.058 152.5
Te2Mo (mp-602) <1 1 0> <1 0 1> 0.061 290.2
CsI (mp-614603) <1 0 0> <1 0 0> 0.063 305.0
TiO2 (mp-2657) <0 0 1> <1 1 0> 0.063 88.0
InP (mp-20351) <1 0 0> <1 1 0> 0.064 176.1
BN (mp-984) <1 0 0> <1 0 0> 0.065 152.5
Cu (mp-30) <1 1 1> <0 0 1> 0.066 155.3
LiTaO3 (mp-3666) <0 0 1> <0 0 1> 0.066 207.1
MgF2 (mp-1249) <1 0 0> <1 0 0> 0.069 101.7
LiTaO3 (mp-3666) <1 0 1> <1 0 0> 0.071 152.5
C (mp-48) <1 0 1> <1 0 0> 0.072 254.2
SrTiO3 (mp-4651) <1 1 0> <1 0 0> 0.078 305.0
TePb (mp-19717) <1 0 0> <1 1 0> 0.079 88.0
LiNbO3 (mp-3731) <1 0 1> <1 0 0> 0.081 152.5
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
21 8 2 0 0 0
8 21 2 0 0 0
2 2 34 0 0 0
0 0 0 2 0 0
0 0 0 0 2 0
0 0 0 0 0 6
Compliance Tensor Sij (10-12Pa-1)
56.8 -20.9 -2.3 0 0 0
-20.9 56.8 -2.3 0 0 0
-2.3 -2.3 30 0 0 0
0 0 0 611 0 0
0 0 0 0 611 0
0 0 0 0 0 155.4
Shear Modulus GV
6 GPa
Bulk Modulus KV
11 GPa
Shear Modulus GR
3 GPa
Bulk Modulus KR
11 GPa
Shear Modulus GVRH
5 GPa
Bulk Modulus KVRH
11 GPa
Elastic Anisotropy
4.83
Poisson's Ratio
0.31

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
3.27 0.00 0.00
0.00 3.27 0.00
0.00 0.00 3.88
Dielectric Tensor εij (total)
7.78 0.00 0.00
0.00 7.78 0.00
0.00 0.00 13.35
Polycrystalline dielectric constant εpoly
(electronic contribution)
3.48
Polycrystalline dielectric constant εpoly
(total)
9.64
Refractive Index n
1.86
Potentially ferroelectric?
Unknown

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
RbNiBr3 (mp-27409) 0.0705 0.000 3
RbNiCl3 (mp-23486) 0.0433 0.000 3
CsCrCl3 (mp-570326) 0.0787 0.080 3
CsMgCl3 (mp-23004) 0.0417 0.000 3
CsMgBr3 (mp-29750) 0.0703 0.000 3
Cs2LiGaF6 (mp-6654) 0.4831 0.000 4
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Cs_sv V_pv Br
Final Energy/Atom
-4.2429 eV
Corrected Energy
-42.4290 eV
-42.4290 eV = -42.4290 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 201829
  • 201833
Submitted by
User remarks:
  • Cesium Vanadium(II) Tribromide- 293K

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)