Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.946 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.01 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap1.388 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP6222 [180] |
HallP 62 2c (0 0 1) |
Point Group622 |
Crystal Systemhexagonal |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 279.0 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 279.0 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 279.0 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 159.4 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 279.0 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 279.0 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 159.4 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 159.4 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 199.3 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 199.3 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 119.6 |
LiF (mp-1138) | <1 1 0> | <1 1 1> | 257.0 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 119.6 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 199.3 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 279.0 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 279.0 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 211.6 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 279.0 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 279.0 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 141.1 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 199.3 |
GaSe (mp-1943) | <0 0 1> | <1 0 1> | 243.1 |
GaSe (mp-1943) | <1 1 1> | <0 0 1> | 119.6 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 279.0 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 279.0 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 279.0 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 199.3 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 119.6 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 159.4 |
Al (mp-134) | <1 1 0> | <1 1 1> | 257.0 |
Al (mp-134) | <1 1 1> | <0 0 1> | 119.6 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 119.6 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 199.3 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 159.4 |
Al (mp-134) | <1 0 0> | <0 0 1> | 199.3 |
Fe3O4 (mp-19306) | <1 1 1> | <0 0 1> | 119.6 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 199.3 |
CdTe (mp-406) | <1 0 0> | <0 0 1> | 318.8 |
CdTe (mp-406) | <1 1 0> | <0 0 1> | 318.8 |
C (mp-66) | <1 1 0> | <0 0 1> | 358.7 |
C (mp-66) | <1 1 1> | <0 0 1> | 159.4 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 159.4 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 279.0 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 119.6 |
TiO2 (mp-2657) | <0 0 1> | <1 0 0> | 211.6 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 279.0 |
Mg (mp-153) | <1 0 1> | <0 0 1> | 279.0 |
PbS (mp-21276) | <1 0 0> | <0 0 1> | 279.0 |
PbS (mp-21276) | <1 1 0> | <0 0 1> | 199.3 |
GdScO3 (mp-5690) | <0 0 1> | <1 1 1> | 128.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Piezoelectric Tensor eij (C/m2) |
|||||
---|---|---|---|---|---|
0.00000 | 0.00000 | 0.00000 | -0.06017 | 0.00000 | 0.00000 |
0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.06017 | 0.00000 |
0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.00000 |
Piezoelectric Modulus ‖eij‖max0.06017 C/m2 |
Crystallographic Direction vmax |
---|
1.00000 |
-1.00000 |
0.00000 |
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
5.60 | 0.00 | 0.00 |
0.00 | 5.60 | 0.00 |
0.00 | 0.00 | 4.36 |
Dielectric Tensor εij (total) |
||
---|---|---|
11.84 | 0.00 | 0.00 |
0.00 | 11.84 | 0.00 |
0.00 | 0.00 | 10.48 |
Polycrystalline dielectric constant
εpoly∞
5.19
|
Polycrystalline dielectric constant
εpoly
11.39
|
Refractive Index n2.28 |
Potentially ferroelectric?Unknown |
Run TypeGGA |
Energy Cutoff700 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Na_pv Hg I O |
Final Energy/Atom-2.9352 eV |
Corrected Energy-58.0925 eV
Uncorrected energy = -52.8335 eV
Composition-based energy adjustment (-0.687 eV/atom x 6.0 atoms) = -4.1220 eV
Composition-based energy adjustment (-0.379 eV/atom x 3.0 atoms) = -1.1370 eV
Corrected energy = -58.0925 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)