Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.024 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density10.64 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPnma [62] |
Hall-P 2ac 2n |
Point Groupmmm |
Crystal Systemorthorhombic |
Topological ClassificationSM*
|
SubclassificationES†
|
Crossing TypePlane
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
KP(HO2)2 (mp-23959) | <0 0 1> | <0 1 1> | 303.3 |
GaTe (mp-542812) | <0 0 1> | <0 0 1> | 74.1 |
TiO2 (mp-2657) | <0 0 1> | <0 1 1> | 303.3 |
Ag (mp-124) | <1 0 0> | <0 1 1> | 121.3 |
BaTiO3 (mp-5986) | <1 0 1> | <0 1 1> | 303.3 |
Au (mp-81) | <1 0 0> | <0 1 1> | 121.3 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 296.4 |
LaF3 (mp-905) | <0 0 1> | <0 1 1> | 182.0 |
GaN (mp-804) | <0 0 1> | <0 1 1> | 242.6 |
GaTe (mp-542812) | <1 0 -1> | <0 1 1> | 303.3 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 288.1 |
C (mp-48) | <0 0 1> | <0 1 0> | 288.1 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 1 1> | 60.7 |
BN (mp-984) | <1 1 0> | <0 0 1> | 333.5 |
TiO2 (mp-390) | <1 0 1> | <0 1 0> | 240.1 |
Al (mp-134) | <1 1 1> | <1 1 0> | 113.5 |
GdScO3 (mp-5690) | <1 0 1> | <1 1 0> | 113.5 |
Ni (mp-23) | <1 1 0> | <0 1 0> | 192.1 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 144.1 |
KTaO3 (mp-3614) | <1 1 1> | <1 1 0> | 113.5 |
GaSe (mp-1943) | <1 0 0> | <1 0 0> | 205.8 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 259.4 |
GaSe (mp-1943) | <0 0 1> | <0 1 1> | 242.6 |
Al2O3 (mp-1143) | <0 0 1> | <0 0 1> | 222.3 |
ZrO2 (mp-2858) | <1 0 0> | <0 0 1> | 259.4 |
WSe2 (mp-1821) | <0 0 1> | <0 1 1> | 242.6 |
MoSe2 (mp-1634) | <0 0 1> | <0 1 1> | 242.6 |
GaTe (mp-542812) | <1 0 0> | <0 1 1> | 182.0 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 296.4 |
CdS (mp-672) | <0 0 1> | <0 1 1> | 60.7 |
Te2W (mp-22693) | <0 0 1> | <0 1 1> | 242.6 |
GaSb (mp-1156) | <1 1 0> | <1 0 1> | 109.3 |
CdSe (mp-2691) | <1 1 0> | <1 0 1> | 109.3 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 296.4 |
PbSe (mp-2201) | <1 1 0> | <1 0 1> | 109.3 |
Ga2O3 (mp-886) | <1 0 0> | <0 1 0> | 144.1 |
LiNbO3 (mp-3731) | <1 1 1> | <0 0 1> | 259.4 |
SiC (mp-7631) | <1 0 0> | <0 0 1> | 333.5 |
Fe2O3 (mp-24972) | <0 0 1> | <0 0 1> | 185.3 |
MgF2 (mp-1249) | <1 0 1> | <0 1 0> | 288.1 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 185.3 |
SiC (mp-8062) | <1 1 0> | <1 0 1> | 109.3 |
BaTiO3 (mp-5986) | <1 1 0> | <0 1 0> | 48.0 |
C (mp-66) | <1 1 0> | <1 0 1> | 109.3 |
YAlO3 (mp-3792) | <0 1 1> | <0 0 1> | 333.5 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 259.4 |
CdS (mp-672) | <1 1 0> | <0 1 1> | 303.3 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 333.5 |
Mg (mp-153) | <1 0 0> | <0 1 0> | 288.1 |
Si (mp-149) | <1 1 0> | <0 0 1> | 333.5 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
47 | 23 | 32 | 0 | 0 | 0 |
23 | 39 | 30 | 0 | 0 | 0 |
32 | 30 | 59 | 0 | 0 | 0 |
0 | 0 | 0 | 13 | 0 | 0 |
0 | 0 | 0 | 0 | 8 | 0 |
0 | 0 | 0 | 0 | 0 | 10 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
35.8 | -9.5 | -14.9 | 0 | 0 | 0 |
-9.5 | 45 | -17.7 | 0 | 0 | 0 |
-14.9 | -17.7 | 34.3 | 0 | 0 | 0 |
0 | 0 | 0 | 75.6 | 0 | 0 |
0 | 0 | 0 | 0 | 121.8 | 0 |
0 | 0 | 0 | 0 | 0 | 98.9 |
Shear Modulus GV10 GPa |
Bulk Modulus KV35 GPa |
Shear Modulus GR10 GPa |
Bulk Modulus KR32 GPa |
Shear Modulus GVRH10 GPa |
Bulk Modulus KVRH34 GPa |
Elastic Anisotropy0.29 |
Poisson's Ratio0.36 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Re3Te4Cl5 (mp-29114) | 0.7462 | 0.000 | 3 |
Re3(TeBr)7 (mp-623087) | 0.7394 | 0.013 | 3 |
Ba2YF7 (mp-753793) | 0.6715 | 0.049 | 3 |
Bi3Rh (mp-581990) | 0.3148 | 0.019 | 2 |
W3Br7 (mp-28880) | 0.6060 | 0.041 | 2 |
SrF3 (mp-1080514) | 0.6720 | 0.000 | 2 |
BaF3 (mp-1080821) | 0.7070 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ni_pv Bi |
Final Energy/Atom-4.3869 eV |
Corrected Energy-70.1899 eV
-70.1899 eV = -70.1899 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)