Final Magnetic Moment3.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.134 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.49 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP63/m [176] |
Hall-P 6c |
Point Group6/m |
Crystal Systemhexagonal |
Topological ClassificationSM*
|
SubclassificationESFD†
|
Crossing TypePoint
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | elastic energy [meV] | MCIA† [Å2] |
---|---|---|---|---|
MgO (mp-1265) | <1 1 0> | <1 0 0> | 0.000 | 128.0 |
NdGaO3 (mp-3196) | <1 0 0> | <1 0 1> | 0.004 | 175.4 |
BN (mp-984) | <0 0 1> | <0 0 1> | 0.005 | 48.9 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 0.005 | 342.6 |
PbS (mp-21276) | <1 1 0> | <1 0 0> | 0.005 | 255.9 |
Ge3(BiO3)4 (mp-23560) | <1 1 1> | <0 0 1> | 0.006 | 195.8 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 0.007 | 195.8 |
C (mp-48) | <1 1 0> | <1 1 0> | 0.007 | 166.2 |
CdS (mp-672) | <1 0 1> | <1 0 1> | 0.008 | 292.4 |
ZnO (mp-2133) | <1 0 0> | <1 1 0> | 0.010 | 277.0 |
Mg (mp-153) | <1 1 1> | <1 1 0> | 0.011 | 332.5 |
SiC (mp-7631) | <1 0 0> | <1 0 1> | 0.016 | 233.9 |
ZnSe (mp-1190) | <1 0 0> | <1 1 0> | 0.016 | 166.2 |
GaAs (mp-2534) | <1 0 0> | <1 1 0> | 0.016 | 166.2 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 0.016 | 342.6 |
YAlO3 (mp-3792) | <1 1 0> | <1 0 0> | 0.017 | 223.9 |
CdWO4 (mp-19387) | <0 1 0> | <1 0 0> | 0.019 | 160.0 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 0.019 | 195.8 |
Al (mp-134) | <1 1 1> | <0 0 1> | 0.019 | 195.8 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 0.020 | 287.9 |
YAlO3 (mp-3792) | <0 1 0> | <1 0 1> | 0.023 | 116.9 |
C (mp-48) | <0 0 1> | <1 0 0> | 0.024 | 32.0 |
Ge (mp-32) | <1 0 0> | <1 1 0> | 0.025 | 166.2 |
C (mp-66) | <1 0 0> | <1 1 0> | 0.026 | 166.2 |
Ni (mp-23) | <1 1 1> | <1 0 0> | 0.026 | 64.0 |
GaN (mp-804) | <1 1 1> | <1 1 0> | 0.026 | 332.5 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 0> | 0.027 | 128.0 |
CdWO4 (mp-19387) | <1 0 1> | <1 0 0> | 0.029 | 223.9 |
Fe3O4 (mp-19306) | <1 0 0> | <1 1 0> | 0.029 | 221.6 |
BaTiO3 (mp-5986) | <1 1 0> | <1 0 0> | 0.031 | 96.0 |
KCl (mp-23193) | <1 0 0> | <1 1 0> | 0.035 | 166.2 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 0.037 | 191.9 |
TiO2 (mp-390) | <1 0 0> | <0 0 1> | 0.038 | 146.8 |
C (mp-48) | <1 0 0> | <1 0 0> | 0.039 | 351.9 |
LiF (mp-1138) | <1 0 0> | <1 1 0> | 0.041 | 166.2 |
CdTe (mp-406) | <1 1 0> | <0 0 1> | 0.043 | 244.7 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 0.044 | 244.7 |
MoS2 (mp-1434) | <1 0 0> | <1 1 0> | 0.045 | 277.0 |
LiGaO2 (mp-5854) | <1 1 0> | <1 0 0> | 0.045 | 96.0 |
SiC (mp-11714) | <0 0 1> | <1 0 0> | 0.046 | 255.9 |
Ga2O3 (mp-886) | <1 0 1> | <1 0 1> | 0.047 | 233.9 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 0.048 | 319.9 |
InSb (mp-20012) | <1 1 0> | <0 0 1> | 0.048 | 244.7 |
SiC (mp-7631) | <0 0 1> | <1 0 0> | 0.049 | 255.9 |
Al (mp-134) | <1 0 0> | <1 1 0> | 0.049 | 166.2 |
YAlO3 (mp-3792) | <1 0 0> | <1 0 0> | 0.051 | 160.0 |
ZrO2 (mp-2858) | <0 0 1> | <1 0 0> | 0.051 | 223.9 |
BaTiO3 (mp-5986) | <1 0 0> | <1 1 0> | 0.051 | 166.2 |
MgO (mp-1265) | <1 0 0> | <1 1 0> | 0.052 | 55.4 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 0.057 | 195.8 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
33 | 11 | 25 | 0 | 0 | 0 |
11 | 33 | 25 | 0 | 0 | 0 |
25 | 25 | 60 | 0 | 0 | 0 |
0 | 0 | 0 | 23 | 0 | 0 |
0 | 0 | 0 | 0 | 23 | 0 |
0 | 0 | 0 | 0 | 0 | 11 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
44.7 | -2.2 | -17.6 | 0 | 0 | 0 |
-2.2 | 44.7 | -17.6 | 0 | 0 | 0 |
-17.6 | -17.6 | 31.4 | 0 | 0 | 0 |
0 | 0 | 0 | 44 | 0 | 0 |
0 | 0 | 0 | 0 | 44 | 0 |
0 | 0 | 0 | 0 | 0 | 93.9 |
Shear Modulus GV16 GPa |
Bulk Modulus KV27 GPa |
Shear Modulus GR13 GPa |
Bulk Modulus KR22 GPa |
Shear Modulus GVRH14 GPa |
Bulk Modulus KVRH25 GPa |
Elastic Anisotropy1.35 |
Poisson's Ratio0.26 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: U Cl |
Final Energy/Atom-5.8972 eV |
Corrected Energy-47.1776 eV
-47.1776 eV = -47.1776 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)