Final Magnetic Moment0.030 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.726 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.001 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.97 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToTb3Ge5 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFdd2 [43] |
HallF 2 2d |
Point Groupmm2 |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaAs (mp-2534) | <1 0 0> | <0 1 0> | 101.1 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 240.9 |
GaN (mp-804) | <1 1 0> | <0 1 1> | 258.3 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 160.6 |
ZnSe (mp-1190) | <1 0 0> | <0 1 0> | 101.1 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 240.9 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 1> | 129.1 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 160.6 |
LiF (mp-1138) | <1 0 0> | <0 1 0> | 101.1 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 240.9 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 240.9 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 240.9 |
GaSe (mp-1943) | <1 0 0> | <0 1 0> | 202.3 |
Al (mp-134) | <1 0 0> | <0 1 1> | 129.1 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 240.9 |
TeO2 (mp-2125) | <0 0 1> | <0 1 1> | 129.1 |
TeO2 (mp-2125) | <1 0 1> | <0 0 1> | 80.3 |
Al (mp-134) | <1 1 0> | <0 0 1> | 160.6 |
C (mp-66) | <1 0 0> | <0 0 1> | 240.9 |
GdScO3 (mp-5690) | <0 0 1> | <0 1 1> | 129.1 |
GdScO3 (mp-5690) | <1 1 0> | <0 1 0> | 202.3 |
Mg (mp-153) | <1 1 0> | <0 1 1> | 258.3 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 240.9 |
TbScO3 (mp-31119) | <0 0 1> | <0 0 1> | 160.6 |
InP (mp-20351) | <1 1 0> | <0 0 1> | 240.9 |
BaTiO3 (mp-5986) | <0 0 1> | <0 1 1> | 129.1 |
BaTiO3 (mp-5986) | <1 0 1> | <0 0 1> | 160.6 |
BaTiO3 (mp-5986) | <1 1 0> | <0 0 1> | 240.9 |
Ga2O3 (mp-886) | <1 0 0> | <0 0 1> | 160.6 |
Au (mp-81) | <1 0 0> | <0 0 1> | 240.9 |
Au (mp-81) | <1 1 0> | <0 0 1> | 240.9 |
Au (mp-81) | <1 1 1> | <0 0 1> | 240.9 |
NaCl (mp-22862) | <1 0 0> | <0 1 1> | 129.1 |
C (mp-48) | <0 0 1> | <0 1 1> | 258.3 |
C (mp-48) | <1 0 1> | <0 1 1> | 258.3 |
WSe2 (mp-1821) | <1 1 0> | <0 1 1> | 258.3 |
ZnO (mp-2133) | <1 0 0> | <0 0 1> | 240.9 |
MgAl2O4 (mp-3536) | <1 0 0> | <0 1 0> | 202.3 |
Ge (mp-32) | <1 1 0> | <0 0 1> | 240.9 |
ZnO (mp-2133) | <1 1 0> | <0 0 1> | 240.9 |
ZnO (mp-2133) | <1 1 1> | <0 1 1> | 129.1 |
Ge (mp-32) | <1 0 0> | <0 1 0> | 101.1 |
Fe2O3 (mp-24972) | <1 1 0> | <0 0 1> | 240.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
BaLaCl5 (mp-772035) | 0.6877 | 0.062 | 3 |
CsMg6Zn (mp-1022712) | 0.6766 | 0.223 | 3 |
Nb(SeCl)2 (mp-27361) | 0.7076 | 0.008 | 3 |
Nb(SeBr)2 (mp-541667) | 0.6856 | 0.000 | 3 |
Dy3Ge5 (mp-505577) | 0.1554 | 0.001 | 2 |
Sm3Ge5 (mp-580126) | 0.2121 | 0.004 | 2 |
Ho3Ge5 (mp-542748) | 0.0665 | 0.000 | 2 |
Y3Ge5 (mp-17118) | 0.0681 | 0.000 | 2 |
Ho14Ge23 (mp-29774) | 0.2866 | 0.066 | 2 |
U (mp-1077335) | 0.7497 | 0.282 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Tb_3 Ge_d |
Final Energy/Atom-5.3498 eV |
Corrected Energy-85.5976 eV
-85.5976 eV = -85.5976 eV (uncorrected energy)
|