Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.067 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density1.91 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap1.775 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP4/n [85] |
HallP 4ab 1ab |
Point Group4/m |
Crystal Systemtetragonal |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 209.5 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 190.2 |
CeO2 (mp-20194) | <1 1 1> | <1 1 0> | 104.8 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 285.2 |
Te2W (mp-22693) | <1 0 0> | <1 0 0> | 296.3 |
YVO4 (mp-19133) | <1 0 1> | <0 0 1> | 285.2 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 222.3 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 285.2 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 222.3 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 285.2 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 285.2 |
BN (mp-984) | <1 1 0> | <1 0 0> | 296.3 |
Al (mp-134) | <1 1 1> | <1 0 0> | 222.3 |
BN (mp-984) | <1 0 0> | <1 1 0> | 209.5 |
BN (mp-984) | <1 0 1> | <1 0 0> | 296.3 |
BN (mp-984) | <1 1 1> | <1 0 0> | 296.3 |
LiGaO2 (mp-5854) | <1 1 0> | <1 0 0> | 148.2 |
LiTaO3 (mp-3666) | <1 0 0> | <1 1 0> | 209.5 |
TiO2 (mp-2657) | <1 0 0> | <1 1 0> | 209.5 |
TiO2 (mp-2657) | <1 1 0> | <1 0 0> | 296.3 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 0> | 296.3 |
GdScO3 (mp-5690) | <1 0 1> | <1 0 0> | 222.3 |
LaF3 (mp-905) | <1 0 0> | <1 0 0> | 222.3 |
GaP (mp-2490) | <1 1 0> | <1 1 0> | 209.5 |
GaP (mp-2490) | <1 1 1> | <1 1 0> | 104.8 |
MoSe2 (mp-1634) | <1 0 0> | <1 0 0> | 148.2 |
Si (mp-149) | <1 1 0> | <1 1 0> | 209.5 |
Si (mp-149) | <1 1 1> | <1 1 0> | 104.8 |
TbScO3 (mp-31119) | <1 0 1> | <1 0 0> | 222.3 |
C (mp-48) | <1 0 0> | <1 1 0> | 209.5 |
C (mp-48) | <1 0 1> | <1 0 0> | 296.3 |
PbSe (mp-2201) | <1 0 0> | <0 0 1> | 190.2 |
BaTiO3 (mp-5986) | <0 0 1> | <1 0 1> | 241.1 |
YAlO3 (mp-3792) | <1 1 0> | <1 0 0> | 222.3 |
NdGaO3 (mp-3196) | <0 1 0> | <1 1 0> | 209.5 |
NdGaO3 (mp-3196) | <1 0 0> | <1 0 0> | 296.3 |
NdGaO3 (mp-3196) | <1 0 1> | <1 0 0> | 222.3 |
NdGaO3 (mp-3196) | <1 1 0> | <1 0 0> | 296.3 |
CdWO4 (mp-19387) | <1 0 1> | <1 0 0> | 222.3 |
CdSe (mp-2691) | <1 0 0> | <0 0 1> | 190.2 |
C (mp-48) | <1 1 0> | <1 0 0> | 296.3 |
ZnO (mp-2133) | <1 0 1> | <1 0 1> | 120.5 |
SrTiO3 (mp-4651) | <1 0 1> | <1 0 0> | 222.3 |
WSe2 (mp-1821) | <1 0 0> | <1 0 0> | 148.2 |
NaCl (mp-22862) | <1 1 1> | <0 0 1> | 285.2 |
ZrO2 (mp-2858) | <0 0 1> | <1 0 0> | 222.3 |
ZrO2 (mp-2858) | <1 0 -1> | <0 0 1> | 285.2 |
LiAlO2 (mp-3427) | <1 0 1> | <1 0 0> | 296.3 |
LiAlO2 (mp-3427) | <1 1 0> | <1 0 0> | 148.2 |
LiAlO2 (mp-3427) | <1 1 1> | <1 0 0> | 222.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
AsCl2F3 (mp-23444) | 0.3075 | 0.000 | 3 |
NbPCl10 (mp-27787) | 0.4743 | 0.000 | 3 |
TaPCl10 (mp-27788) | 0.4791 | 0.000 | 3 |
UPCl10 (mp-540927) | 0.5058 | 0.000 | 3 |
Sn(PCl6)4 (mp-685443) | 0.5551 | 0.001 | 3 |
SiH8(NF3)2 (mp-759722) | 0.6245 | 0.000 | 4 |
SbP(Cl2F3)2 (mp-559301) | 0.2838 | 0.095 | 4 |
AsSOF9 (mp-556515) | 0.6179 | 0.042 | 4 |
MgPHO9 (mp-632723) | 0.5773 | 0.860 | 4 |
MgPHO9 (mp-720260) | 0.5536 | 0.859 | 4 |
PCl5 (mp-569410) | 0.6282 | 0.006 | 2 |
NaCrH8(NF3)2 (mp-976447) | 0.6719 | 0.013 | 5 |
FeB2C6(O3F4)2 (mp-567042) | 0.5809 | 0.311 | 5 |
NaGaH8(NF3)2 (mp-865095) | 0.6682 | 0.008 | 5 |
NaInH8(NF3)2 (mp-643394) | 0.6149 | 0.028 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: P Cl |
Final Energy/Atom-3.0130 eV |
Corrected Energy-72.3131 eV
-72.3131 eV = -72.3131 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)