Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.847 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.099 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density1.50 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToBCl3 + B |
Band Gap0.901 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP212121 [19] |
HallP 2ac 2ab |
Point Group222 |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <0 0 1> | 224.4 |
GaAs (mp-2534) | <1 1 0> | <0 1 0> | 241.2 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 241.2 |
ZnSe (mp-1190) | <1 1 0> | <0 1 0> | 241.2 |
CdS (mp-672) | <1 1 0> | <1 0 0> | 198.0 |
GaSe (mp-1943) | <0 0 1> | <0 1 0> | 241.2 |
BN (mp-984) | <1 1 1> | <0 1 0> | 241.2 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 1 0> | 120.6 |
LiGaO2 (mp-5854) | <1 0 1> | <0 0 1> | 224.4 |
TeO2 (mp-2125) | <0 1 1> | <0 0 1> | 224.4 |
GdScO3 (mp-5690) | <0 1 0> | <0 0 1> | 224.4 |
PbS (mp-21276) | <1 1 1> | <0 1 0> | 120.6 |
InP (mp-20351) | <1 1 1> | <0 1 0> | 120.6 |
Ge (mp-32) | <1 1 0> | <0 1 0> | 241.2 |
LiAlO2 (mp-3427) | <1 0 0> | <0 1 1> | 164.7 |
Al2O3 (mp-1143) | <0 0 1> | <0 1 0> | 120.6 |
MoSe2 (mp-1634) | <0 0 1> | <0 1 0> | 241.2 |
WS2 (mp-224) | <1 1 0> | <0 1 0> | 241.2 |
WS2 (mp-224) | <1 1 1> | <0 1 0> | 241.2 |
C (mp-48) | <1 1 1> | <0 1 0> | 241.2 |
WSe2 (mp-1821) | <0 0 1> | <0 1 0> | 241.2 |
NaCl (mp-22862) | <1 1 1> | <0 0 1> | 112.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Rb(BH)5 (mp-780534) | 0.5981 | 0.085 | 3 |
B2AsCl2 (mp-29028) | 0.7326 | 0.133 | 3 |
K(BH)5 (mp-24270) | 0.6839 | 0.067 | 3 |
WOF4 (mp-765187) | 0.7413 | 0.060 | 3 |
B2PCl2 (mp-28426) | 0.7084 | 0.220 | 3 |
B5PH4Cl (mp-758806) | 0.7458 | 0.027 | 4 |
K2B10H9O (mp-705892) | 0.7131 | 0.387 | 4 |
KVOF4 (mp-566952) | 0.7486 | 0.000 | 4 |
BBr (mp-685043) | 0.4660 | 0.009 | 2 |
VF5 (mp-766786) | 0.7125 | 0.037 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: B Cl |
Final Energy/Atom-4.8132 eV |
Corrected Energy-308.0471 eV
-308.0471 eV = -308.0471 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)