Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-3.427 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.197 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density8.58 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToUO3 |
Band Gap0.468 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCmmm [65] |
Hall-C 2 2 |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 174.5 |
AlN (mp-661) | <0 0 1> | <0 1 1> | 155.1 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 142.0 |
AlN (mp-661) | <1 1 1> | <1 1 0> | 198.5 |
CeO2 (mp-20194) | <1 1 0> | <0 1 1> | 124.1 |
CeO2 (mp-20194) | <1 1 1> | <0 1 0> | 157.7 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 187.0 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 232.7 |
CeO2 (mp-20194) | <1 0 0> | <1 0 1> | 158.0 |
GaAs (mp-2534) | <1 0 0> | <1 0 1> | 158.0 |
GaAs (mp-2534) | <1 1 0> | <0 1 1> | 93.1 |
GaAs (mp-2534) | <1 1 1> | <1 1 0> | 231.6 |
BaF2 (mp-1029) | <1 0 0> | <0 1 0> | 347.0 |
BaF2 (mp-1029) | <1 1 0> | <0 1 1> | 341.2 |
BaF2 (mp-1029) | <1 1 1> | <1 0 1> | 276.4 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 110.4 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 145.4 |
GaN (mp-804) | <1 0 1> | <0 1 1> | 248.2 |
GaN (mp-804) | <1 1 0> | <1 0 1> | 118.5 |
GaN (mp-804) | <1 1 1> | <1 0 1> | 158.0 |
SiO2 (mp-6930) | <0 0 1> | <1 0 1> | 197.4 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 165.4 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 106.8 |
SiO2 (mp-6930) | <1 1 0> | <1 0 1> | 197.4 |
SiO2 (mp-6930) | <1 1 1> | <0 1 0> | 157.7 |
KCl (mp-23193) | <1 0 0> | <0 1 0> | 283.9 |
KCl (mp-23193) | <1 1 0> | <0 1 0> | 236.6 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 1> | 158.0 |
DyScO3 (mp-31120) | <0 1 0> | <1 1 0> | 132.3 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 0> | 165.4 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 1> | 93.1 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 1> | 276.4 |
InAs (mp-20305) | <1 0 0> | <0 1 0> | 347.0 |
InAs (mp-20305) | <1 1 0> | <0 1 1> | 341.2 |
ZnSe (mp-1190) | <1 1 0> | <0 1 1> | 93.1 |
ZnSe (mp-1190) | <1 1 1> | <0 1 0> | 283.9 |
KTaO3 (mp-3614) | <1 0 0> | <1 1 0> | 33.1 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 29.1 |
CdS (mp-672) | <1 1 1> | <1 1 0> | 264.7 |
LiF (mp-1138) | <1 1 1> | <0 1 0> | 173.5 |
Te2W (mp-22693) | <0 1 0> | <1 0 0> | 319.9 |
Te2W (mp-22693) | <0 1 1> | <1 0 1> | 118.5 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 87.3 |
Te2Mo (mp-602) | <1 0 0> | <1 0 1> | 276.4 |
Te2Mo (mp-602) | <1 1 0> | <1 0 1> | 276.4 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 87.3 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 99.3 |
Ag (mp-124) | <1 1 1> | <1 1 1> | 297.7 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 1 1> | 186.1 |
GaSe (mp-1943) | <0 0 1> | <0 1 1> | 155.1 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
500 | 14 | 31 | 0 | 0 | 0 |
14 | 209 | 249 | 0 | 0 | 0 |
31 | 249 | 322 | 0 | 0 | 0 |
0 | 0 | 0 | -13 | 0 | 0 |
0 | 0 | 0 | 0 | 38 | 0 |
0 | 0 | 0 | 0 | 0 | 24 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
2 | 1.1 | -1.1 | 0 | 0 | 0 |
1.1 | 60.1 | -46.5 | 0 | 0 | 0 |
-1.1 | -46.5 | 39.1 | 0 | 0 | 0 |
0 | 0 | 0 | -78.3 | 0 | 0 |
0 | 0 | 0 | 0 | 26.6 | 0 |
0 | 0 | 0 | 0 | 0 | 42.2 |
Shear Modulus GV59 GPa |
Bulk Modulus KV180 GPa |
Shear Modulus GR27 GPa |
Bulk Modulus KR119 GPa |
Shear Modulus GVRH43 GPa |
Bulk Modulus KVRH150 GPa |
Elastic Anisotropy6.51 |
Poisson's Ratio0.37 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: U O |
Final Energy/Atom-9.4337 eV |
Corrected Energy-39.8416 eV
-39.8416 eV = -37.7347 eV (uncorrected energy) - 2.1069 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)