Final Magnetic Moment0.022 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.050 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.78 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap3.426 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP63 [173] |
HallP 6c |
Point Group6 |
Crystal Systemhexagonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <1 0 0> | 210.9 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 274.0 |
CeO2 (mp-20194) | <1 0 0> | <1 1 0> | 91.3 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 210.9 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 263.6 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 210.9 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 274.0 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 91.3 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 210.9 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 52.7 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 163.7 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 0> | 210.9 |
KTaO3 (mp-3614) | <1 0 0> | <1 1 0> | 274.0 |
CdS (mp-672) | <0 0 1> | <1 1 1> | 122.6 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 210.9 |
YVO4 (mp-19133) | <1 0 0> | <1 0 0> | 316.4 |
YVO4 (mp-19133) | <1 0 1> | <1 0 0> | 210.9 |
TePb (mp-19717) | <1 1 0> | <1 0 0> | 316.4 |
Ag (mp-124) | <1 0 0> | <1 1 0> | 274.0 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 263.6 |
BN (mp-984) | <1 0 0> | <1 1 0> | 274.0 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 1 1> | 122.6 |
MoS2 (mp-1434) | <0 0 1> | <1 0 0> | 52.7 |
MoS2 (mp-1434) | <1 0 0> | <1 0 0> | 210.9 |
Al (mp-134) | <1 0 0> | <1 1 0> | 274.0 |
LiGaO2 (mp-5854) | <0 0 1> | <1 1 0> | 274.0 |
LiGaO2 (mp-5854) | <1 0 0> | <1 0 0> | 105.5 |
LiGaO2 (mp-5854) | <1 0 1> | <1 1 0> | 91.3 |
CdTe (mp-406) | <1 1 0> | <1 0 0> | 316.4 |
CdWO4 (mp-19387) | <1 0 1> | <1 0 0> | 316.4 |
TiO2 (mp-390) | <0 0 1> | <1 0 0> | 263.6 |
TiO2 (mp-390) | <1 0 0> | <1 0 0> | 263.6 |
TiO2 (mp-390) | <1 1 0> | <1 0 0> | 52.7 |
CsI (mp-614603) | <1 0 0> | <1 1 0> | 182.7 |
ZnO (mp-2133) | <1 0 0> | <1 0 0> | 52.7 |
ZnO (mp-2133) | <1 1 0> | <1 1 0> | 91.3 |
ZnO (mp-2133) | <1 1 1> | <1 0 0> | 210.9 |
MgAl2O4 (mp-3536) | <1 0 0> | <1 1 0> | 274.0 |
SrTiO3 (mp-4651) | <0 0 1> | <1 1 0> | 91.3 |
SrTiO3 (mp-4651) | <1 0 0> | <1 0 0> | 210.9 |
SrTiO3 (mp-4651) | <1 0 1> | <1 0 0> | 52.7 |
SrTiO3 (mp-4651) | <1 1 0> | <1 1 0> | 182.7 |
SrTiO3 (mp-4651) | <1 1 1> | <1 0 0> | 210.9 |
Cu (mp-30) | <1 1 0> | <1 0 0> | 263.6 |
GaTe (mp-542812) | <1 0 0> | <1 0 0> | 316.4 |
LiAlO2 (mp-3427) | <0 0 1> | <1 1 0> | 274.0 |
Al2O3 (mp-1143) | <0 0 1> | <1 0 0> | 158.2 |
Al2O3 (mp-1143) | <1 0 1> | <1 0 0> | 263.6 |
CaF2 (mp-2741) | <1 0 0> | <1 1 0> | 91.3 |
CaF2 (mp-2741) | <1 1 0> | <1 0 0> | 210.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Piezoelectric Tensor eij (C/m2) |
|||||
---|---|---|---|---|---|
0.00000 | 0.00000 | 0.00000 | 0.01692 | 0.82479 | 0.00000 |
0.00000 | 0.00000 | 0.00000 | 0.82479 | -0.01693 | 0.00000 |
0.37284 | 0.37284 | 0.85063 | 0.00000 | 0.00000 | 0.00000 |
Piezoelectric Modulus ‖eij‖max1.00080 C/m2 |
Crystallographic Direction vmax |
---|
0.00000 |
-1.00000 |
1.00000 |
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
3.93 | -0.00 | 0.00 |
0.00 | 3.93 | 0.00 |
0.00 | 0.00 | 3.45 |
Dielectric Tensor εij (total) |
||
---|---|---|
7.93 | -0.00 | 0.00 |
0.00 | 7.93 | 0.00 |
0.00 | 0.00 | 6.11 |
Polycrystalline dielectric constant
εpoly∞
3.77
|
Polycrystalline dielectric constant
εpoly
7.33
|
Refractive Index n1.94 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ni(IO3)2 (mp-772376) | 0.4566 | 0.046 | 3 |
Sr(IO3)2 (mp-754869) | 0.4230 | 0.026 | 3 |
Al(IO3)3 (mp-555903) | 0.3068 | 0.000 | 3 |
Fe(IO3)3 (mp-24993) | 0.1669 | 0.097 | 3 |
Ga(IO3)3 (mp-561104) | 0.2027 | 0.000 | 3 |
LiIn(IO3)4 (mp-973966) | 0.6749 | 0.000 | 4 |
MgH2(SO4)2 (mp-690765) | 0.4923 | 0.622 | 4 |
CrHSe3O8 (mp-762136) | 0.5429 | 0.000 | 4 |
SbSeCl7O (mp-572726) | 0.6288 | 0.000 | 4 |
SnSe2(Cl4O)2 (mp-560193) | 0.5964 | 0.000 | 4 |
V2F7 (mp-765242) | 0.7277 | 0.089 | 2 |
TiZnH12(OF)6 (mp-866807) | 0.6762 | 0.020 | 5 |
FeH12Pt(ClO)6 (mp-542912) | 0.6269 | 0.000 | 5 |
H2RhN2Cl5O (mp-706921) | 0.7181 | 0.929 | 5 |
FeH12Pt(ClO)6 (mp-605175) | 0.6112 | 0.000 | 5 |
AlH2PbO2F3 (mp-643387) | 0.7299 | 0.000 | 5 |
Run TypeGGA |
Energy Cutoff700 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: In_d I O |
Final Energy/Atom-4.5530 eV |
Corrected Energy-131.0204 eV
-131.0204 eV = -118.3791 eV (uncorrected energy) - 12.6412 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)