Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.495 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.60 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFm3m [225] |
Hall-F 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Topological ClassificationSM*
|
SubclassificationESFD†
|
Crossing TypePoint
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
KP(HO2)2 (mp-23959) | <0 0 1> | <1 1 1> | 299.3 |
GaTe (mp-542812) | <0 0 1> | <1 1 1> | 299.3 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 276.4 |
SiC (mp-8062) | <1 0 0> | <1 0 0> | 172.8 |
Ga2O3 (mp-886) | <1 1 0> | <1 1 0> | 146.6 |
GaSe (mp-1943) | <0 0 1> | <1 1 1> | 239.4 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 48.9 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 172.8 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 34.6 |
TiO2 (mp-2657) | <0 0 1> | <1 0 0> | 172.8 |
Al2O3 (mp-1143) | <0 0 1> | <1 1 1> | 59.9 |
GaTe (mp-542812) | <1 0 0> | <1 1 1> | 179.6 |
PbSe (mp-2201) | <1 0 0> | <1 0 0> | 311.0 |
SrTiO3 (mp-4651) | <1 1 0> | <1 0 0> | 311.0 |
Al (mp-134) | <1 0 0> | <1 0 0> | 276.4 |
ZrO2 (mp-2858) | <0 0 1> | <1 0 0> | 138.2 |
WS2 (mp-224) | <0 0 1> | <1 1 1> | 239.4 |
GaSb (mp-1156) | <1 0 0> | <1 0 0> | 311.0 |
MoS2 (mp-1434) | <0 0 1> | <1 1 1> | 239.4 |
Au (mp-81) | <1 1 0> | <1 1 0> | 48.9 |
CsI (mp-614603) | <1 0 0> | <1 0 0> | 311.0 |
Au (mp-81) | <1 0 0> | <1 0 0> | 34.6 |
CdSe (mp-2691) | <1 0 0> | <1 0 0> | 311.0 |
AlN (mp-661) | <0 0 1> | <1 1 1> | 59.9 |
ZnO (mp-2133) | <0 0 1> | <1 1 1> | 179.6 |
ZrO2 (mp-2858) | <1 0 1> | <1 1 0> | 342.1 |
Cu (mp-30) | <1 1 0> | <1 1 0> | 146.6 |
Mg (mp-153) | <0 0 1> | <1 1 1> | 239.4 |
SrTiO3 (mp-4651) | <0 0 1> | <1 0 0> | 276.4 |
GaN (mp-804) | <0 0 1> | <1 1 1> | 239.4 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 276.4 |
CaF2 (mp-2741) | <1 0 0> | <1 0 0> | 276.4 |
Au (mp-81) | <1 1 1> | <1 0 0> | 241.9 |
WS2 (mp-224) | <1 1 1> | <1 1 1> | 239.4 |
LaAlO3 (mp-2920) | <0 0 1> | <1 1 1> | 179.6 |
LiAlO2 (mp-3427) | <0 0 1> | <1 0 0> | 138.2 |
Te2W (mp-22693) | <0 1 1> | <1 1 0> | 293.2 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 172.8 |
LaF3 (mp-905) | <0 0 1> | <1 1 1> | 179.6 |
NdGaO3 (mp-3196) | <0 0 1> | <1 0 0> | 276.4 |
Ga2O3 (mp-886) | <1 0 0> | <1 1 0> | 146.6 |
Ag (mp-124) | <1 1 1> | <1 0 0> | 241.9 |
MgF2 (mp-1249) | <1 0 0> | <1 0 0> | 172.8 |
GaP (mp-2490) | <1 0 0> | <1 0 0> | 276.4 |
C (mp-66) | <1 1 0> | <1 1 0> | 146.6 |
YAlO3 (mp-3792) | <1 1 0> | <1 0 0> | 276.4 |
Ga2O3 (mp-886) | <1 0 -1> | <1 0 0> | 311.0 |
LiGaO2 (mp-5854) | <0 1 0> | <1 1 1> | 299.3 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 207.3 |
Mg (mp-153) | <1 0 1> | <1 0 0> | 207.3 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
190 | 24 | 24 | 0 | 0 | 0 |
24 | 190 | 24 | 0 | 0 | 0 |
24 | 24 | 190 | 0 | 0 | 0 |
0 | 0 | 0 | 22 | 0 | 0 |
0 | 0 | 0 | 0 | 22 | 0 |
0 | 0 | 0 | 0 | 0 | 22 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
5.4 | -0.6 | -0.6 | 0 | 0 | 0 |
-0.6 | 5.4 | -0.6 | 0 | 0 | 0 |
-0.6 | -0.6 | 5.4 | 0 | 0 | 0 |
0 | 0 | 0 | 44.4 | 0 | 0 |
0 | 0 | 0 | 0 | 44.4 | 0 |
0 | 0 | 0 | 0 | 0 | 44.4 |
Shear Modulus GV47 GPa |
Bulk Modulus KV79 GPa |
Shear Modulus GR32 GPa |
Bulk Modulus KR79 GPa |
Shear Modulus GVRH39 GPa |
Bulk Modulus KVRH79 GPa |
Elastic Anisotropy2.35 |
Poisson's Ratio0.29 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Sr4SO3 (mp-1079788) | 0.0000 | 0.200 | 3 |
BaSr3O4 (mp-984729) | 0.0000 | 0.044 | 3 |
ScH4Pd3 (mp-981386) | 0.0000 | 0.039 | 3 |
Sr3CdO4 (mp-981103) | 0.0000 | 0.019 | 3 |
SrCa3O4 (mp-978844) | 0.0000 | 0.040 | 3 |
TiH (mp-1060435) | 0.0000 | 0.044 | 2 |
USe (mp-911057) | 0.0000 | 0.146 | 2 |
TcC (mp-1009876) | 0.0000 | 0.650 | 2 |
TcC (mp-1009837) | 0.0000 | 0.650 | 2 |
MgCd (mp-1039157) | 0.0000 | 0.249 | 2 |
Sc (mp-1008681) | 0.0000 | 0.719 | 1 |
Ca (mp-10683) | 0.0000 | 0.393 | 1 |
C (mp-998866) | 0.0000 | 2.763 | 1 |
Sb (mp-133) | 0.0000 | 0.051 | 1 |
Na (mp-1093989) | 0.0000 | 1.074 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: La S |
Final Energy/Atom-6.6993 eV |
Corrected Energy-14.0621 eV
-14.0621 eV = -13.3987 eV (uncorrected energy) - 0.6635 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)