Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.614 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.87 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap1.956 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 0 1> | 201.4 |
AlN (mp-661) | <1 1 0> | <1 0 -1> | 249.2 |
SiO2 (mp-6930) | <1 0 0> | <1 0 -1> | 249.2 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 100.7 |
YVO4 (mp-19133) | <1 1 1> | <1 0 -1> | 249.2 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 102.5 |
LiGaO2 (mp-5854) | <0 0 1> | <1 0 -1> | 249.2 |
TeO2 (mp-2125) | <1 1 0> | <0 0 1> | 100.7 |
SiC (mp-7631) | <1 1 1> | <1 0 -1> | 249.2 |
SiC (mp-7631) | <1 1 0> | <1 0 -1> | 249.2 |
Mg (mp-153) | <1 0 0> | <1 0 -1> | 249.2 |
Mg (mp-153) | <1 0 1> | <0 1 0> | 151.8 |
MgO (mp-1265) | <1 0 0> | <0 1 1> | 182.1 |
GdScO3 (mp-5690) | <1 1 0> | <0 0 1> | 201.4 |
MoSe2 (mp-1634) | <1 0 0> | <1 0 -1> | 249.2 |
BaTiO3 (mp-5986) | <0 0 1> | <1 0 1> | 160.5 |
BaTiO3 (mp-5986) | <1 0 0> | <0 0 1> | 100.7 |
Ga2O3 (mp-886) | <1 0 -1> | <0 1 0> | 151.8 |
Ga2O3 (mp-886) | <1 0 1> | <0 1 1> | 182.1 |
WS2 (mp-224) | <1 0 0> | <1 1 0> | 183.1 |
WSe2 (mp-1821) | <1 0 1> | <1 0 -1> | 249.2 |
WSe2 (mp-1821) | <1 0 0> | <1 0 -1> | 249.2 |
ZrO2 (mp-2858) | <0 0 1> | <1 0 -1> | 249.2 |
ZrO2 (mp-2858) | <0 1 0> | <1 0 -1> | 249.2 |
ZrO2 (mp-2858) | <1 0 -1> | <0 1 1> | 182.1 |
YAlO3 (mp-3792) | <0 0 1> | <1 0 -1> | 249.2 |
MgAl2O4 (mp-3536) | <1 0 0> | <0 0 1> | 201.4 |
SiC (mp-8062) | <1 0 0> | <1 0 -1> | 249.2 |
SrTiO3 (mp-4651) | <1 1 0> | <1 0 -1> | 124.6 |
SrTiO3 (mp-4651) | <0 0 1> | <1 0 -1> | 124.6 |
Al2O3 (mp-1143) | <0 0 1> | <1 0 1> | 160.5 |
Cu (mp-30) | <1 0 0> | <1 1 -1> | 196.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Pt4(O3F8)3 (mp-675449) | 0.4918 | 0.179 | 3 |
Te4WCl6 (mp-616228) | 0.5937 | 0.024 | 3 |
NbTeCl9 (mp-669348) | 0.5694 | 0.003 | 3 |
TaTeCl9 (mp-669345) | 0.5630 | 0.000 | 3 |
Ta(TeBr3)2 (mp-29427) | 0.5254 | 0.005 | 3 |
TeAs(SeF3)2 (mp-651161) | 0.5301 | 0.104 | 4 |
TeAs(IF2)3 (mp-555034) | 0.6128 | 0.084 | 4 |
AsSe(IF2)3 (mp-559575) | 0.6154 | 0.006 | 4 |
AsS3(ClF2)3 (mp-23112) | 0.5528 | 0.039 | 4 |
AsS3(ClF2)3 (mp-562439) | 0.5909 | 0.039 | 4 |
Sb4F15 (mp-28180) | 0.7260 | 0.001 | 2 |
MgCoH16(ClO2)4 (mp-743870) | 0.6195 | 0.011 | 5 |
HfMo2Se8(Cl7O)2 (mp-629742) | 0.6093 | 0.024 | 5 |
ZrMo2Se8(Cl7O)2 (mp-565934) | 0.6161 | 0.013 | 5 |
CaMg2H24(ClO2)6 (mp-696387) | 0.5959 | 0.009 | 5 |
FeH12Pt(ClO)6 (mp-605175) | 0.7337 | 0.000 | 5 |
Te2As2Se8S(OF6)2 (mp-557236) | 0.6650 | 0.074 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: F Cl As Se |
Final Energy/Atom-3.7229 eV |
Corrected Energy-193.5898 eV
-193.5898 eV = -193.5898 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)