material

Hf5Al3

ID:

mp-2361

DOI:

10.17188/1199616


Tags: Pentahafnium trialuminium - intersitial oxygen Aluminium hafnium (3/5) Hafnium aluminide (5/3)

Material Details

Final Magnetic Moment
0.036 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.292 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.053 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
9.93 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Hf4Al3 + Hf
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P63/mcm [193]
Hall
-P 6c 2
Point Group
6/mmm
Crystal System
hexagonal

Electronic Structure

Topological data for ICSD ID 57898 from Topological Materials Database
Topological Classification
SM*
Subclassification
ESFD
Crossing Type
Point
* Semimetal
Enforced Semimetal with Fermi point Degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
CdTe (mp-406) <1 1 1> <0 0 1> 0.002 228.0
ZnSe (mp-1190) <1 1 1> <0 0 1> 0.003 57.0
Ni (mp-23) <1 0 0> <1 1 1> 0.003 98.4
AlN (mp-661) <1 0 1> <1 1 0> 0.004 160.4
InSb (mp-20012) <1 1 1> <0 0 1> 0.006 228.0
BaF2 (mp-1029) <1 0 0> <1 1 1> 0.009 196.8
Ni (mp-23) <1 1 0> <1 0 0> 0.012 138.9
AlN (mp-661) <0 0 1> <0 0 1> 0.013 228.0
LaAlO3 (mp-2920) <1 0 1> <0 0 1> 0.016 228.0
GaAs (mp-2534) <1 1 1> <0 0 1> 0.019 57.0
GaN (mp-804) <0 0 1> <0 0 1> 0.020 171.0
Al (mp-134) <1 1 0> <1 0 0> 0.021 46.3
TiO2 (mp-2657) <1 1 0> <1 0 1> 0.024 293.8
MgF2 (mp-1249) <1 1 0> <1 0 0> 0.036 185.3
CdTe (mp-406) <1 1 0> <1 0 0> 0.039 185.3
ZnSe (mp-1190) <1 1 0> <1 0 0> 0.044 46.3
TeO2 (mp-2125) <1 0 1> <1 0 0> 0.045 231.6
MgF2 (mp-1249) <0 0 1> <1 1 1> 0.048 196.8
InSb (mp-20012) <1 1 0> <1 0 0> 0.052 185.3
KTaO3 (mp-3614) <1 1 0> <1 0 0> 0.058 46.3
DyScO3 (mp-31120) <1 0 1> <1 0 0> 0.064 277.9
CdWO4 (mp-19387) <0 1 1> <1 0 0> 0.066 324.2
GdScO3 (mp-5690) <0 1 1> <1 0 1> 0.070 220.3
BaTiO3 (mp-5986) <1 1 1> <1 0 0> 0.070 231.6
Ge (mp-32) <1 1 1> <0 0 1> 0.075 57.0
BaTiO3 (mp-5986) <1 1 0> <1 1 0> 0.078 240.7
GaAs (mp-2534) <1 1 0> <1 0 0> 0.078 46.3
TbScO3 (mp-31119) <1 0 1> <1 0 0> 0.087 277.9
Te2Mo (mp-602) <0 0 1> <0 0 1> 0.092 228.0
C (mp-48) <0 0 1> <1 0 0> 0.093 185.3
SiC (mp-11714) <0 0 1> <1 0 0> 0.093 231.6
TiO2 (mp-2657) <0 0 1> <1 1 1> 0.094 196.8
SiC (mp-7631) <0 0 1> <1 0 0> 0.097 231.6
NaCl (mp-22862) <1 1 0> <1 0 0> 0.103 46.3
SiO2 (mp-6930) <1 0 0> <1 0 1> 0.122 220.3
LiF (mp-1138) <1 0 0> <1 0 0> 0.127 231.6
Cu (mp-30) <1 0 0> <1 0 0> 0.132 324.2
TePb (mp-19717) <1 1 0> <1 0 0> 0.136 185.3
C (mp-48) <1 0 1> <1 0 1> 0.137 220.3
Ge (mp-32) <1 1 0> <1 0 0> 0.159 46.3
NaCl (mp-22862) <1 0 0> <1 1 0> 0.162 160.4
MgO (mp-1265) <1 1 0> <1 0 0> 0.162 277.9
TiO2 (mp-2657) <1 1 1> <1 0 0> 0.169 324.2
CdS (mp-672) <1 0 1> <0 0 1> 0.181 228.0
ZrO2 (mp-2858) <1 1 0> <1 0 0> 0.183 277.9
DyScO3 (mp-31120) <0 0 1> <1 0 0> 0.183 92.6
AlN (mp-661) <1 0 0> <1 0 1> 0.183 220.3
PbSe (mp-2201) <1 0 0> <1 1 1> 0.186 196.8
SiO2 (mp-6930) <1 0 1> <1 0 0> 0.192 138.9
ZnO (mp-2133) <1 0 1> <1 0 1> 0.197 293.8
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
186 100 66 0 0 0
100 186 66 0 0 0
66 66 169 0 0 0
0 0 0 47 0 0
0 0 0 0 47 0
0 0 0 0 0 43
Compliance Tensor Sij (10-12Pa-1)
7.9 -3.6 -1.7 0 0 0
-3.6 7.9 -1.7 0 0 0
-1.7 -1.7 7.2 0 0 0
0 0 0 21.3 0 0
0 0 0 0 21.3 0
0 0 0 0 0 23.1
Shear Modulus GV
48 GPa
Bulk Modulus KV
112 GPa
Shear Modulus GR
47 GPa
Bulk Modulus KR
110 GPa
Shear Modulus GVRH
48 GPa
Bulk Modulus KVRH
111 GPa
Elastic Anisotropy
0.10
Poisson's Ratio
0.31

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Hf3Nb2Ga3 (mp-30644) 0.2868 0.000 3
Ca5MnPb3 (mp-680842) 0.7225 0.181 3
Zr3Ti2Ga3 (mp-30676) 0.2118 0.000 3
Ta5Ge3 (mp-17013) 0.0468 0.088 2
Hf5Ga3 (mp-22337) 0.1433 0.000 2
Ti5Ga3 (mp-30674) 0.1294 0.017 2
Fe5Si3 (mp-449) 0.0831 0.034 2
Mn5Ge3 (mp-617291) 0.1399 0.000 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Hf_pv Al
Final Energy/Atom
-7.9195 eV
Corrected Energy
-126.7121 eV
Uncorrected energy = -126.7121 eV Corrected energy = -126.7121 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 60633
  • 57898
  • 608077
Submitted by
User remarks:
  • Pentahafnium trialuminium - intersitial oxygen

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)