Final Magnetic Moment1.995 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.599 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.005 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.97 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNpO2 + Cs7Np3(Cl2O)6 + CsCl |
Band Gap0.228 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/c [15] |
Hall-C 2yc |
Point Group2/m |
Crystal Systemmonoclinic |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 0 1> | 233.4 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 194.1 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 194.1 |
InAs (mp-20305) | <1 1 1> | <1 0 0> | 194.1 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 194.1 |
CdS (mp-672) | <0 0 1> | <1 0 1> | 182.6 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 291.1 |
Te2W (mp-22693) | <1 1 0> | <1 0 -1> | 112.7 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 233.4 |
YVO4 (mp-19133) | <1 0 1> | <1 0 0> | 291.1 |
Ag (mp-124) | <1 0 0> | <1 0 -1> | 225.5 |
BN (mp-984) | <1 0 0> | <0 0 1> | 116.7 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 1> | 182.6 |
Al (mp-134) | <1 1 1> | <1 0 0> | 194.1 |
LiGaO2 (mp-5854) | <1 0 0> | <1 0 0> | 291.1 |
LiGaO2 (mp-5854) | <1 1 0> | <1 0 0> | 97.0 |
CdTe (mp-406) | <1 0 0> | <1 0 -1> | 225.5 |
SiC (mp-7631) | <1 0 0> | <0 0 1> | 233.4 |
SiC (mp-7631) | <1 1 0> | <0 0 1> | 233.4 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 233.4 |
Ge3(BiO3)4 (mp-23560) | <1 1 1> | <1 0 0> | 194.1 |
GdScO3 (mp-5690) | <1 1 1> | <1 0 0> | 291.1 |
LaF3 (mp-905) | <0 0 1> | <1 0 1> | 182.6 |
LaF3 (mp-905) | <1 0 1> | <1 0 0> | 291.1 |
LaF3 (mp-905) | <1 1 0> | <1 0 1> | 182.6 |
PbS (mp-21276) | <1 1 1> | <1 0 0> | 194.1 |
InP (mp-20351) | <1 1 1> | <1 0 0> | 194.1 |
Ni (mp-23) | <1 1 1> | <1 0 0> | 194.1 |
InSb (mp-20012) | <1 0 0> | <1 0 -1> | 225.5 |
PbSe (mp-2201) | <1 1 1> | <1 0 0> | 194.1 |
NdGaO3 (mp-3196) | <1 1 1> | <1 0 0> | 291.1 |
Ga2O3 (mp-886) | <1 0 1> | <1 0 -1> | 225.5 |
Au (mp-81) | <1 0 0> | <1 0 -1> | 225.5 |
Au (mp-81) | <1 1 0> | <1 0 -1> | 225.5 |
CdSe (mp-2691) | <1 1 1> | <1 0 0> | 194.1 |
C (mp-48) | <1 0 0> | <0 0 1> | 116.7 |
ZrO2 (mp-2858) | <0 0 1> | <1 0 -1> | 112.7 |
ZrO2 (mp-2858) | <1 1 -1> | <1 0 -1> | 225.5 |
Ge(Bi3O5)4 (mp-23352) | <1 1 1> | <1 0 0> | 194.1 |
YAlO3 (mp-3792) | <0 1 0> | <0 0 1> | 116.7 |
YAlO3 (mp-3792) | <1 1 0> | <1 0 -1> | 112.7 |
CdWO4 (mp-19387) | <0 0 1> | <0 1 0> | 181.8 |
CdWO4 (mp-19387) | <1 0 1> | <1 0 -1> | 225.5 |
TiO2 (mp-390) | <0 0 1> | <0 0 1> | 116.7 |
TiO2 (mp-390) | <1 0 0> | <1 0 0> | 291.1 |
MgF2 (mp-1249) | <1 1 0> | <1 0 -1> | 225.5 |
GaSb (mp-1156) | <1 1 1> | <1 0 0> | 194.1 |
Cu (mp-30) | <1 0 0> | <1 0 0> | 291.1 |
LiAlO2 (mp-3427) | <1 1 0> | <1 0 0> | 97.0 |
ZnTe (mp-2176) | <1 1 1> | <1 0 0> | 194.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CaV2O6 (mvc-11947) | 0.6240 | 0.131 | 3 |
BaWO4 (mp-641366) | 0.5319 | 0.052 | 3 |
Rb2PdI6 (mp-29936) | 0.6601 | 0.000 | 3 |
Ba3(BN2)2 (mp-30905) | 0.6132 | 0.000 | 3 |
CsSb2F7 (mp-561569) | 0.5936 | 0.012 | 3 |
KI(OF)2 (mp-753054) | 0.6648 | 0.039 | 4 |
K2OsNCl5 (mp-569207) | 0.6727 | 0.111 | 4 |
NbTlCl4O (mp-561523) | 0.5751 | 0.000 | 4 |
TlAg(CN)2 (mp-621981) | 0.7164 | 0.253 | 4 |
WXeOF6 (mp-565584) | 0.6776 | 0.134 | 4 |
MoO3 (mp-715463) | 0.6660 | 0.038 | 2 |
MoO3 (mp-510584) | 0.6874 | 0.039 | 2 |
K2IrCBr5O (mp-648833) | 0.6463 | 0.206 | 5 |
K2OsCBr5O (mp-556047) | 0.7482 | 0.000 | 5 |
Tl2OsCBr2OF3 (mp-556622) | 0.7205 | 0.014 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Cs_sv Np Cl O |
Final Energy/Atom-5.5134 eV |
Corrected Energy-113.0773 eV
-113.0773 eV = -110.2681 eV (uncorrected energy) - 2.8092 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)