Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.235 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.71 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap5.237 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFdd2 [43] |
HallF 2 2d |
Point Groupmm2 |
Crystal Systemorthorhombic |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 121.4 |
LaAlO3 (mp-2920) | <1 0 0> | <1 0 1> | 145.8 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 244.9 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 121.4 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 121.4 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 242.2 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 161.4 |
Te2W (mp-22693) | <1 1 0> | <0 1 1> | 114.8 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 161.4 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 242.2 |
CdS (mp-672) | <1 1 0> | <0 1 0> | 244.9 |
YVO4 (mp-19133) | <1 0 0> | <0 1 1> | 229.6 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 242.2 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 242.2 |
MoS2 (mp-1434) | <0 0 1> | <0 1 0> | 244.9 |
BN (mp-984) | <1 0 0> | <0 1 1> | 114.8 |
BN (mp-984) | <1 1 1> | <1 1 1> | 167.1 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 242.2 |
TeO2 (mp-2125) | <0 1 1> | <1 0 1> | 145.8 |
LiGaO2 (mp-5854) | <1 1 1> | <0 1 0> | 163.3 |
SiC (mp-7631) | <1 0 0> | <1 0 0> | 242.8 |
Ge3(BiO3)4 (mp-23560) | <1 1 0> | <0 0 1> | 161.4 |
MgO (mp-1265) | <1 1 0> | <0 1 1> | 229.6 |
C (mp-66) | <1 1 0> | <0 0 1> | 161.4 |
C (mp-66) | <1 1 1> | <0 0 1> | 242.2 |
Mg (mp-153) | <0 0 1> | <0 1 0> | 244.9 |
GdScO3 (mp-5690) | <1 1 0> | <0 1 0> | 244.9 |
Mg (mp-153) | <1 1 1> | <1 0 0> | 121.4 |
KP(HO2)2 (mp-23959) | <1 0 0> | <0 0 1> | 242.2 |
LaF3 (mp-905) | <1 0 0> | <0 0 1> | 161.4 |
GaP (mp-2490) | <1 0 0> | <1 0 0> | 121.4 |
NdGaO3 (mp-3196) | <0 0 1> | <1 0 0> | 121.4 |
Ga2O3 (mp-886) | <1 0 1> | <0 1 1> | 229.6 |
Ga2O3 (mp-886) | <1 1 -1> | <1 1 1> | 167.1 |
ZrO2 (mp-2858) | <1 1 -1> | <0 1 1> | 229.6 |
ZrO2 (mp-2858) | <1 1 1> | <0 1 0> | 244.9 |
TbScO3 (mp-31119) | <1 1 0> | <0 0 1> | 242.2 |
Ni (mp-23) | <1 0 0> | <0 1 0> | 244.9 |
YAlO3 (mp-3792) | <0 1 0> | <0 1 1> | 114.8 |
NdGaO3 (mp-3196) | <1 1 0> | <1 0 0> | 121.4 |
MgF2 (mp-1249) | <1 1 0> | <0 1 1> | 229.6 |
Si (mp-149) | <1 0 0> | <1 0 0> | 121.4 |
ZnO (mp-2133) | <1 1 1> | <0 1 0> | 244.9 |
SrTiO3 (mp-4651) | <0 0 1> | <1 0 0> | 121.4 |
SrTiO3 (mp-4651) | <1 1 0> | <1 0 0> | 121.4 |
WS2 (mp-224) | <0 0 1> | <0 1 0> | 244.9 |
C (mp-48) | <1 0 0> | <0 1 1> | 114.8 |
ZrO2 (mp-2858) | <0 1 0> | <1 1 1> | 167.1 |
LiAlO2 (mp-3427) | <0 0 1> | <1 0 0> | 242.8 |
LiAlO2 (mp-3427) | <1 1 0> | <0 1 1> | 229.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Piezoelectric Tensor eij (C/m2) |
|||||
---|---|---|---|---|---|
0.00000 | 0.00000 | 0.00000 | 0.00000 | -0.01914 | 0.00000 |
0.00000 | 0.00000 | 0.00000 | 0.07491 | 0.00000 | 0.00000 |
0.05746 | 0.13329 | -0.04110 | 0.00000 | 0.00000 | 0.00000 |
Piezoelectric Modulus ‖eij‖max0.15085 C/m2 |
Crystallographic Direction vmax |
---|
0.00000 |
0.00000 |
1.00000 |
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
2.31 | 0.00 | 0.00 |
0.00 | 2.28 | 0.00 |
0.00 | 0.00 | 2.21 |
Dielectric Tensor εij (total) |
||
---|---|---|
7.40 | 0.00 | 0.00 |
0.00 | 8.47 | 0.00 |
0.00 | 0.00 | 5.11 |
Polycrystalline dielectric constant
εpoly∞
2.27
|
Polycrystalline dielectric constant
εpoly
6.99
|
Refractive Index n1.51 |
Potentially ferroelectric?Unknown |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Rb_sv P H O |
Final Energy/Atom-5.9669 eV |
Corrected Energy-100.9667 eV
Uncorrected energy = -95.4707 eV
Composition-based energy adjustment (-0.687 eV/atom x 8.0 atoms) = -5.4960 eV
Corrected energy = -100.9667 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)