material

LiH

ID:

mp-23703

DOI:

10.17188/1199672


Tags: Lithium hydride - 1 Lithium hydride Lithium hydride - 2 Lithium hydride (1/1) Lithium deuteride

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.496 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
0.82 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
3.175 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Fm3m [225]
Hall
-F 4 2 3
Point Group
m3m
Crystal System
cubic

Electronic Structure

Topological data for ICSD ID 26873 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

Vibrational Properties

Reference for phonon calculations and visualization: Visualize with phononwebsite

Phonon dispersion

Density of States
Warning! These calculations were performed using a PBEsol exchange correlation functional in the framework of DFPT using the Abinit code. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
TePb (mp-19717) <1 1 0> <1 1 0> 0.000 182.6
MgO (mp-1265) <1 0 0> <1 0 0> 0.001 145.2
MgO (mp-1265) <1 1 0> <1 1 0> 0.001 205.4
Fe3O4 (mp-19306) <1 0 0> <1 0 0> 0.001 145.2
Fe3O4 (mp-19306) <1 1 0> <1 1 0> 0.001 205.4
NaCl (mp-22862) <1 0 0> <1 0 0> 0.002 32.3
NaCl (mp-22862) <1 1 0> <1 1 0> 0.002 45.6
YVO4 (mp-19133) <0 0 1> <1 0 0> 0.002 209.8
BaTiO3 (mp-5986) <1 1 0> <1 1 1> 0.004 167.7
ZnO (mp-2133) <0 0 1> <1 1 1> 0.004 28.0
C (mp-48) <0 0 1> <1 1 1> 0.005 83.9
LiGaO2 (mp-5854) <0 1 0> <1 1 0> 0.005 296.7
GdScO3 (mp-5690) <1 1 0> <1 0 0> 0.005 64.6
Ge3(BiO3)4 (mp-23560) <1 1 1> <1 1 1> 0.006 195.7
KTaO3 (mp-3614) <1 0 0> <1 0 0> 0.006 16.1
KTaO3 (mp-3614) <1 1 0> <1 1 0> 0.006 22.8
KTaO3 (mp-3614) <1 1 1> <1 1 1> 0.006 28.0
PbS (mp-21276) <1 0 0> <1 0 0> 0.007 145.2
BaTiO3 (mp-5986) <0 0 1> <1 0 0> 0.007 16.1
PbS (mp-21276) <1 1 0> <1 1 0> 0.007 205.4
BN (mp-984) <1 0 1> <1 1 0> 0.009 182.6
Cu (mp-30) <1 1 0> <1 1 0> 0.012 205.4
TiO2 (mp-390) <0 0 1> <1 0 0> 0.012 129.1
C (mp-66) <1 0 0> <1 0 0> 0.013 64.6
CeO2 (mp-20194) <1 1 0> <1 1 0> 0.014 251.1
Al (mp-134) <1 0 0> <1 0 0> 0.014 16.1
Ge(Bi3O5)4 (mp-23352) <1 0 0> <1 0 0> 0.015 209.8
Si (mp-149) <1 1 0> <1 1 0> 0.015 251.1
Al (mp-134) <1 1 0> <1 1 0> 0.015 22.8
Al (mp-134) <1 1 1> <1 1 1> 0.015 28.0
ZnO (mp-2133) <1 1 0> <1 1 0> 0.018 91.3
Cu (mp-30) <1 0 0> <1 0 0> 0.021 64.6
KCl (mp-23193) <1 0 0> <1 0 0> 0.023 80.7
Ga2O3 (mp-886) <1 0 1> <1 0 0> 0.023 322.8
LiGaO2 (mp-5854) <1 1 0> <1 1 1> 0.025 195.7
AlN (mp-661) <0 0 1> <1 1 1> 0.027 111.8
BaTiO3 (mp-5986) <1 1 1> <1 1 0> 0.027 114.1
InAs (mp-20305) <1 1 1> <1 1 1> 0.029 195.7
TbScO3 (mp-31119) <1 1 0> <1 0 0> 0.031 64.6
LaAlO3 (mp-2920) <1 1 0> <1 1 0> 0.032 251.1
BaTiO3 (mp-5986) <1 0 0> <1 1 0> 0.033 68.5
ZnTe (mp-2176) <1 1 1> <1 1 1> 0.033 195.7
GaSe (mp-1943) <0 0 1> <1 1 1> 0.034 111.8
Ni (mp-23) <1 1 0> <1 1 0> 0.036 68.5
DyScO3 (mp-31120) <1 0 0> <1 1 0> 0.037 45.6
TiO2 (mp-390) <1 0 0> <1 1 1> 0.037 111.8
Ni (mp-23) <1 1 1> <1 1 1> 0.037 83.9
CdS (mp-672) <1 1 1> <1 0 0> 0.039 209.8
CdWO4 (mp-19387) <0 0 1> <1 0 0> 0.043 242.1
MgF2 (mp-1249) <1 1 1> <1 0 0> 0.044 242.1
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
84 13 13 0 0 0
13 84 13 0 0 0
13 13 84 0 0 0
0 0 0 48 0 0
0 0 0 0 48 0
0 0 0 0 0 48
Compliance Tensor Sij (10-12Pa-1)
12.3 -1.6 -1.6 0 0 0
-1.6 12.3 -1.6 0 0 0
-1.6 -1.6 12.3 0 0 0
0 0 0 20.8 0 0
0 0 0 0 20.8 0
0 0 0 0 0 20.8
Shear Modulus GV
43 GPa
Bulk Modulus KV
37 GPa
Shear Modulus GR
42 GPa
Bulk Modulus KR
37 GPa
Shear Modulus GVRH
43 GPa
Bulk Modulus KVRH
37 GPa
Elastic Anisotropy
0.10
Poisson's Ratio
0.08

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
4.36 -0.00 -0.00
-0.00 4.36 0.00
-0.00 0.00 4.36
Dielectric Tensor εij (total)
14.26 -0.00 -0.00
-0.00 14.26 0.00
-0.00 0.00 14.26
Polycrystalline dielectric constant εpoly
(electronic contribution)
4.36
Polycrystalline dielectric constant εpoly
(total)
14.26
Refractive Index n
2.09
Potentially ferroelectric?
Unknown

Equations of State

Reference:
Equation E0 (eV) V0 (Å3) B C
mie_gruneisen -3.057 8.112 2.035 2.984
pack_evans_james -3.057 8.112 0.226 2.333
vinet -3.057 8.110 2.053 3.531
tait -3.057 8.108 0.229 4.424
birch_euler -3.057 8.110 0.256 -0.637
pourier_tarantola -3.057 8.110 0.038 1.345
birch_lagrange -3.058 8.112 0.138 5.171
murnaghan -3.057 8.116 0.222 2.261
Equations reference

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Sr4SO3 (mp-1079788) 0.0000 0.200 3
BaSr3O4 (mp-984729) 0.0000 0.044 3
ScH4Pd3 (mp-981386) 0.0000 0.114 3
Sr3CdO4 (mp-981103) 0.0000 0.019 3
SrCa3O4 (mp-978844) 0.0000 0.040 3
TiH (mp-1060435) 0.0000 0.045 2
USe (mp-911057) 0.0000 0.000 2
TcC (mp-1009876) 0.0000 0.650 2
TcC (mp-1009837) 0.0000 0.650 2
MgCd (mp-1039157) 0.0000 0.249 2
Sc (mp-1008681) 0.0000 0.719 1
Ca (mp-10683) 0.0000 0.400 1
C (mp-998866) 0.0000 2.755 1
Sb (mp-133) 0.0000 0.051 1
Na (mp-1093989) 0.0000 1.084 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
700 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Li_sv H
Final Energy/Atom
-3.0569 eV
Corrected Energy
-6.2927 eV
Uncorrected energy = -6.1137 eV Composition-based energy adjustment (-0.179 eV/atom x 1.0 atoms) = -0.1790 eV Corrected energy = -6.2927 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 638265
  • 638263
  • 44748
  • 61751
  • 173192
  • 61749
  • 61754
  • 61752
  • 26874
  • 638266
  • 173177
  • 173178
  • 26873
  • 157495
  • 173205
  • 168789
  • 61750
  • 187680
  • 28557
  • 61753
  • 187681
  • 56066
  • 53975
  • 603869
Submitted by
User remarks:
  • Lithium hydride

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)