material

MnPd

ID:

mp-238

DOI:

10.17188/1199737


Tags: Manganese palladium (1/1)

Material Details

Final Magnetic Moment
4.459 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
FM
Formation Energy / Atom
-0.200 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.002 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
8.76 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Mn3Pd5 + Mn
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P4/mmm [123]
Hall
-P 4 2
Point Group
4/mmm
Crystal System
tetragonal

Electronic Structure

Topological data for ICSD ID 104938 from Topological Materials Database
Topological Classification
SM*
Subclassification
ESFD
Crossing Type
Point
* Semimetal
Enforced Semimetal with Fermi point Degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Al (mp-134) <1 0 0> <0 0 1> 0.001 81.7
KCl (mp-23193) <1 0 0> <0 0 1> 0.002 81.7
MgO (mp-1265) <1 0 0> <0 0 1> 0.002 18.1
Cu (mp-30) <1 0 0> <0 0 1> 0.003 118.0
TiO2 (mp-390) <0 0 1> <0 0 1> 0.003 72.6
Fe3O4 (mp-19306) <1 0 0> <0 0 1> 0.006 72.6
ZrO2 (mp-2858) <1 1 1> <1 0 1> 0.015 204.2
KTaO3 (mp-3614) <1 0 0> <0 0 1> 0.018 81.7
TbScO3 (mp-31119) <0 1 1> <1 0 0> 0.022 162.4
AlN (mp-661) <1 0 1> <1 0 0> 0.024 71.1
PbS (mp-21276) <1 0 0> <0 0 1> 0.033 36.3
DyScO3 (mp-31120) <0 0 1> <1 1 0> 0.044 186.6
CdWO4 (mp-19387) <0 1 0> <1 0 0> 0.046 132.0
GaN (mp-804) <1 0 1> <1 1 1> 0.051 152.9
GdScO3 (mp-5690) <0 1 1> <1 0 0> 0.052 162.4
LiTaO3 (mp-3666) <0 0 1> <1 0 1> 0.054 163.4
BaTiO3 (mp-5986) <1 1 0> <1 1 0> 0.055 71.8
ZnSe (mp-1190) <1 0 0> <0 0 1> 0.057 163.3
YVO4 (mp-19133) <1 1 0> <1 1 0> 0.060 129.2
KTaO3 (mp-3614) <1 1 1> <1 0 0> 0.071 253.8
Al (mp-134) <1 1 1> <1 0 0> 0.073 253.8
LiGaO2 (mp-5854) <0 1 1> <0 0 1> 0.076 217.8
MgO (mp-1265) <1 1 1> <0 0 1> 0.078 217.8
DyScO3 (mp-31120) <0 1 1> <1 0 0> 0.078 162.4
LiGaO2 (mp-5854) <1 0 0> <1 0 1> 0.089 177.0
GaAs (mp-2534) <1 0 0> <0 0 1> 0.096 163.3
LaAlO3 (mp-2920) <1 0 1> <1 1 0> 0.102 301.5
CdS (mp-672) <1 0 0> <1 1 0> 0.103 28.7
SiO2 (mp-6930) <1 0 1> <1 0 1> 0.112 177.0
WSe2 (mp-1821) <1 0 0> <1 0 0> 0.117 50.8
NaCl (mp-22862) <1 1 0> <1 1 1> 0.118 135.9
TeO2 (mp-2125) <0 1 1> <1 1 0> 0.119 229.7
CeO2 (mp-20194) <1 0 0> <0 0 1> 0.120 118.0
Fe2O3 (mp-24972) <0 0 1> <1 0 0> 0.122 91.4
NdGaO3 (mp-3196) <0 1 0> <0 0 1> 0.122 172.4
LiGaO2 (mp-5854) <1 1 0> <0 0 1> 0.127 190.6
LiNbO3 (mp-3731) <0 0 1> <1 0 1> 0.129 163.4
Si (mp-149) <1 0 0> <0 0 1> 0.129 118.0
Al2O3 (mp-1143) <1 0 1> <1 1 0> 0.130 201.0
Te2W (mp-22693) <0 1 0> <1 0 0> 0.138 213.2
Ga2O3 (mp-886) <1 1 0> <1 0 1> 0.141 217.9
TbScO3 (mp-31119) <0 0 1> <1 1 0> 0.146 186.6
GaSe (mp-1943) <0 0 1> <1 1 0> 0.153 114.9
YVO4 (mp-19133) <1 1 1> <1 0 0> 0.157 253.8
C (mp-48) <1 1 1> <0 0 1> 0.162 99.8
DyScO3 (mp-31120) <1 0 0> <1 1 1> 0.164 135.9
TiO2 (mp-390) <1 1 1> <1 1 0> 0.169 330.2
CdWO4 (mp-19387) <0 0 1> <0 0 1> 0.170 90.7
Ge (mp-32) <1 0 0> <0 0 1> 0.180 163.3
Cu (mp-30) <1 1 1> <1 0 0> 0.184 91.4
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
192 81 125 0 0 0
81 192 125 0 0 0
125 125 161 0 0 0
0 0 0 84 0 0
0 0 0 0 84 0
0 0 0 0 0 65
Compliance Tensor Sij (10-12Pa-1)
10.8 1.8 -9.7 0 0 0
1.8 10.8 -9.7 0 0 0
-9.7 -9.7 21.3 0 0 0
0 0 0 11.9 0 0
0 0 0 0 11.9 0
0 0 0 0 0 15.3
Shear Modulus GV
61 GPa
Bulk Modulus KV
134 GPa
Shear Modulus GR
42 GPa
Bulk Modulus KR
133 GPa
Shear Modulus GVRH
51 GPa
Bulk Modulus KVRH
134 GPa
Elastic Anisotropy
2.31
Poisson's Ratio
0.33

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Li2CuGe (mp-676117) 0.3918 0.008 3
YHfMg6 (mp-1022697) 0.2629 0.089 3
FeSnRh2 (mp-1018062) 0.7286 0.000 3
UAg3 (mp-979274) 0.0483 0.367 2
Ru3Cl (mp-974467) 0.0408 1.142 2
Rh3F (mp-974386) 0.0927 0.717 2
TaRu (mp-1601) 0.0482 0.000 2
NbRu (mp-432) 0.0703 0.000 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Mn_pv Pd
Final Energy/Atom
-7.3707 eV
Corrected Energy
-14.7413 eV
Uncorrected energy = -14.7413 eV Corrected energy = -14.7413 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 104938
  • 643303
Submitted by
User remarks:
  • Manganese palladium (1/1)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)