Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingUnknown |
Formation Energy / Atom-1.580 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.09 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFm3m [225] |
Hall-F 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <1 0 0> | 292.9 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 310.7 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 329.5 |
GaN (mp-804) | <0 0 1> | <1 1 1> | 63.4 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 219.7 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 146.5 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 109.8 |
SiO2 (mp-6930) | <1 0 1> | <1 1 1> | 317.1 |
SiO2 (mp-6930) | <1 1 1> | <1 0 0> | 256.3 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 329.5 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 329.5 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 36.6 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 292.9 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 146.5 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 207.1 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 183.1 |
CdS (mp-672) | <1 0 1> | <1 1 0> | 258.9 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 146.5 |
LiF (mp-1138) | <1 1 1> | <1 1 1> | 253.7 |
Te2W (mp-22693) | <0 1 1> | <1 0 0> | 292.9 |
YVO4 (mp-19133) | <1 0 0> | <1 1 1> | 190.2 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 183.1 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 109.8 |
Te2Mo (mp-602) | <1 1 1> | <1 0 0> | 183.1 |
Ag (mp-124) | <1 1 1> | <1 0 0> | 183.1 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 109.8 |
AlN (mp-661) | <1 1 1> | <1 1 0> | 207.1 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 146.5 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 292.9 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 292.9 |
BN (mp-984) | <1 0 1> | <1 0 0> | 219.7 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 183.1 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 310.7 |
Bi2Se3 (mp-541837) | <1 0 0> | <1 0 0> | 256.3 |
Al (mp-134) | <1 0 0> | <1 0 0> | 146.5 |
Al (mp-134) | <1 1 0> | <1 1 0> | 207.1 |
Al (mp-134) | <1 1 1> | <1 1 1> | 190.2 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 51.8 |
InAs (mp-20305) | <1 1 1> | <1 1 1> | 63.4 |
KTaO3 (mp-3614) | <1 1 1> | <1 1 1> | 190.2 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 0> | 219.7 |
TeO2 (mp-2125) | <0 0 1> | <1 0 0> | 292.9 |
TeO2 (mp-2125) | <1 1 0> | <1 0 0> | 292.9 |
SiC (mp-7631) | <1 0 1> | <1 0 0> | 183.1 |
SiC (mp-7631) | <1 1 0> | <1 1 0> | 155.3 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 207.1 |
Te2W (mp-22693) | <0 0 1> | <1 1 0> | 258.9 |
YVO4 (mp-19133) | <0 0 1> | <1 1 1> | 317.1 |
Fe3O4 (mp-19306) | <1 0 0> | <1 0 0> | 73.2 |
Fe3O4 (mp-19306) | <1 1 0> | <1 1 0> | 103.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
LiNi6O6F (mp-765554) | 0.2658 | 0.060 | 4 |
Li2TiCrO4 (mp-773295) | 0.2736 | 0.085 | 4 |
LiNiOF (mp-765787) | 0.2509 | 0.041 | 4 |
LiNi4O4F (mp-765814) | 0.2638 | 0.066 | 4 |
Li2FeCuO4 (mp-773460) | 0.2552 | 0.045 | 4 |
TaN (mp-251) | 0.0000 | 0.327 | 2 |
ThC (mp-1164) | 0.0000 | 0.000 | 2 |
PuB (mp-2765) | 0.0000 | 0.854 | 2 |
SnP (mp-475) | 0.0000 | 0.033 | 2 |
HgS (mp-10764) | 0.0000 | 0.180 | 2 |
KNaH2 (mp-1007637) | 0.0000 | 0.055 | 3 |
MnCdO2 (mp-763469) | 0.0000 | 0.053 | 3 |
ScH4Pd3 (mp-981386) | 0.0000 | 0.035 | 3 |
CaCdO2 (mp-753287) | 0.0000 | 0.000 | 3 |
RbNaH2 (mp-999274) | 0.0000 | 0.105 | 3 |
As (mp-10) | 0.0000 | 0.107 | 1 |
Sc (mp-1008681) | 0.0000 | 0.716 | 1 |
C (mp-998866) | 0.0000 | 2.757 | 1 |
Ca (mp-10683) | 0.0000 | 0.396 | 1 |
Se (mp-7755) | 0.0000 | 0.181 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-points60 |
U Values-- |
PseudopotentialsVASP PAW: P La |
Final Energy/Atom-6.7459 eV |
Corrected Energy-13.4919 eV
-13.4919 eV = -13.4919 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)