Final Magnetic Moment2.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom0.000 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom< 0.001 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density0.04 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToH2 |
Band Gap7.496 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP63/mmc [194] |
Hall-P 6c 2c |
Point Group6/mmm |
Crystal Systemhexagonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 171.3 |
LaAlO3 (mp-2920) | <1 0 1> | <1 1 0> | 300.6 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 158.1 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 123.9 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 74.4 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 276.7 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 223.1 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 148.7 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 210.8 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 52.7 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 198.3 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 276.7 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 329.4 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 171.3 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 118.6 |
GaN (mp-804) | <1 0 0> | <1 0 1> | 196.5 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 74.4 |
GaN (mp-804) | <1 1 0> | <1 1 1> | 314.4 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 171.7 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 210.8 |
SiO2 (mp-6930) | <1 0 0> | <1 1 1> | 134.7 |
GaN (mp-804) | <1 1 1> | <1 0 1> | 365.0 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 171.7 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 210.8 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 92.2 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 173.5 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 237.1 |
SiO2 (mp-6930) | <1 1 1> | <1 1 1> | 269.5 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 123.9 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 210.8 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 1> | 269.5 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 198.3 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 171.7 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 1> | 252.7 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 1> | 224.6 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 223.1 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 1> | 252.7 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 276.7 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 171.3 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 210.8 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 329.4 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 257.6 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 316.2 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 118.6 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 210.8 |
CdS (mp-672) | <1 0 0> | <1 1 0> | 85.9 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 99.2 |
CdS (mp-672) | <1 1 0> | <1 0 1> | 196.5 |
CdS (mp-672) | <1 1 1> | <1 1 1> | 269.5 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 223.1 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
0 | 0 | -0 | 0 | 0 | 0 |
0 | 0 | -0 | 0 | 0 | 0 |
-0 | -0 | -0 | 0 | 0 | 0 |
0 | 0 | 0 | -0 | 0 | 0 |
0 | 0 | 0 | 0 | -0 | 0 |
0 | 0 | 0 | 0 | 0 | 0 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
-336457.4 | 340284.5 | -2054.7 | 0 | 0 | 0 |
340284.5 | -336457.3 | -2054.7 | 0 | 0 | 0 |
-2054.7 | -2054.7 | -4215.9 | 0 | 0 | 0 |
0 | 0 | 0 | -67222 | 0 | 0 |
0 | 0 | 0 | 0 | -67222 | 0 |
0 | 0 | 0 | 0 | 0 | -1353483.8 |
Shear Modulus GV0 GPa |
Bulk Modulus KV-0 GPa |
Shear Modulus GR-0 GPa |
Bulk Modulus KR-0 GPa |
Shear Modulus GVRH-0 GPa |
Bulk Modulus KVRH-0 GPa |
Elastic Anisotropy-6.60 |
Poisson's Ratio0.50 |
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
1.26 | 0.00 | 0.00 |
0.00 | 1.26 | 0.00 |
0.00 | 0.00 | 1.26 |
Dielectric Tensor εij (total) |
||
---|---|---|
1.26 | 0.00 | 0.00 |
0.00 | 1.26 | 0.00 |
0.00 | 0.00 | 1.26 |
Polycrystalline dielectric constant
εpoly∞
1.26
|
Polycrystalline dielectric constant
εpoly
1.26
|
Refractive Index n1.12 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Cr8Ni50Mo15W2 (mp-767372) | 0.2684 | 0.028 | 4 |
CrFeCoNi (mp-1012640) | 0.2199 | 0.065 | 4 |
CrFeCoNi (mp-1096923) | 0.4137 | 0.193 | 4 |
Pm3I (mp-976867) | 0.0037 | 0.351 | 2 |
LiRh (mp-600561) | 0.0002 | 0.000 | 2 |
Mg5Sb (mp-1094564) | 0.0028 | 0.116 | 2 |
MgAl (mp-1039019) | 0.0020 | 0.064 | 2 |
Li2Mg (mp-1094576) | 0.0044 | 0.014 | 2 |
In (mp-973111) | 0.0002 | 0.048 | 1 |
He (mp-23156) | 0.0014 | 0.002 | 1 |
Ni (mp-10257) | 0.0055 | 0.026 | 1 |
N2 (mp-12103) | 0.0027 | 0.000 | 1 |
Ag (mp-10597) | 0.0057 | 0.008 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: H |
Final Energy/Atom-1.1174 eV |
Corrected Energy-6.4795 eV
-6.4795 eV = -2.2348 eV (uncorrected energy) - 4.2447 eV (MP Gas Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)