material

CuH

ID:

mp-24093

DOI:

10.17188/1199906


Tags: Copper(I) hydride

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
0.049 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.049 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
6.67 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
H2 + Cu
Band Gap
0.731 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P63mc [186]
Hall
P 6c 2c
Point Group
6mm
Crystal System
hexagonal

Electronic Structure

Topological data for ICSD ID 44859 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
ZnO (mp-2133) <0 0 1> <0 0 1> 0.000 28.1
C (mp-48) <0 0 1> <0 0 1> 0.000 21.1
Fe2O3 (mp-24972) <0 0 1> <0 0 1> 0.000 91.4
KTaO3 (mp-3614) <1 1 1> <0 0 1> 0.000 28.1
C (mp-48) <1 1 0> <1 0 1> 0.001 133.2
TiO2 (mp-390) <1 1 1> <1 0 1> 0.005 162.8
C (mp-48) <1 0 0> <0 0 1> 0.006 77.3
SiC (mp-8062) <1 1 1> <0 0 1> 0.007 133.5
Al (mp-134) <1 1 1> <0 0 1> 0.008 28.1
LiAlO2 (mp-3427) <1 1 0> <1 0 0> 0.009 234.4
GdScO3 (mp-5690) <0 1 0> <1 0 0> 0.010 221.4
BaTiO3 (mp-5986) <0 0 1> <0 0 1> 0.011 112.4
Ga2O3 (mp-886) <1 0 -1> <0 0 1> 0.011 267.0
AlN (mp-661) <1 1 1> <1 1 1> 0.011 141.7
TiO2 (mp-390) <1 0 1> <1 0 1> 0.016 118.4
Cu (mp-30) <1 1 1> <0 0 1> 0.021 91.4
MgF2 (mp-1249) <1 1 1> <1 1 0> 0.023 90.2
SiC (mp-7631) <1 0 1> <1 0 1> 0.024 236.8
LaF3 (mp-905) <1 0 0> <1 1 1> 0.025 212.6
Te2W (mp-22693) <0 0 1> <1 0 0> 0.027 156.3
SrTiO3 (mp-4651) <1 1 1> <1 0 0> 0.027 208.3
PbS (mp-21276) <1 1 0> <1 1 0> 0.029 203.0
LiNbO3 (mp-3731) <1 1 1> <1 0 0> 0.029 130.2
ZnO (mp-2133) <1 0 1> <0 0 1> 0.030 119.5
NaCl (mp-22862) <1 0 0> <0 0 1> 0.031 224.9
Au (mp-81) <1 1 1> <0 0 1> 0.033 91.4
GaAs (mp-2534) <1 1 0> <0 0 1> 0.035 140.5
NdGaO3 (mp-3196) <1 0 1> <1 1 1> 0.036 212.6
LaAlO3 (mp-2920) <1 0 0> <1 0 0> 0.037 143.2
Ge (mp-32) <1 1 0> <0 0 1> 0.037 140.5
SiO2 (mp-6930) <1 1 1> <0 0 1> 0.037 105.4
Ni (mp-23) <1 1 1> <0 0 1> 0.038 21.1
ZnSe (mp-1190) <1 1 0> <0 0 1> 0.040 140.5
SiC (mp-7631) <1 1 1> <1 1 1> 0.041 165.4
TbScO3 (mp-31119) <0 1 0> <1 0 0> 0.045 221.4
TiO2 (mp-2657) <1 0 1> <1 0 1> 0.048 177.6
CdWO4 (mp-19387) <0 1 0> <0 0 1> 0.049 105.4
KTaO3 (mp-3614) <1 0 0> <0 0 1> 0.050 112.4
TiO2 (mp-390) <1 1 0> <1 0 1> 0.051 103.6
YVO4 (mp-19133) <1 1 1> <1 0 0> 0.052 247.4
PbS (mp-21276) <1 1 1> <0 0 1> 0.053 63.2
BaTiO3 (mp-5986) <1 1 0> <1 0 1> 0.053 118.4
MgAl2O4 (mp-3536) <1 1 0> <0 0 1> 0.054 281.1
TeO2 (mp-2125) <1 0 1> <1 0 0> 0.056 78.1
ZnO (mp-2133) <1 1 1> <1 0 0> 0.059 156.3
Te2Mo (mp-602) <0 0 1> <0 0 1> 0.063 133.5
MoS2 (mp-1434) <1 0 1> <1 0 0> 0.064 208.3
BaF2 (mp-1029) <1 1 0> <1 0 1> 0.066 281.1
ZnO (mp-2133) <1 1 0> <1 0 0> 0.067 91.2
GdScO3 (mp-5690) <1 0 1> <0 0 1> 0.069 56.2
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
156 90 86 0 0 0
90 156 86 0 0 0
86 86 142 0 0 0
0 0 0 34 0 0
0 0 0 0 34 0
0 0 0 0 0 33
Compliance Tensor Sij (10-12Pa-1)
11.2 -4.1 -4.3 0 0 0
-4.1 11.2 -4.3 0 0 0
-4.3 -4.3 12.3 0 0 0
0 0 0 29.2 0 0
0 0 0 0 29.2 0
0 0 0 0 0 30.6
Shear Modulus GV
33 GPa
Bulk Modulus KV
109 GPa
Shear Modulus GR
33 GPa
Bulk Modulus KR
108 GPa
Shear Modulus GVRH
33 GPa
Bulk Modulus KVRH
108 GPa
Elastic Anisotropy
0.02
Poisson's Ratio
0.36

Piezoelectricity

Reference for tensor and properties: Methodology
Piezoelectric Tensor eij (C/m2)
0.00000 0.00000 0.00000 0.00000 -0.21634 0.00000
0.00000 0.00000 0.00000 -0.21634 0.00000 0.00000
-0.13582 -0.13582 0.32230 0.00000 0.00000 0.00000
Piezoelectric Modulus ‖eijmax
0.37520 C/m2
Crystallographic Direction vmax
0.00000
-1.00000
-0.00000

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
13.02 0.00 0.00
0.00 13.02 0.00
0.00 0.00 14.04
Dielectric Tensor εij (total)
13.95 0.00 -0.00
0.00 13.95 -0.00
-0.00 -0.00 15.22
Polycrystalline dielectric constant εpoly
(electronic contribution)
13.36
Polycrystalline dielectric constant εpoly
(total)
14.37
Refractive Index n
3.66
Potentially ferroelectric?
Unknown

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
BeSiN2 (mp-7913) 0.1050 0.000 3
LiInSe2 (mp-20310) 0.1366 0.001 3
MgSnN2 (mp-1029791) 0.0676 0.000 3
ZnSnN2 (mp-1029469) 0.0968 0.000 3
Zn2SbN3 (mp-1029334) 0.1434 0.020 3
LiCo7O7F (mp-764039) 0.2392 0.061 4
LiCo5O5F (mp-764225) 0.2720 0.069 4
Li2ZnSnS4 (mp-555186) 0.2063 0.000 4
ZnGaNO (mp-558481) 0.2637 0.058 4
ZnGa3N3O (mp-555777) 0.2904 5.250 4
MnS (mp-2562) 0.0126 0.015 2
InN (mp-22205) 0.0228 0.000 2
AgI (mp-22894) 0.0201 0.001 2
ZnO (mp-2133) 0.0173 0.000 2
AgH (mp-1096804) 0.0044 0.121 2
Ge (mp-1007760) 0.1383 0.022 1
Si (mp-165) 0.1454 0.013 1
C (mp-611426) 0.3046 0.146 1
C (mp-47) 0.1524 0.162 1
Ge (mp-1091415) 0.3101 0.014 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Cu_pv H
Final Energy/Atom
-3.6079 eV
Corrected Energy
-14.7895 eV
Uncorrected energy = -14.4315 eV Composition-based energy adjustment (-0.179 eV/atom x 2.0 atoms) = -0.3580 eV Corrected energy = -14.7895 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 44859
Submitted by
User remarks:
  • Copper(I) hydride

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)