Final Magnetic Moment0.972 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-1.669 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.005 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.51 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToRbHSO4 + H2O + CuO |
Band Gap0.600 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 235.5 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 233.0 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 282.8 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 78.5 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 116.5 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 78.5 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 314.0 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 314.0 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 78.5 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 282.8 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 235.5 |
GaN (mp-804) | <1 1 0> | <0 1 1> | 290.3 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 157.0 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 282.8 |
DyScO3 (mp-31120) | <1 1 1> | <0 1 0> | 282.8 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 314.0 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 314.0 |
Te2Mo (mp-602) | <0 0 1> | <0 1 0> | 282.8 |
LiF (mp-1138) | <1 0 0> | <0 1 0> | 282.8 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 157.0 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 314.0 |
Ag (mp-124) | <1 0 0> | <1 0 1> | 156.1 |
Ag (mp-124) | <1 1 0> | <0 1 0> | 282.8 |
Al (mp-134) | <1 1 0> | <0 1 0> | 282.8 |
LiGaO2 (mp-5854) | <1 0 0> | <0 0 1> | 314.0 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 235.5 |
LiNbO3 (mp-3731) | <0 0 1> | <0 1 0> | 169.7 |
MoS2 (mp-1434) | <0 0 1> | <0 1 0> | 282.8 |
TeO2 (mp-2125) | <0 0 1> | <0 1 0> | 339.4 |
TeO2 (mp-2125) | <1 0 0> | <0 1 0> | 282.8 |
LiGaO2 (mp-5854) | <1 0 1> | <0 0 1> | 235.5 |
SiC (mp-7631) | <0 0 1> | <0 1 1> | 290.3 |
SiC (mp-7631) | <1 0 1> | <0 1 0> | 282.8 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 314.0 |
TiO2 (mp-2657) | <1 1 0> | <0 1 0> | 339.4 |
TiO2 (mp-2657) | <1 1 1> | <0 1 1> | 290.3 |
Mg (mp-153) | <1 0 1> | <0 1 0> | 56.6 |
Mg (mp-153) | <1 1 0> | <0 1 1> | 290.3 |
PbS (mp-21276) | <1 0 0> | <0 0 1> | 314.0 |
GaP (mp-2490) | <1 0 0> | <0 0 1> | 157.0 |
TbScO3 (mp-31119) | <0 1 0> | <0 1 0> | 226.2 |
TbScO3 (mp-31119) | <1 1 0> | <0 0 1> | 314.0 |
TbScO3 (mp-31119) | <1 1 1> | <0 1 0> | 282.8 |
Ni (mp-23) | <1 0 0> | <0 1 0> | 169.7 |
BaTiO3 (mp-5986) | <1 0 0> | <0 1 0> | 169.7 |
Au (mp-81) | <1 0 0> | <1 0 1> | 156.1 |
CdSe (mp-2691) | <1 0 0> | <0 0 1> | 78.5 |
WS2 (mp-224) | <0 0 1> | <0 1 0> | 282.8 |
C (mp-48) | <0 0 1> | <0 1 0> | 169.7 |
LiTaO3 (mp-3666) | <0 0 1> | <0 1 0> | 282.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CrH6SO7 (mp-745180) | 0.5746 | 0.026 | 4 |
Co5P4(HO2)10 (mp-743741) | 0.5811 | 0.187 | 4 |
Na2PH3O5 (mp-644245) | 0.5611 | 0.008 | 4 |
VH10SO10 (mp-745140) | 0.5806 | 0.001 | 4 |
Mn5P4(HO2)10 (mp-744430) | 0.5871 | 0.003 | 4 |
K2CuH12(SO7)2 (mp-24038) | 0.2176 | 0.006 | 5 |
Tl2CuH12(SO7)2 (mp-24196) | 0.1991 | 0.000 | 5 |
Rb2CuH12(SeO7)2 (mp-510018) | 0.2284 | 0.000 | 5 |
Rb2CuH12(SO7)2 (mp-559981) | 0.0663 | 0.005 | 5 |
K2CuH12(SO7)2 (mp-559018) | 0.2252 | 0.006 | 5 |
K2FePH5(CO5)2 (mp-604118) | 0.7221 | 0.119 | 6 |
CsKTeH6SO10 (mp-559375) | 0.7109 | 0.000 | 6 |
NaCoBP2H2O9 (mp-601388) | 0.7415 | 0.072 | 6 |
Be2CoH20N2(O3F4)2 (mp-25732) | 0.7297 | 0.000 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Rb_sv Cu_pv H S O |
Final Energy/Atom-5.2597 eV |
Corrected Energy-348.4190 eV
-348.4190 eV = -326.1010 eV (uncorrected energy) - 22.3180 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)