Final Magnetic Moment0.012 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.045 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.52 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFm3m [225] |
Hall-F 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Topological ClassificationSM*
|
SubclassificationESFD†
|
Crossing TypePoint
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <1 1 0> | 141.4 |
LaAlO3 (mp-2920) | <1 1 1> | <1 1 1> | 123.7 |
AlN (mp-661) | <0 0 1> | <1 1 1> | 24.7 |
AlN (mp-661) | <1 0 0> | <1 1 0> | 141.4 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 80.8 |
AlN (mp-661) | <1 1 1> | <1 1 1> | 197.9 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 28.6 |
CeO2 (mp-20194) | <1 1 1> | <1 0 0> | 257.1 |
LaAlO3 (mp-2920) | <0 0 1> | <1 1 1> | 24.7 |
LaAlO3 (mp-2920) | <1 0 1> | <1 1 1> | 74.2 |
LaAlO3 (mp-2920) | <1 1 0> | <1 1 0> | 121.2 |
AlN (mp-661) | <1 0 1> | <1 1 0> | 181.8 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 40.4 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 128.5 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 181.8 |
GaAs (mp-2534) | <1 1 1> | <1 1 1> | 173.1 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 357.0 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 161.6 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 181.8 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 128.5 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 181.8 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 157.1 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 85.7 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 214.2 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 60.6 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 285.6 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 214.2 |
SiO2 (mp-6930) | <0 0 1> | <1 1 1> | 296.8 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 128.5 |
Te2W (mp-22693) | <0 1 0> | <1 1 0> | 161.6 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 185.7 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 314.2 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 142.8 |
SiO2 (mp-6930) | <1 1 1> | <1 1 0> | 161.6 |
KCl (mp-23193) | <1 0 0> | <1 1 1> | 123.7 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 60.6 |
KCl (mp-23193) | <1 1 1> | <1 1 1> | 74.2 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 257.1 |
YVO4 (mp-19133) | <1 0 0> | <1 1 0> | 242.4 |
YVO4 (mp-19133) | <1 1 0> | <1 0 0> | 314.2 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 228.5 |
TePb (mp-19717) | <1 1 0> | <1 1 0> | 60.6 |
TePb (mp-19717) | <1 1 1> | <1 1 1> | 74.2 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 60.6 |
DyScO3 (mp-31120) | <0 1 0> | <1 1 0> | 262.6 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 0> | 161.6 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 0> | 181.8 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 214.2 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 128.5 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 0> | 271.3 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
460 | 127 | 127 | 0 | 0 | 0 |
127 | 460 | 127 | 0 | 0 | 0 |
127 | 127 | 460 | 0 | 0 | 0 |
0 | 0 | 0 | 120 | 0 | 0 |
0 | 0 | 0 | 0 | 120 | 0 |
0 | 0 | 0 | 0 | 0 | 120 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
2.5 | -0.5 | -0.5 | 0 | 0 | 0 |
-0.5 | 2.5 | -0.5 | 0 | 0 | 0 |
-0.5 | -0.5 | 2.5 | 0 | 0 | 0 |
0 | 0 | 0 | 8.3 | 0 | 0 |
0 | 0 | 0 | 0 | 8.3 | 0 |
0 | 0 | 0 | 0 | 0 | 8.3 |
Shear Modulus GV139 GPa |
Bulk Modulus KV238 GPa |
Shear Modulus GR136 GPa |
Bulk Modulus KR238 GPa |
Shear Modulus GVRH137 GPa |
Bulk Modulus KVRH238 GPa |
Elastic Anisotropy0.13 |
Poisson's Ratio0.26 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Sr4SO3 (mp-1079788) | 0.0000 | 0.200 | 3 |
BaSr3O4 (mp-984729) | 0.0000 | 0.044 | 3 |
ScH4Pd3 (mp-981386) | 0.0000 | 0.039 | 3 |
Sr3CdO4 (mp-981103) | 0.0000 | 0.019 | 3 |
SrCa3O4 (mp-978844) | 0.0000 | 0.040 | 3 |
EuP (mp-20300) | 0.0000 | 0.000 | 2 |
TaO (mp-1895) | 0.0000 | 1.108 | 2 |
NpSb (mp-20969) | 0.0000 | 0.000 | 2 |
NpO (mp-6927) | 0.0000 | 0.157 | 2 |
HoSe (mp-464) | 0.0000 | 0.000 | 2 |
As (mp-10) | 0.0000 | 0.126 | 1 |
Sc (mp-1008681) | 0.0000 | 0.719 | 1 |
Ca (mp-10683) | 0.0000 | 0.393 | 1 |
C (mp-998866) | 0.0000 | 2.763 | 1 |
Sb (mp-133) | 0.0000 | 0.051 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Cr_pv H |
Final Energy/Atom-6.4914 eV |
Corrected Energy-12.9827 eV
-12.9827 eV = -12.9827 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)